patent.fyi
Applications  /  US 2026/0357035
United States Patent Application Publication

US 2026/0357035 A1

Published
Nov 12, 2026
Filed
Oct 17, 2022
Earliest date on the face
Oct 17, 2022
Classification
C08K 3/041
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Polyphenylene sulfide matrix

What ifWhat if polyphenylene sulfide forms the entire polymer matrix of the carrier?
Claim language“poly(aryl ether ketone) polymer”

A twin-screw extruder compounds the polyphenylene sulfide with conductive carbon black and 25 wt. % ground mica. Injection molding forms the carrier, and interconnected carbon black aggregates conduct charge to a grounded contact.

1.1Polyetherimide matrix

What ifWhat if amorphous polyetherimide forms the entire polymer matrix of the carrier?
Claim language“poly(aryl ether ketone) polymer”

A twin-screw extruder blends dried polyetherimide pellets with multiwall carbon nanotubes and 25 wt. % ground fused silica. Injection molding forms the carrier, and the nanotube network conducts charge from substrate contact surfaces to a grounding tab.

1.2Stainless steel fiber network

What ifWhat if micrometer-diameter stainless steel fibers provide all electrical conduction through the molded carrier?
Claim language“electrically conductive carbon nanofiller”

A late extruder feed introduces stainless steel fibers of about 8 micrometers in diameter into a melt containing poly(aryl ether ketone) and ground mica. Fiber contacts form conductive paths through the molded part, and the fiber loading is set using resistance measurements taken from substrate seats to the grounding point.

1.2Grounded resistive oxide film

What ifWhat if a continuous resistive oxide film carries charge along the carrier surface while the molded body contains only polymer and insulating filler?
Claim language“electrically conductive carbon nanofiller”

Reactive sputtering deposits a tin oxide film across the substrate seats and a continuous track to a grounded metal tab. Deposition conditions and film thickness set sheet resistance, and the continuous film provides a surface path for charge to drain.

1.3Glass fibers for stiffness

What ifWhat if chopped glass fibers are the sole reinforcing filler in a poly(aryl ether ketone) carrier that uses carbon nanotubes for charge dissipation?
Claim language“non-fibrous filler”

A twin-screw extruder disperses the nanotubes in the polymer melt before chopped glass fibers enter through a downstream feed port. The retained glass fibers carry mechanical load, and interconnected nanotubes conduct charge to the grounding contact.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Dissipative guides for pharmaceutical packaging

Mold replaceable conveyor guides from poly(aryl ether ketone) compounded with conductive carbon nanofiller and at least 20 wt. % non-fibrous mineral filler. Machine a smooth contact face where dry polymer trays slide past the guides. Clamp the back of each guide against a grounded metal bracket so charge on the guide drains through the composite and bracket.

Component substitution

Graphene nanoplatelets as the conductive phase

Use conductive graphene nanoplatelets in place of carbon nanotubes and retain 25 wt. % ground fused silica as the non-fibrous filler. Feed a graphene nanoplatelet masterbatch in poly(aryl ether ketone) into a twin-screw extruder with the remaining resin, then add the silica downstream. Mold plaques at several nanoplatelet loadings and select the loading that produces the specified surface resistance across the molded contact face.

Parameter or scale variation

Controlled filler size for thin ribs

Compound poly(aryl ether ketone) and conductive carbon nanofiller with 25 wt. % spherical fused silica having a median particle diameter of 8 µm and a 90th-percentile diameter of 20 µm. Injection mold a 2 mm base with 0.8 mm ribs and gate the part so melt enters each rib from the base. Measure resistance from each rib tip to a common contact pad on the base to check electrical continuity through the molded section.

Two particle sizes in one blend

Blend 18 wt. % spherical alumina with a median particle diameter of 30 µm and 12 wt. % spherical alumina with a median diameter of 3 µm into a poly(aryl ether ketone) formulation containing conductive carbon nanofiller. Meter both alumina fractions into a downstream feed port after the resin and carbon nanofiller enter the melt mixing zone. The fine particles occupy spaces between coarser particles, and resistance measurements on molded plaques quantify the effect of the size blend on the conductive network.

Combination with existing systems

Grounded rails in an inspection station

Fit a machine-vision inspection station with locating rails molded from poly(aryl ether ketone), conductive carbon nanofiller and at least 20 wt. % non-fibrous filler. Seat each rail on a conductive mounting plate and connect the plate to the station’s grounding point. A positioning actuator slides each workpiece against the rails to establish a repeatable camera position while charge on the rails drains to ground.

Automated or data-driven variant

Automated resistance mapping of molded parts

Mold parts from poly(aryl ether ketone) compounded with conductive carbon nanofiller and at least 20 wt. % non-fibrous filler. A programmable gantry places a spring-loaded electrode at predefined contact locations while a fixture electrode contacts the part’s grounding pad. Software records resistance at each location after a fixed settling time and flags parts with any reading outside the configured acceptance range.

Specific version of a part

Semicrystalline ether ketone matrix

Poly(ether ether ketone) forms the continuous phase and binds the conductive carbon and mineral filler into a molded carrier. A heated mold promotes matrix crystallization during cooling.

Multiwall carbon nanotube network

Multiwall carbon nanotubes with outer diameters of 10 to 30 nanometers enter the melt through a masterbatch in the same matrix polymer. Intertube contacts and tunneling across small gaps provide conductive paths through the molded carrier.

Ground mica platelet filler

Ground muscovite mica with a median particle size of 20 micrometers supplies plate-shaped mineral reinforcement. The platelets orient preferentially along melt flow during injection molding and limit shrinkage in the plane of the molded wall.

Twenty five percent silica

Ground fused silica accounts for 25 wt. % of the total compounded mass, including the matrix polymer and conductive carbon. Gravimetric feeders meter 25 kilograms of silica per 100 kilograms of total feed.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2011/0168288 A1
Published
Jul 14, 2011
Filed
Sep 18, 2009
Class
F16L 11/00
Document BUS 9,896,564 B2
Published
Feb 20, 2018
Filed
Jun 3, 2013
Class
C08K 3/04
Document CUS 2020/0239655 A1
Published
Jul 30, 2020
Filed
Dec 13, 2019
Class
C08J 7/18
Claim 1
Document A
Document B
1.1at least one poly(aryl ether ketone) polymer (PAEK polymer),
Flexible pipe (fP) suitable for transporting hydrocarbons, said flexible pipe comprising at least one polymer layer (L) composed of a polymer composition (C) comprising at least one poly(aryl ether ketone) (P1), and at least one per(halo)fluoropolymer (P2).
A · US 2011/0168288 A1 · abstract
The method according to claim 3, wherein the thermoplastic polymer is selected from the group consisting of homo- and copolymers of olefins; acrylic homo- and copolymers and poly(alkyl (meth)acrylate)s; homo- and copolyamides; polycarbonates; polyesters; polyethers; polystyrene; copolymers of styrene and maleic anhydride; poly(vinyl chloride); fluoropolymer; natural or synthetic rubbers; thermoplastic polyurethanes; polyaryletherketones (PAEKs); polyetherimide; polysulphone;
B · US 9,896,564 B2 · claim 4
1.2at least one electrically conductive carbon nanofiller (component A1), and
The polymer composition (C) may further contain conventional ingredients of poly(aryl ether ketone) and per(halo)fluoropolymer compositions, including lubricating agents, heat stabilizers, anti-static agents, organic and/or inorganic pigments, carbon black, acid scavengers, such as MgO, stabilizers, i.e., metal oxides and sulfides such as zinc oxide and zinc sulfide, antioxidants, flame retardants and smoke-suppressing agents.
A · US 2011/0168288 A1 · ¶ 103
A composite product comprising a composite material, the composite material stabilized with respect to UV light using a content of between 1 ppm and 0.1% by weight, of carbon-based nanofillers chosen from carbon nanotubes, carbon nanofibers, graphene or a mixture of these in all proportions, wherein the composite product is selected from yarns, films, tubes, fibers, and nonwovens.
B · US 9,896,564 B2 · abstract
1.3at least one non-fibrous filler (component A2),
1.4wherein the polyarylether composition (C) comprises, based on the total weight of the polyarylether composition (C), at least 20 wt. % of the component A2.

An empty cell means only that no passage was reproduced there.

Statements in these documents
In fact, flexible pipes can be useful for transporting virtually any fluid in any environment, including when the fluid to be transported and/or the environment where to transport it, is chemically aggressive.
A · US 2011/0168288 A1 · ¶ 3
Yet, flexible pipes must also be strong enough to survive stresses imparted by waves, currents, and tides as well as severe pressures and sharp temperature fluctuations.
A · US 2011/0168288 A1 · ¶ 4
The present invention relates to the use of very low contents of carbon-based nanofillers, in particular of carbon nanotubes, for improving the resistance to ageing, in particular the protection with regard to ultraviolet (UV) light, of a composite material based on a polymer matrix.
B · US 9,896,564 B2 · ¶ 1
However, CNTs prove to be difficult to handle and to disperse, due to their small size, their dusty nature and possibly, when they are obtained by the CVD technique, their entangled structure, all the more so when it is desired to increase their mass productivity for the purposes of improving the production and of reducing the residual ash content.
B · US 9,896,564 B2 · ¶ 5
Cite aspatent.fyi, US 2026/0357035 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357035/, SHA-256 1f417b207bc3d546a9bf0378e2546af4d722803a6101a56db89d112fad1a9de4
First published
Permanent addresshttps://patent.fyi/US20260357035/
Content fingerprint (SHA-256)1f417b207bc3d546a9bf0378e2546af4d722803a6101a56db89d112fad1a9de4