Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Acrylic block copolymer toughening
What ifWhat if the blend uses a linear acrylic triblock copolymer as its impact modifier?
A triblock with poly(methyl methacrylate) end blocks and a poly(n-butyl acrylate) midblock disperses during melt compounding. The end blocks anchor the modifier in the rigid phase, while the rubbery midblock forms domains that promote local yielding under impact.
1.2Methacrylate homopolymer matrix
What ifWhat if poly(methyl methacrylate) homopolymer supplies the rigid matrix?
Claim language“a styrene-based copolymer”
A poly(methyl methacrylate)-rich formulation forms a continuous glassy phase around dispersed graft-rubber particles. The matrix supplies stiffness and surface hardness, while the rubber particles promote energy dissipation under impact.
1.3Factory scrap as feedstock
What ifWhat if recovered ABS comes from factory sprues and rejected moldings collected before distribution?
Claim language“post-consumer recycled ABS resin”
A granulator reduces segregated factory scrap to regrind for dosing into a melt-compounding extruder. Segregation by molding grade keeps the melt flow and rubber content of the regrind consistent across batches.
1.3Recycled acrylic feedstock
What ifWhat if recovered poly(methyl methacrylate) supplies the recycled fraction?
Claim language“post-consumer recycled ABS resin”
Sorted used acrylic sheet is granulated, dried, and melt compounded with a styrene–acrylonitrile grade selected for miscibility with poly(methyl methacrylate). The recovered acrylic contributes to the rigid phase, and the acrylate graft copolymer supplies the rubber particles for impact modification.
1.4Low recycled ABS loading
What ifWhat if post-consumer recycled ABS makes up 15% of the total blend by mass?
Claim language“20 to 70% by weight”
Gravimetric feeders meter 15 parts recycled ABS, 25 parts acrylate graft copolymer, and 60 parts styrene–acrylonitrile copolymer by mass. The styrene–acrylonitrile copolymer supplies the rigid matrix, and the acrylate graft copolymer supplies most of the impact-modifying rubber.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Molded covers for irrigation valves
The cover uses a blend of 30 wt% acrylate rubber graft copolymer with styrene and acrylonitrile, 30 wt% styrene–acrylonitrile copolymer, and 40 wt% post-consumer recycled acrylonitrile–butadiene–styrene resin. Injection molding forms a sloped top, downward-facing louvers, and mounting bosses in one piece. The top and louvers shed water while the bosses fasten the cover to the irrigation valve frame.
Component substitution
Styrene maleimide copolymer as matrix
A styrene–N-phenylmaleimide copolymer replaces the styrene–acrylonitrile copolymer as the matrix component. The feed contains 30 wt% acrylate rubber graft copolymer with styrene and acrylonitrile, 20 wt% styrene–N-phenylmaleimide copolymer, and 50 wt% post-consumer recycled acrylonitrile–butadiene–styrene resin. A twin-screw extruder disperses the graft copolymer and recycled resin in the melt, and the pelletized blend feeds an injection molding machine.
Parameter or scale variation
Compounding at two recycled resin loadings
Two formulations contain 25 and 60 wt% post-consumer recycled acrylonitrile–butadiene–styrene resin, respectively. The acrylate rubber graft copolymer with styrene and acrylonitrile stays at 25 wt%, and the styrene–acrylonitrile copolymer makes up the remaining 50 or 15 wt%. Three gravimetric feeders meter the resins into a vented twin-screw extruder for separate runs at a measured melt temperature of 230 to 245 °C.
Combination with existing systems
Coextruded sheet with a weathering cap
A sheet coextrusion line feeds a core blend of 25 wt% acrylate rubber graft copolymer with styrene and acrylonitrile, 25 wt% styrene–acrylonitrile copolymer, and 50 wt% post-consumer recycled acrylonitrile–butadiene–styrene resin through the main extruder. A second extruder feeds an acrylonitrile–styrene–acrylate cap resin to a feedblock that places the cap on one face of the core. A flat die and chill rolls form a 3 mm sheet with a nominal 0.3 mm cap, and subsequent thermoforming places the capped face on the exterior of the panel.
Injection molding over a continuous fiber insert
A preheated continuous glass fiber sheet with a styrene–acrylonitrile matrix sits against one face of an injection mold. The overmolding feed contains 30 wt% acrylate rubber graft copolymer with styrene and acrylonitrile, 25 wt% styrene–acrylonitrile copolymer, and 45 wt% post-consumer recycled acrylonitrile–butadiene–styrene resin. The injected melt fills rib and boss cavities against the insert, and molded tabs through holes in the sheet mechanically retain the insert after cooling.
Automated or data-driven variant
Feeder control from measured melt flow
A compounding line starts with 30 wt% acrylate rubber graft copolymer with styrene and acrylonitrile, 30 wt% styrene–acrylonitrile copolymer, and 40 wt% post-consumer recycled acrylonitrile–butadiene–styrene resin. A side-stream capillary rheometer measures apparent melt viscosity at fixed temperature and shear rate. The controller uses a calibration for the current resin lots to adjust the recycled resin and styrene–acrylonitrile feeder rates in opposite directions while holding the graft copolymer and total feed rates constant. The controller waits one measured extruder residence time between adjustments and limits the recycled fraction to 30 to 50 wt%.
Specific version of a part
Crosslinked butyl acrylate cores
Emulsion polymerization produces crosslinked poly(n-butyl acrylate) seed particles with a mean diameter of about 200 nm. A subsequent styrene and acrylonitrile feed forms a grafted outer phase that promotes dispersion of the rubber particles in the rigid matrix.
Bulk polymerized styrene copolymer
Continuous bulk radical polymerization produces a styrene–acrylonitrile copolymer containing 25% acrylonitrile by mass. Vacuum devolatilization removes residual monomers before pelletizing the copolymer for compounding.
Recovered appliance housing resin
Used appliance housings are disassembled, and ABS pieces are identified by infrared spectroscopy and segregated. The selected pieces are washed, granulated, dried, and melt filtered to produce recycled pellets.
Forty percent recycled ABS
Gravimetric feeders supply 40 kg of post-consumer recycled ABS, 20 kg of acrylate graft copolymer, and 40 kg of styrene–acrylonitrile copolymer per 100 kg of blend. A twin-screw extruder melt mixes the feed and discharges strands for pelletizing.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Poly(styrene-co-acrylonitrile) (SAN) copolymer forms the continuous phase and the second phase consists of dispersed butadiene, or butadiene copolymer. The butadiene particles have a layer of SAN grafted onto their surface, which makes the two phases compatible.
B · US 2023/0193018 A1 · ¶ 7
1.2a styrene-based copolymer (B); and
(14) the recycling system according to item (1) above, characterized in that the used plastic material is a plastic material salvaged from a used magnetic recording product; and (15) the recycling system according to item (14) above, characterized in that the used plastic material is a mixture of an ABS (acrylonitrile/butadiene/styrene) resin and an AS (acrylonitrile/styrene) resin or a mixture of a HIPS (high impact polystyrene) resin and a PS (polystyrene) resin.
A · US 2005/0203196 A1 · ¶ 31
Poly(styrene-co-acrylonitrile) (SAN) copolymer forms the continuous phase and the second phase consists of dispersed butadiene, or butadiene copolymer.
B · US 2023/0193018 A1 · ¶ 7
1.3a post-consumer recycled ABS resin (C),
It is also expected that for post-consumer recycled ABS, the exposure from light, elevated temperature, and chemicals during use will cause further degradation, it is believed that ABS degrades due to chain scission and crosslinking, creating oligomeric products that can migrate to the surface and brittle crosslinked polybutadiene particles.
B · US 2023/0193018 A1 · ¶ 14
1.4wherein the post-consumer recycled ABS resin (C) is comprised in an amount of 20 to 70% by weight.
The amount of the unused ABS resin (B) and/or another used ABS resin (C) added to the used ABS resin (A) may be determined as described above, but it is generally about 1 to 99% by weight, preferably about 1 to 80% by weight, further desirably about 1 to 50% by weight from the viewpoint of effective utilization of resources.
A · US 2005/0203196 A1 · ¶ 131
An empty cell means only that no passage was reproduced there.
Statements in these documents
The present invention relates to a system for recycling a used plastic material, and more particularly to a recycling system which enables revival of a physical property of a used plastic material, and quality assurance of a reclaimed plastic.
A · US 2005/0203196 A1 · ¶ 1
The reason that the above-mentioned recycling method is mainly employed in the recycling of plastics resides in that a change with time during the use of the plastic or mixing of foreign matter or heat experience during the recycling of the plastic causes the reclaimed plastic to have physical properties lowered, thus making recycling of the plastic as a material (material recycling) difficult.
A · US 2005/0203196 A1 · ¶ 8
The present disclosure relates to toy building elements made of a recycled Acrylonitrile Butadiene Styrene (ABS) material arid manufactured by processing of a. resin comprising a recycled ABS polymer.
B · US 2023/0193018 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0357051 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357051/, SHA-256 d2d81a796c850e22c74a72cdad2c20c916538bead182356bce1ebf1b19494937