What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Cyanate ester matrix

What ifWhat if a multifunctional cyanate ester forms the encapsulating matrix in place of the epoxy compound?
Claim language“an epoxy compound (A)”

A liquid blend of aromatic cyanate esters flows around the assembly under vacuum. Heating with a metal carboxylate catalyst cyclotrimerizes the cyanate groups into triazine rings and forms a rigid crosslinked network.

1.1Aromatic diamine curing

What ifWhat if a hindered aromatic diamine cures the epoxy compound in place of the acid anhydride?
Claim language“an acid anhydride (B)”

A liquid hindered aromatic diamine is mixed with a multifunctional epoxy resin at a ratio based on amine hydrogen and epoxide content. During heat cure, the amine hydrogens react with epoxide groups to form a crosslinked network.

1.1Spherical alumina filler

What ifWhat if spherical alumina particles fill the resin in place of silica?
Claim language“a silica filler (C)”

Two particle size grades of spherical alumina pack together while preserving flow during dispensing. The alumina reduces the cured composite’s thermal expansion and increases its thermal conductivity relative to the unfilled resin.

1.1Stoichiometric polyamine cure

What ifWhat if the resin uses a reactive polyamine hardener and has no separate curing accelerator?
Claim language“a curing accelerator (D)”

A liquid aliphatic polyamine and an epoxy resin are stored separately and combined in a static mixer during dispensing. The polyamine acts as the stoichiometric hardener, with its amine hydrogens consumed in epoxide ring-opening reactions that build the network.

1.2Rubbery silicone encapsulation

What ifWhat if the cured encapsulant has a glass transition temperature below room temperature and stays rubbery at its operating temperature?
Claim language“175 °C or higher”

A two-part silicone cures by platinum-catalyzed addition of silicon hydride groups to vinyl groups. The resulting elastomer remains compliant during thermal cycling and limits the mechanical stress transferred to copper conductors.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Potting for heated process probes

A room-temperature liquid epoxy formulation containing an acid anhydride, silica filler, and a curing accelerator fills the rear cavity of a heated process probe. A ceramic feedthrough separates the sensing tip from the cavity, and the resin surrounds the lead terminations behind the feedthrough. The resin cures in place, and differential scanning calorimetry on a witness sample from the same cure measures the glass transition temperature against a 175 °C minimum.

Component substitution

Zircon flour as the mineral filler

Micronized zircon flour replaces the silica filler in a room-temperature liquid blend of multifunctional epoxy, acid anhydride, and a curing accelerator. An initial formulation uses 35 volume percent zircon with a median particle diameter of 5 µm. Vacuum mixing disperses the zircon, and the blend is dispensed immediately after mixing to limit settling. A room-temperature fill test checks flow, and differential scanning calorimetry on a cured sample checks the formulation against a 175 °C glass transition target.

Phosphonium salt as the curing accelerator

Ethyltriphenylphosphonium bromide serves as the curing accelerator in a room-temperature liquid formulation of epoxy, acid anhydride, and silica filler. The salt is dissolved in a warmed portion of the anhydride, and the concentrate is cooled before it is mixed with the remaining components. Gel-time measurements at the selected cure temperature guide accelerator loading, and the mixed formulation is dispensed before gelation. Differential scanning calorimetry on cured samples checks the glass transition temperature against a 175 °C minimum.

Parameter or scale variation

Staged curing for deeper potting cavities

A room-temperature liquid epoxy, acid anhydride, silica filler, and accelerator mixture fills a 30 mm deep cavity in three 10 mm lifts. Each of the first two lifts receives a partial cure, and the next lift is poured while the preceding surface remains tacky. A thermocouple at the center of the cavity records the peak temperature during each heating cycle. A final oven cure completes crosslinking, and differential scanning calorimetry on a witness specimen checks the 175 °C glass transition target.

Combination with existing systems

Potting inside a liquid cooled inverter

A room-temperature liquid epoxy formulation with an acid anhydride, silica filler, and a curing accelerator fills the terminal compartment of a liquid-cooled inverter. A molded dam separates the potting cavity from the connector mating surfaces, and a sealed cold plate beneath the compartment circulates coolant. The resin surrounds the busbar joints and cures in place to electrically insulate them. A cured witness sample is checked for a glass transition temperature of at least 175 °C.

Automated or data-driven variant

Gravimetric feedback for two stream dispensing

One feed vessel holds the epoxy and silica filler, and a second holds the acid anhydride and compatible curing accelerator. Before each production run, the controller dispenses a calibration shot from each stream onto a load cell and adjusts pump delivery to the formulation's specified mass ratio. The streams join in a static mixer, and a load cell beneath the receiving fixture signals the controller to stop both pumps at the programmed shot mass. A witness shot follows the production cure cycle and is checked against the 175 °C glass transition target.

Specific version of a part

Liquid cycloaliphatic epoxy blend

A liquid cycloaliphatic diepoxide is blended with methylhexahydrophthalic anhydride as the hardener. A low loading of tertiary amine accelerates the heat cure, forming a crosslinked network with ester linkages.

Bimodal fused silica filler

Spherical fused silica with median particle diameters of about 3 and 20 micrometers fills the epoxy blend. The smaller particles occupy gaps between the larger particles, increasing packing density at a given solids loading.

Postcured high transition epoxy

A liquid cycloaliphatic epoxy and anhydride blend uses a multifunctional epoxy component to increase network crosslink density. A staged heat cure and postcure increase conversion, and dynamic mechanical analysis verifies a cured glass transition temperature of at least 175 °C using the loss tangent peak.

Room temperature dispensing blend

A liquid cycloaliphatic diepoxide and a liquid cyclic anhydride form the continuous phase at 23 °C. Spherical silica is dispersed under vacuum, and the filler loading is set by measuring the pressure required to dispense the blend through the potting nozzle.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2006/0089465 A1
Published
Apr 27, 2006
Filed
Apr 18, 2005
Class
C08L 63/00
Document BUS 9,748,158 B2
Published
Aug 29, 2017
Filed
Jun 23, 2016
Class
H01L 23/295
Claim 1
Document A
Document B
1.1an epoxy compound (A), an acid anhydride (B), a silica filler (C), and a curing accelerator (D)
To 200 weight portions of NBR (containing 27.1 weight % of the acrylonitrile content and 4.3 weight % of the carboxyl functional group content) were added 100 weight portions of novolac epoxy resin represented in the following chemical structure 1, 100 weight portions of phenol resin represented in the following chemical structure 2, 3 weight portions of hexamethoxy methylmelamine as hardener and 3 weight portions of phthalic anhydride, and then 10 weight portions of zinc oxi
A · US 2006/0089465 A1 · ¶ 31
A liquid sealing material comprising: (A) a liquid bisphenol epoxy resin;
B · US 9,748,158 B2 · claim 9
1.2wherein the resin composition has a glass transition temperature (Tg) of 175 °C or higher and is liquid at room temperature.
In addition, the liquid sealing materials (1) and (2) of the invention have a glass transition temperature (Tg) of 55° C. or more and are excellent in reinforcing properties of bump electrodes in a flip-chip semiconductor apparatus when used as underfill.
B · US 9,748,158 B2 · ¶ 105

An empty cell means only that no passage was reproduced there.

Statements in these documents
The present invention relates to an adhesive tape composition, and, more particularly, to an adhesive tape composition for electronic components that can be used for bonding electronic components such as FPC (Flexible Printed Circuit boards), TAB (Tape Automated Bonding), leads of lead frames, PRH (plate of radiant heat), semiconductor chips, die pads, and the like, used in semiconductor devices.
A · US 2006/0089465 A1 · ¶ 2
Accordingly, there has been a need for developing adhesive tape compositions for electronic components excellent in adhesive strength, workability and the like together with sufficient electric reliability and durability.
A · US 2006/0089465 A1 · ¶ 8
The thus configured semiconductor apparatus suffers from the following problem: When heat is applied as in temperature cycling, the bump electrodes are stressed due to a difference in coefficient of thermal expansion between the substrate made of an organic material such as epoxy resin and the semiconductor device, thus causing the bump electrodes to have defects such as cracking.
B · US 9,748,158 B2 · ¶ 4
In order to suppress the occurrence of such defects, it is widely performed to seal gaps between the semiconductor device and the substrate with a sealant called “underfill” to secure them to each other, thereby improving the thermal cycle resistance.
B · US 9,748,158 B2 · ¶ 4
Cite aspatent.fyi, US 2026/0357057 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357057/, SHA-256 b14ba2169a67e0a6a1076129eff4ce46554de2eca196497c6bf433d51a1a441f
First published
Permanent addresshttps://patent.fyi/US20260357057/
Content fingerprint (SHA-256)b14ba2169a67e0a6a1076129eff4ce46554de2eca196497c6bf433d51a1a441f
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi