Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Higher residual ash
What ifWhat if the recovered carbon black contains 12 mass % ash?
Claim language“10 mass % or less”
The process removes steel from the tire feed and mills the pyrolysis solid while retaining fine mineral residue in the powder. A sidewall formulation blends the recovered powder with a reinforcing furnace carbon black to reach the specified modulus.
1.1Lower area with branched aggregates
What ifWhat if the recovered carbon black has a statistical thickness specific surface area of 40 m2/g and a high proportion of branched aggregates?
Claim language“statistical thickness specific surface area of 50 m2/g or more”
Feedstock selection and mild milling retain branched aggregates. The branches immobilize some rubber within their voids, increasing the effective filler volume and the compound modulus.
1.1Lower area with platelet reinforcement
What ifWhat if the recovered carbon black has a statistical thickness specific surface area of 35 m2/g and exfoliated clay supplies additional reinforcement?
Claim language“statistical thickness specific surface area of 50 m2/g or more”
An internal mixer incorporates an organophilic clay masterbatch into a natural rubber compound containing the lower-area recovered powder. Dispersed clay platelets carry part of the load and increase the cured compound modulus.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Recovered carbon black in asphalt
This asphalt binder uses recovered carbon black containing 85–97 mass % carbon and 0.5–10 mass % ash, with a statistical thickness specific surface area of at least 50 m²/g. A rotor-stator mixer disperses 4 parts of dry powder per 100 parts of asphalt binder at 160 °C for 30 minutes. The modified binder coats heated mineral aggregate during asphalt mixing.
Component substitution
Furnace carbon black as reinforcing filler
Furnace carbon black with a statistical thickness specific surface area of 75–85 m²/g replaces recovered carbon black in a tire tread compound. An internal mixer disperses 50 parts of the furnace carbon black per 100 parts of styrene-butadiene and butadiene rubber. The compound cools before a second mixing pass incorporates sulfur and accelerators for vulcanization.
Parameter or scale variation
Higher surface area filler blend
Two recovered carbon black lots each contain 88–94 mass % carbon and 6–9 mass % ash. The lots have statistical thickness specific surface areas of 65–75 m²/g and 100–110 m²/g, respectively. A ribbon blender mixes the lots in a 1:4 mass ratio, and nitrogen adsorption measurements verify a finished blend target of 90–105 m²/g.
Split filler addition during tread mixing
A batch internal mixer compounds 45 parts of recovered carbon black per 100 parts of rubber using two filler additions. The first addition supplies 30 parts after 30 seconds of rubber mastication, and the second supplies 15 parts with the process oil when the stock reaches 100 °C. The mixer discharges the batch at 150 °C, and a separate finishing pass adds sulfur and accelerators below 105 °C.
Combination with existing systems
Pellet feed for continuous rubber mixing
A pin mixer agglomerates recovered carbon black with water, and a rotary dryer reduces the pellet moisture content to below 1 mass %. A screen collects pellets between 0.5 and 2 mm for delivery to a loss-in-weight feeder. The feeder meters the pellets into a continuous twin-screw rubber mixer downstream of the rubber feed, where kneading blocks break the pellets apart and disperse the filler.
Automated or data-driven variant
Automated blending from lot measurements
A controller receives dry-basis carbon and ash measurements and statistical thickness specific surface area results for recovered carbon black stored in separate bins. Software calculates blend fractions using mass-weighted averages as initial estimates and targets 90–94 mass % carbon, 6–8 mass % ash, and at least 60 m²/g. Load cells track discharge from each bin, and the controller adjusts the feeder speeds to deliver the calculated fractions to a batch blender. A composite sample from the finished batch supplies measurements for release.
Specific version of a part
Steam treated recovered powder
A short steam treatment removes residual carbonaceous deposits from a washed pyrolysis solid and exposes aggregate surfaces. The finished powder contains 94 mass % carbon and 4 mass % ash, and nitrogen adsorption gives a statistical thickness specific surface area of 65 m2/g.
Blended recovered powder lots
A ribbon blender combines equal dry masses of two recovered powder lots with measured statistical thickness specific surface areas of 52 and 72 m2/g. The finished blend measures 62 m2/g and contains 93 mass % carbon and 5 mass % ash.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1Recovered carbon black having a carbon content of 85 mass % or more and 97 mass % or less, an ash content of 0.5 mass % or more and 10 mass % or less, and a statistical thickness specific surface area of 50 m2/g or more.
A pyrolytic carbon black produced from pyrolyzed rubber, said pyrolytic carbon black having: a) an ash content ranging between 9-15%; b) a toluene discoloration at 425 mu of 80-90% transmission; c) an iodine adsorption between 30 and 45 mg/gm; and, d) an n-dibutyl phthalate absorption number of up to 65 cc/100 gm.
A · US 2010/0249353 A1 · claim 17
Data analysis shows that sulfonated tire rubber yields carbon with 64 m2/g specific surface area; whereas that of the control carbon (fluffy carbon from Sample #1) is 96 m2/g.
B · US 2015/0021525 A1 · ¶ 50
An empty cell means only that no passage was reproduced there.
Statements in these documents
Moreover, the demanding product specifications for safe, durable tires make scrap tires difficult and expensive to break down.
A · US 2010/0249353 A1 · ¶ 6
Punching or die cutting small sections of rubber from tire treads or sidewalls can be used to create items such as water troughs.
A · US 2010/0249353 A1 · ¶ 8
Isolation of the carbon black from tire formulations was tried but such products are not necessarily good reinforcing fillers for a new rubber formulation.
B · US 2015/0021525 A1 · ¶ 4
Utilization of tire rubber materials for value-added applications would be very attractive not only for the recovery of materials but also to control global pollution.
B · US 2015/0021525 A1 · ¶ 4
Cite aspatent.fyi, US 2026/0357033 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357033/, SHA-256 9a281be25206caf2b2202015d9052ea9364a77e3d4f9b17f04275a7553869a99