1.1Chain extension of recycled polyester
What ifWhat if a difunctional epoxide replaces the BHET feed?
Dried recycled polyethylene terephthalate and a difunctional epoxide enter a vented twin-screw extruder. The epoxide groups react with carboxyl end groups on separate polyester chains, increasing molecular weight and melt viscosity before preform molding.
1.1Polycondensation with butylene terephthalate oligomers
What ifWhat if hydroxyl-terminated butylene terephthalate oligomers replace the BHET feed?
The oligomers enter a stirred melt reactor with dried recycled polyethylene terephthalate and an ester-exchange catalyst. Ester exchange incorporates butylene terephthalate units into the copolyester, and reduced pressure removes released glycols as polycondensation increases molecular weight.
1.2Crystallization control with isophthalic acid
What ifWhat if isophthalic acid supplies the comonomer units?
Claim language“polyethylene furanoate (PEF) or furandicarboxylic acid (FDCA)”
Isophthalic acid reacts with ethylene glycol in the esterification stage, and the resulting oligomers enter melt polycondensation with the terephthalate feed. Isophthalate units disrupt regular chain packing and slow crystallization during preform cooling.
1.2Gas barrier from naphthalate units
What ifWhat if dimethyl 2,6-naphthalenedicarboxylate supplies the comonomer units?
Claim language“polyethylene furanoate (PEF) or furandicarboxylic acid (FDCA)”
The diester reacts with ethylene glycol through ester exchange, and methanol leaves the reactor overhead. The resulting naphthalate units enter the terephthalate copolyester during polycondensation and restrict segmental motion, reducing gas diffusion through the container wall.
1.3Preforms from virgin polyester pellets
What ifWhat if virgin bottle-grade polyethylene terephthalate supplies the base resin?
Virgin polyethylene terephthalate pellets with an intrinsic viscosity of 0.80 dL/g are dried and metered as the main resin feed. The high-molecular-weight polyester supplies melt viscosity for injection molding, and the cooled preform is reheated for stretch blow molding.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Specific version of a part
BHET from glycolyzed bottle flakes
Washed polyethylene terephthalate flakes react with excess ethylene glycol and zinc acetate at 190–200 °C. Hot filtration removes insoluble solids, and cooling crystallizes BHET for filtration and drying.
PEF pellets for melt blending
Dried polyethylene furanoate pellets enter a twin-screw extruder with dried terephthalate polyester pellets. Kneading sections disperse the furanoate polyester through the melt, and a vacuum vent removes moisture and volatile material before pelletizing.
FDCA in the esterification feed
Finely divided 2,5-furandicarboxylic acid is mixed with ethylene glycol to form a pumpable slurry. The acid esterifies with the glycol as water is removed, and the resulting furanoate oligomers enter melt polycondensation with terephthalate oligomers.
Recycled pellets with restored viscosity
Washed bottle flakes are melt-filtered, pelletized, and crystallized. Solid-state polycondensation at 200–220 °C under dry nitrogen removes reaction byproducts and raises the intrinsic viscosity to a target of 0.80 dL/g.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
(In this process step depolymerization reaction can be carried out without using a catalyst) At the end of the depolymerization process a mixture formed of bishydroxyethylterephthalate (BHET), MEG and a coloring agent is obtained,
B · US 2023/0092877 A1 · ¶ 45
1.2polyethylene furanoate (PEF) or furandicarboxylic acid (FDCA); and
Preforms and methods of processing 2,5-furandicarboxylic acid (FDCA) polymers, such as poly(ethylene-2,5-furandicaboxylate (PEF), to produce preforms and articles, such as containers.
A · US 11,117,700 B2 · abstract
1.3recycled polyethylene terephthalate (rPET);
However the PET flakes obtained by physical recycling are not homogenous.
B · US 2023/0092877 A1 · ¶ 4
An empty cell means only that no passage was reproduced there.
Statements in these documents
As such, there remains a need for novel strategies to provide small plastic containers offering improved gas barrier properties.
A · US 11,117,700 B2 · ¶ 6
Possible applications for FDCA-based polymers include the numerous and varied current uses of polymers containing terephthalic acid (TA), for which FDCA can substitute.
A · US 11,117,700 B2 · ¶ 7
The PET flakes are taken into the extruder and are melted and the obtained molten PET is passed through a polymer filter and a cleaner and homogenous polymer is obtained.
B · US 2023/0092877 A1 · ¶ 4
In this chemical recycling method that is also called the glycolysis method, the characteristics of the final product is also dependent on inputs and color separation and purification process is not available in the related process.
B · US 2023/0092877 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0357059 A1, claim 1, first published 2026-11-20T09:31:44-05:00, https://patent.fyi/US20260357059/, SHA-256 313f2ca4ba4e10a6e2f94e1f6945803866ce7adacc943b61da6dbdd8b19ed572