1.1Polybutylene succinate molding matrix
Dry polybutylene succinate pellets melt in the injection barrel and fill a temperature-controlled mold. The polyester chains crystallize during cooling and give the part enough stiffness for ejection.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Dry polybutylene succinate pellets melt in the injection barrel and fill a temperature-controlled mold. The polyester chains crystallize during cooling and give the part enough stiffness for ejection.
An injection screw melts isotactic polypropylene pellets and forces the melt into a cooled cavity. The stereoregular chains pack into crystalline lamellae as the part solidifies.
A twin-screw extruder disperses talc platelets through the molten polyester. During mold cooling, the platelet surfaces provide heterogeneous nucleation sites from which polymer crystallites grow.
A melt-compounded concentrate distributes hexagonal boron nitride platelets throughout the molding feed. The dispersed platelet surfaces provide sites for crystal formation as the polyester cools.
The additive is 2-hydroxyethyl lactate, with a terminal hydroxyl on its ester side chain. Its hydroxyl groups form hydrogen bonds with polyester carbonyls, and the mold temperature and hold time control how long chain segments have to organize into crystals.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Polyhydroxyalkanoate pellets and ethyl lactate feed a compounding extruder, with the liquid metered into the molten polymer downstream of the pellet feed. A flat die casts the compound into sheet, and chill rolls set the sheet thickness. A vacuum forming station reheats the sheet until pliable, draws it into a temperature-controlled tool with instrument-shaped recesses, and holds it there until the insert retains its shape on release.
Micronized talc replaces the lactic acid additive in a polyhydroxyalkanoate molding compound. A side feeder introduces the talc into molten polymer at 2 parts by mass per 100 parts polymer, and a twin-screw extruder disperses the particles before pelletizing the compound. The talc surfaces provide sites for heterogeneous crystal nucleation as the compound cools in the mold.
A plate mold forms 1 mm thick plaques from polyhydroxyalkanoate containing ethyl lactate. Differential scanning calorimetry locates the crystallization peak of the compounded resin during cooling, and a recirculating fluid loop sets the mold surface to that temperature before filling. The controller holds the initial setpoint for 20 seconds after filling, then switches to a second fluid loop set 25 °C lower to cool the plaque before ejection.
An annular die extrudes a polyhydroxyalkanoate melt compounded with ethyl lactate into a continuous tube. The tube enters a vacuum sizing sleeve that fixes its outside diameter while a tempered water bath controls cooling through the crystallization interval measured for the blend. A second water bath cools the tube before a belt puller feeds it to a cut-to-length station.
A flat-die extrusion coating line deposits molten polyhydroxyalkanoate containing ethyl lactate onto the exterior face of a moving paperboard web. A pressure roll presses the coating against the paperboard, and a temperature-controlled roll sets the coating before the web enters a heated dwell zone for further crystallization. Cooling rolls stabilize the laminate before a rotary die cuts blanks for folding into trays.
An injection mold for polyhydroxyalkanoate compounded with ethyl lactate carries an ultrasonic pulse-echo transducer behind a cavity insert. The controller records echo timing and amplitude during cooling and calibrates the signal against plaque crystallinity measured by differential scanning calorimetry and against part distortion measured after ejection. During production, the controller commands ejection when the signal reaches the calibrated threshold and remains there for a preset interval.
Poly(3-hydroxybutyrate) supplies the molding matrix. Its stereoregular chains crystallize into lamellae during cooling in the mold.
The molding resin contains 3-hydroxybutyrate and 3-hydroxyvalerate repeat units, with 3-hydroxyvalerate at 5 mole percent. The hydroxyvalerate units introduce ethyl side groups that change crystal packing and the melting behavior of the copolymer.
Ethyl lactate retains the hydroxyl group adjacent to the ester carbonyl and carries an ethyl group on the ester oxygen. A metering pump feeds the liquid into a closed mixing section to disperse it through the molten polyester.
Lactamide uses nitrogen for Y and hydrogen for both R1 and R2, giving the structure CH3–CH(OH)–C(=O)–NH2. Its hydroxyl and amide N–H groups serve as hydrogen-bond donors to carbonyl groups in the polyester.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Polyhydroxybutyrate (PHB) is accumulated as a carbon and energy storage material in various microorganisms and is the best-characterized member of the polyhydroxyalkanoates (PHAs), which have drawn much attention as biodegradable substitutes for conventional nonbiodegradable plastics.A · US 2005/0227340 A1 · ¶ 6
In one embodiment, the degradable polyester is at least one of polylactic acid, polyglycolic acid, polybutylene succinate, polyhydroxyalkanoate, polycaprolactone, polyethylene glycol adipate, a polylactic-co-glycolic acid or a polyhydroxybutyrate valerate copolymer.B · US 10,973,948 B2 · ¶ 16
Polylactic acid was separated and purified through a GPC method, so as to obtain polylactic acid containing a residual monomer at a mass fraction of 0.1%.B · US 10,973,948 B2 · ¶ 53
An empty cell means only that no passage was reproduced there.
When PHA is produced in bacterial fermentation systems, the unit cost of production is at least five times higher than that of chemically synthesized polyethylene.A · US 2005/0227340 A1 · ¶ 5
The recovery cost is considerably decreased with increasing PHA content (P/X, %).A · US 2005/0227340 A1 · ¶ 8
The iron-based device is corroded slowly in an environment of an organism, and accelerated corrosion of the iron-based device may be realized by applying degradable polyester to its surface.B · US 10,973,948 B2 · ¶ 3
However, the degradable polyester applied to the surface of the iron-based device may increase the non-uniformity degree of the corrosion of the iron-based device, which possibly leads to local fracture of the iron-based device and affects the mechanical property of the iron-based device in the early stage after implantation.B · US 10,973,948 B2 · ¶ 4
patent.fyi, US 2026/0357039 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357039/, SHA-256 ecbfbd474086fc68b0a19c2401ab1772d2cd3e6c266b2df318537eecd482fee4