Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Lower glass transition temperature
What ifWhat if every elastomer in the composition had a glass transition temperature below −100 °C?
Claim language“−95 °C to about −75 °C”
The formulation uses 100 phr of high-cis polybutadiene with a glass transition temperature near −105 °C. The low glass transition temperature preserves chain mobility at low service temperatures, and sulfur curing forms the elastic network.
1.2Disulfide silane coupling
What ifWhat if the coupling agent used a bis(triethoxysilylpropyl) disulfide?
Claim language“a blocked mercapto silane”
The triethoxysilyl groups hydrolyze and condense with silica surface hydroxyl groups during mixing. The disulfide group participates in sulfur vulcanization and links the surface-bound silane to the polydiene network.
1.3Hydrocarbon resin for tack
What ifWhat if the resin fraction consisted of 40 phr of a hydrocarbon resin made from a five-carbon olefin feed?
Claim language“an ester of a resin acid and a polyhydric alcohol”
The mixer incorporates a solid aliphatic hydrocarbon resin with a softening point near 95 °C during the initial mixing stage. The resin softens and disperses in the polydiene, increasing tack in the uncured compound.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Automated or data-driven variant
Temperature and energy controlled mixing
Load-cell hoppers meter precipitated silica, 6 phr of blocked mercapto silane, and 45 phr of resin-acid polyol ester into an internal mixer with 100 phr of polydiene that includes an elastomer with a glass transition temperature between −95 °C and −75 °C. A stock temperature probe supplies feedback to a controller that adjusts rotor speed to maintain 145–155 °C during the hot mixing stage. The controller integrates net rotor power over time, divides the accumulated energy by batch mass, and releases the batch when it reaches a setpoint established from batches that meet the silica dispersion target. After cooling, the controller starts a separate pass for sulfur and accelerators and discharges the stock at the programmed mixing time or at 105 °C, whichever comes first.
Specific version of a part
Glycerol ester of rosin
The compound contains 45 phr of a solid resin made by esterifying rosin acids with glycerol. The resin softens during hot mixing and contributes tack to the uncured compound.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a polydiene in the amount of about 75 phr to about 100 phr, wherein the polydiene comprises one or more elastomers, and wherein at least one elastomer has a glass transition temperature of from about −95 °C to about −75 °C;
Suitable polybutadiene rubbers may be prepared, for example, by organic solution polymerization of 1,3-butadiene. The PBD may be conveniently characterized, for example, by having at least a 90 wt. % cis-1,4-microstructure content (“high cis” content), or at least 95 wt. %, or at least 96 wt. %.
B · US 2025/0109286 A1 · ¶ 58
1.2at least about 5 phr of a coupling agent comprising a blocked mercapto silane; and
The coupling agent can also include other silane sulphides, e.g., silanes having at least one thiol (—SH) functional group and/or at least one masked thiol functional group.
A · US 2021/0087369 A1 · ¶ 51
The organosilane coupling agent includes a blocked mercapto organosilane, such as 3-octanoylthio-1-propyltriethoxysilane.
B · US 2025/0109286 A1 · ¶ 14
1.3at least about 40 phr of a resin, where the resin comprises an ester of a resin acid and a polyhydric alcohol.
In embodiments, the rosin ester resin is a phenolic modified rosin ester, prepared by the reaction of rosin with a formaldehyde-containing compound and a phenolic compound, to yield an intermediate phenolic resin, which is then esterified with a polyhydric alcohol.
A · US 2021/0087369 A1 · ¶ 31
Such resins may be in the form of esters of rosin acids and polyols such as pentaerythritol or glycol.
B · US 2025/0109286 A1 · ¶ 140
An empty cell means only that no passage was reproduced there.
Statements in these documents
Treads of high performance tires are expected to be safe and have outstanding traction and handling properties, wet grip, rolling resistance, and good wear characteristics.
A · US 2021/0087369 A1 · ¶ 3
The two attributes, lower rolling resistance and higher wet grip performance, are influenced by properties that generally conflict with each other.
A · US 2021/0087369 A1 · ¶ 5
It is desirable for tires to have good wet skid resistance, low rolling resistance, and good wear characteristics.
B · US 2025/0109286 A1 · ¶ 2
For year-round use, tires with treads for promoting traction on snowy and icy surfaces as well as wet traction on wet roads are desirable.
B · US 2025/0109286 A1 · ¶ 4
Cite aspatent.fyi, US 2026/0357047 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357047/, SHA-256 3654c3a6a2bd501b3e498e4404c349b2f95180d43bc3663a0a311127bfce9566