Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Polyphenylene ether matrix
What ifWhat if a crosslinked polyphenylene ether resin forms the continuous phase?
Claim language“cyclic olefin-based polymer”
Vinyl-terminated polyphenylene ether is mixed with barium titanate and alumina, then cured under heat and pressure. The crosslinked matrix retains its shape during heating, and the ceramic particles raise the effective dielectric constant.
1.1Silicone rubber particle toughening
What ifWhat if silicone rubber particles with an acrylic shell provide impact toughening?
The core-shell particles disperse in the cyclic olefin matrix during melt compounding. Under impact, the rubber cores cavitate and promote plastic deformation in the surrounding matrix, dissipating energy as a crack advances.
1.1High ceramic content sheet
What ifWhat if the filler accounts for 75% of the sheet by mass?
Claim language“35% to 70% of filler”
The blend contains 35% barium titanate, 40% rutile titanium dioxide, 20% cyclic olefin copolymer and 5% maleic anhydride grafted polyethylene by mass. Coarse and fine ceramic particle grades improve packing, and vacuum hot pressing consolidates the blend into a dielectric sheet.
1.2Rutile as the dielectric filler
What ifWhat if rutile titanium dioxide and alumina form the entire ceramic fraction?
Claim language“a titanate filler”
A cyclic olefin blend contains 30% rutile titanium dioxide and 20% alumina by mass. Rutile raises the effective dielectric constant, and alumina adds stiffness and contributes to heat conduction through the composite.
1.2Rutile content above forty percent
What ifWhat if rutile titanium dioxide accounts for 45% of the composition by mass?
Claim language“a mass percentage of the non-titanate filler ranges from 0% to 40%”
The blend contains 45% rutile titanium dioxide, 10% calcium titanate, 38% cyclic olefin copolymer and 7% ethylene-octene copolymer by mass. Melt compounding disperses both ceramics, and rutile supplies most of the ceramic volume that raises the effective dielectric constant.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Dielectric window for liquid level sensing
Mold a 2 mm window from 45 mass percent cyclic olefin polymer, 10 mass percent polyethylene, 25 mass percent calcium titanate, and 20 mass percent rutile titanium dioxide. Clamp the window against a gasket in the wall of a liquid reservoir and mount two coplanar electrodes against its dry face. An alternating voltage across the electrodes produces a fringing field through the window, and the sensing circuit measures the capacitance change as liquid covers the wetted face.
Component substitution
Calcium zirconate replaces titanate filler
Formulate the composite with 45 mass percent cyclic olefin polymer, 10 mass percent ethylene–octene copolymer, 25 mass percent calcium zirconate, and 20 mass percent rutile titanium dioxide. Calcium zirconate replaces the titanate fraction and supplies part of the dielectric response alongside the rutile particles. Melt the polymers in a twin-screw extruder, side-feed both ceramic powders into the melt, and pelletize the compound for injection molding.
Parameter or scale variation
Bimodal particle sizes at high loading
Compound 33 mass percent cyclic olefin polymer, 5 mass percent polyethylene, 35 mass percent calcium titanate, and 27 mass percent rutile titanium dioxide. Use calcium titanate with a median particle diameter of 8 to 12 µm and rutile with a median particle diameter of 0.5 to 1.0 µm. Side-feed the powders into a molten polymer blend and vacuum-vent the extruder before pelletizing. The finer rutile particles occupy gaps between the larger titanate particles when the powders are dispersed.
Thin low-filler skins on a ceramic core
Coextrude a 1.0 mm sheet with a 0.8 mm core between two 0.1 mm skins. Use 35 mass percent cyclic olefin polymer, 5 mass percent polyethylene, 35 mass percent calcium titanate, and 25 mass percent rutile titanium dioxide in the core. Use the same ingredients at 55, 10, 20, and 15 mass percent, respectively, in both skins. Bring the three molten layers together in a feedblock, pass them through a flat die, and cool the sheet on rolls so the interfaces fuse while the higher ceramic loading stays concentrated in the core.
Combination with existing systems
Dielectric loading in a patch antenna
Press a 1 mm sheet from 45 mass percent cyclic olefin polymer, 10 mass percent ethylene–octene copolymer, 30 mass percent calcium titanate, and 15 mass percent rutile titanium dioxide. Bond a rectangular copper patch to one face and a continuous copper ground plane to the opposite face, then feed the patch with a coaxial probe through a clearance hole in the ground plane. Set the patch length from the measured dielectric constant of the sheet at the target frequency and adjust the probe position to match the feed impedance.
Automated or data-driven variant
Closed-loop control of dielectric composition
Feed cyclic olefin polymer, polyethylene, calcium titanate, and rutile titanium dioxide into a twin-screw extruder using four loss-in-weight feeders set initially to 45, 10, 25, and 20 mass percent, respectively. Extrude a continuous strip through a slot die and measure its thickness and temperature before it passes through a microwave resonator. Software converts the resonant frequency shift to a dielectric constant using a calibration against molded samples and corrects the result for strip thickness and temperature. The controller adjusts the two ceramic feed rates in opposite directions to hold total filler at 45 mass percent and waits one measured transport delay before evaluating each correction.
Specific version of a part
Grafted polyethylene blend
The blend contains 45% ethylene-norbornene copolymer, 7% maleic anhydride grafted polyethylene, 28% barium titanate and 20% rutile titanium dioxide by mass. During twin-screw compounding, the grafted polyethylene provides polar functionality at the polymer-ceramic interfaces.
Ethylene octene impact modifier
A blend of 42% hydrogenated ring-opened norbornene polymer, 8% ethylene-octene copolymer and 50% ceramic powder is melt compounded and compression molded. The ethylene-octene copolymer forms dispersed rubbery domains that dissipate energy under impact.
Calcium titanate and rutile
The composition contains 25% calcium titanate and 25% rutile titanium dioxide by mass, with median particle diameters of 3 and 0.8 micrometers, respectively. The finer rutile particles occupy spaces between the coarser calcium titanate particles during consolidation.
Strontium titanate and zirconia
The composition contains 30% strontium titanate and 15% yttria-stabilized zirconia by mass. The zirconia grade has a relative permittivity above 20 at the operating frequency, and both ceramic powders are dispersed in the polymer melt before sheet extrusion.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1the resin composition comprises the following components in mass percentages: 30% to 60% of cyclic olefin-based polymer, 3% to 15% of polyolefin and/or modified polyolefin, and 35% to 70% of filler
The polymeric matrix may comprise elastomeric materials, for example urethane, silicone, or EPDM; thermoplastic polymers, for example polyethylene or polypropylene; adhesives, for example those based on ethylene-vinyl-acetate or urethane; thermoplastic elastomers; gels; thermosetting materials, for example epoxy resins; or a combination of such materials, including co-polymers, for example a combination of polyisobutylene and amorphous polypropylene.
A · US 2012/0049135 A1 · ¶ 38
A thermoplastic resin composition comprising: a base resin comprising a polycyclohexylenedimethylene terephthalate (PCT) resin; a white pigment; and inorganic fillers; a core-shell structured impact modifier, wherein the core-shell structured impact modifier has a polydimethylsiloxane rubber core; and a modified polyolefin resin, wherein the composition comprises 1 parts by weight to 10 parts by weight of the core-shell structured impact modifier and 0.1 parts by weight to 1
B · US 11,355,683 B2 · claim 1
1.2the filler comprises a titanate filler and a non-titanate filler, a mass percentage of the titanate filler ranges from 10% to 40%, a mass percentage of the non-titanate filler ranges from 0% to 40%, and a dielectric constant of the non-titanate filler is greater than 20.
The compositions and materials include a polymeric material and calcined calcium copper titanate filler material and have a reversible non-linear current-voltage characteristic.
A · US 2012/0049135 A1 · abstract
An empty cell means only that no passage was reproduced there.
Statements in these documents
The composition can be made into materials suitable for use in electrical stress control devices and surge arrester devices.
A · US 2012/0049135 A1 · ¶ 5
An advantage of at least one embodiment of the present invention is that it provides a polymeric composition and material having both a high dielectric constant and non-linear current voltage characteristics.
A · US 2012/0049135 A1 · ¶ 9
Therefore, there is a need for a thermoplastic resin composition which has excellent mechanical properties in terms of reflectance, reflectance maintenance at high temperature, and flexural strength without suffering the above problems, and can thus be used for components for light emitting diodes.
B · US 11,355,683 B2 · ¶ 7
Exemplary embodiments provide a thermoplastic resin composition that can have excellent properties in terms of reflectance, reflectance maintenance at high temperature, and/or flexural strength, and a molded article formed from the same.
B · US 11,355,683 B2 · ¶ 8
Cite aspatent.fyi, US 2026/0357049 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357049/, SHA-256 718915b5f5f2da41d33c3e4ec8dea7cfad28e814ab03998667c591199883e5da