1.1Crosslinked silicone matrix
Aluminum nitride powder is dispersed in an addition-curing silicone and molded into a sheet. Curing forms a crosslinked network that holds the powder in place while the sheet compresses against mating surfaces.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Aluminum nitride powder is dispersed in an addition-curing silicone and molded into a sheet. Curing forms a crosslinked network that holds the powder in place while the sheet compresses against mating surfaces.
Alumina powder is melt compounded into high-density polyethylene and pressed into a thin sheet. The polyethylene forms crystalline regions during cooling, and the dispersed alumina increases heat conduction through the sheet.
A molded polycarbonate frame captures the perimeter of a copper slug and leaves both faces exposed. Clamping seats those faces against the heat source and heat sink, and heat flows through the bulk copper.
An unfilled polycarbonate carrier positions a flattened copper heat pipe with its evaporator seated against the heat source and its condenser coupled to the heat sink. Water evaporates at the hot end, condenses at the cool end, and returns through a capillary wick.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Mold an amorphous polycarbonate sheet containing zinc oxide particles into a curved shim that matches the outside of a refrigeration pipe. Clamp the shim between the pipe and a copper sensor shoe with a spring band. A thermistor seated in the shoe measures the temperature conducted from the pipe through the shim.
Use zinc oxide powder with a median particle diameter of 5 micrometers as the heat dissipation filler in an amorphous polycarbonate matrix. Dry the resin, melt compound it with the powder in a twin-screw extruder, and compression mold the compound into a flat sheet. Clamp the sheet between a heater block and a metal heat spreader so that heat passes through the filled matrix.
Compression mold an amorphous polycarbonate and zinc oxide compound into a single stepped sheet with a 0.25 mm section and a 0.50 mm section. Position the thicker section over the shorter of two adjacent packages whose top surfaces differ in height by 0.25 mm. Clamp a flat heat spreader over both sections so that each package has a conductive path to the spreader.
Melt compound amorphous polycarbonate with graphite flakes and extrude it through a slit die into a 0.6 mm sheet. Pass the hot sheet through a calender set to a 0.4 mm gap so that rolling aligns the broad faces of the flakes approximately parallel to the sheet surfaces. Clamp a heater near the sheet center and a metal frame around its perimeter so that heat travels laterally along the aligned flakes toward the frame.
Die cut a sheet of amorphous polyetherimide filled with zinc oxide to match the footprint of a power module baseplate. Place the sheet between the baseplate and an aluminum cold plate with internal coolant channels, then clamp the assembly with spring-loaded screws. Heat crosses the sheet and the channel wall before the flowing coolant carries it away.
Produce compression-molded pads from the same amorphous polycarbonate and zinc oxide compound in several calibrated thicknesses. At an assembly station, a laser displacement sensor measures the package top and the heat sink seating surface relative to a common fixture datum. A controller calculates the assembled gap, selects a pad whose thickness brings it into contact with both surfaces at the specified clamp load, and directs a pick-and-place head to install it.
Aluminum nitride powder is melt compounded into amorphous polyetherimide using a twin-screw extruder. The compound is pelletized and compression molded into solid interface pads.
Spherical alumina powders with median particle diameters of 3 and 25 micrometers are blended and melt compounded into amorphous polysulfone. The smaller particles occupy gaps among the larger particles and increase the packing density of the filler.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
It is preferable that the thermoplastic resin used for the thermally conductive resin sheet does not cause any trouble even at 290° C. for 5 minutes, which is the reflow condition for the heat dissipation circuit board. To meet this requirement, it is preferable to use an amorphous thermoplastic resin having a glass transition temperature (Tg) of at least 300° C. or higher, or a crystalline thermoplastic resin having a melting point (Tm) of at least 300° C. or higher.A · US 2022/0002608 A1 · ¶ 52
The thermoplastic surfacer includes a broadgood having an amorphous thermoplastic resin, one or more fillers embedded into the broadgood, and a lightning strike protection mesh or foil embedded into the broadgood.B · US 11,504,925 B2 · abstract
An empty cell means only that no passage was reproduced there.
In recent years, especially in the electric and electronic fields, heat generation due to high implementation density of integrated circuits has become a major problem, and how to dissipate the heat has become an urgent issue.A · US 2022/0002608 A1 · ¶ 5
However, the ceramic substrates have the disadvantages of being easily broken by impact, and being difficult to thin film and downsize.A · US 2022/0002608 A1 · ¶ 5
If the part is thereafter subjected to a lightning strike, the current passes from the entry point to an exit point via the conductive mesh or foil eliminating structural damage to the aircraft part.B · US 11,504,925 B2 · ¶ 3
Moreover, the low surface energy of the semi-crystalline thermoplastic parts makes it difficult for the secondary application of lightning strike protection to a thermoplastic skin in a durable fashion.B · US 11,504,925 B2 · ¶ 7
patent.fyi, US 2026/0357036 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357036/, SHA-256 3c7c676d47db5b9489fcfb45fdb065d689cee130157cd0c657688cb12a33109d