United States Patent Application Publication

US 2026/0357061 A1

Published
Nov 12, 2026
Filed
Oct 2, 2023
Earliest date on the face
Oct 18, 2022
Classification
C08L 69/00
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Higher polycarbonate loading

What ifWhat if polycarbonate accounts for 75 wt. % of the finished blend?
Claim language“from 40 to 70 wt. % of a polycarbonate composition”

Melt compound 75 wt. % bisphenol A polycarbonate, 24 wt. % polybutylene terephthalate, and 1 wt. % epoxy-functional acrylic oligomer. The polycarbonate forms the continuous phase and supplies ductility, while the oligomer reacts with polyester chain ends during compounding.

1.2Single polyester viscosity grade

What ifWhat if a single intermediate-viscosity polyester grade supplies the entire polyester fraction?
Claim language“the first polyester having a higher intrinsic viscosity than the second polyester”

Use polybutylene terephthalate with an intrinsic viscosity of 0.85 dL/g measured in a phenol and tetrachloroethane solvent mixture at 25 °C. The intermediate-viscosity grade provides a single feedstock for setting melt flow, and its crystallization during cooling contributes stiffness.

1.2Higher polyester loading

What ifWhat if polyester accounts for 48 wt. % of the finished blend?
Claim language“from 10 to 40 wt. % of a polyester composition”

Compound 51 wt. % polycarbonate, 24 wt. % higher-viscosity polybutylene terephthalate, 24 wt. % lower-viscosity polybutylene terephthalate, and 1 wt. % epoxy-functional acrylic oligomer. The larger polyester fraction increases the amount of material that can crystallize during mold cooling, and the lower-viscosity grade helps the melt fill the cavity.

1.3Carbodiimide polyester end group stabilization

What ifWhat if a polymeric carbodiimide serves as the hydrolytic stabilizer?
Claim language“compound containing epoxy functional groups”

Melt compound dried polycarbonate and polyester with 0.5 to 1.5 wt. % polymeric carbodiimide. Carbodiimide groups react with polyester carboxyl end groups and reduce the concentration of acidic sites that accelerate ester hydrolysis.

1.3Higher rubber modifier loading

What ifWhat if a core-shell impact modifier accounts for 18 wt. % of the finished blend?
Claim language“from 0 to 15 wt. % of impact modifier”

Disperse 18 wt. % acrylic core-shell particles in a blend of 55 wt. % polycarbonate, 26 wt. % polyester, and 1 wt. % epoxy-functional stabilizer. Under impact, the rubber cores form small cavities that promote plastic deformation in the surrounding matrix and dissipate energy.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Bobbin flanges for wet textile processing

Injection mold removable yarn bobbin flanges from a blend containing 60 wt. % polycarbonate, 35 wt. % polyester, 2 wt. % epoxy-functional stabilizer and 3 wt. % impact modifier. Use a 40:60 mass split between higher- and lower-molecular-weight polycarbonate grades and a 50:50 mass split between higher- and lower-intrinsic-viscosity polyester grades. Mold radial ribs between the hub and rim and fit the flanges over the bobbin core with a keyed bore. The ribs stiffen the flange against yarn winding loads, and open slots between ribs let wash water drain.

Component substitution

Polyethylene terephthalate replaces both polyester grades

Use two polyethylene terephthalate grades as the polyester fraction, with intrinsic viscosities of 0.84 and 0.64 dL/g measured under the same solvent and temperature conditions. Blend the grades in equal masses to form 34 wt. % of the composition, with 62 wt. % polycarbonate and 4 wt. % epoxy-functional stabilizer. Dry the polyester and polycarbonate feeds separately and melt compound them at 265 to 275 °C. The epoxy groups react with polyester carboxyl end groups during melt mixing.

Silicone acrylic core shell impact modifier

Use 6 wt. % core-shell impact modifier with a silicone-acrylate rubber core and a poly(methyl methacrylate) shell. Combine it with 60 wt. % polycarbonate, 32 wt. % polyester divided equally between two intrinsic viscosity grades, and 2 wt. % epoxy-functional stabilizer. Feed the modifier into the molten blend through a downstream side feeder and disperse it with a short kneading section before pelletizing. The rubber cores deform under impact and promote energy dissipation through shear yielding in the surrounding matrix.

Parameter or scale variation

Short residence time for pilot compounding

Compound a blend of 63 wt. % polycarbonate, 35 wt. % polyester and 2 wt. % epoxy-functional stabilizer on a 25 mm co-rotating twin-screw extruder. Divide the polycarbonate in a 30:70 higher- to lower-molecular-weight ratio and divide the polyester equally between its higher- and lower-intrinsic-viscosity grades. Run the extruder at 250 to 350 rpm with a measured melt temperature of 250 to 265 °C and adjust feed rate to give a mean residence time of 45 to 90 seconds. Measure residence time by pulsing a pigment tracer into the feed and tracking its concentration at the die.

Combination with existing systems

Insert molded feedthrough for pump controls

Integrate the blend into a centrifugal pump control enclosure as an injection-molded electrical feedthrough flange. Use 62 wt. % polycarbonate, 34 wt. % polyester, 1 wt. % epoxy-functional stabilizer and 3 wt. % impact modifier, with a 50:50 mass split between the two polyester viscosity grades. Mold the flange around copper alloy terminals with retention notches and form a gasket groove in the mounting face. Seat an elastomer gasket in the groove and clamp the flange against the enclosure wall to seal the mounting opening.

Automated or data-driven variant

Gravimetric control of blend feed rates

Equip a twin-screw compounding line with five loss-in-weight feeders for the two polycarbonate grades, the two polyester grades and the epoxy-functional stabilizer. Program mass-flow setpoints of 20, 42, 18, 18 and 2 kg/h, respectively, with the higher-molecular-weight polycarbonate and higher-intrinsic-viscosity polyester first in their respective pairs. A controller estimates each stream's mass flow from its hopper weight trend and adjusts its feed screw speed to maintain the selected ratio. During hopper refill, the controller temporarily uses the last stable screw speed and resumes gravimetric control after the weight signal settles.

Specific version of a part

Two polycarbonate molecular weights

Use 60 wt. % total bisphenol A polycarbonate, with 30 wt. % of that fraction at a weight-average molecular weight of 32,000 g/mol and 70 wt. % at 22,000 g/mol. The higher-molecular-weight chains contribute melt strength, and the lower-molecular-weight fraction promotes flow during injection molding.

Two polyester viscosity grades

Use 30 wt. % total polybutylene terephthalate, with equal masses of grades having intrinsic viscosities of 1.00 and 0.75 dL/g under the same solvent and temperature conditions. The higher-viscosity grade contributes melt strength, and the lower-viscosity grade improves flow.

Epoxy functional acrylic stabilizer

Add 1 wt. % of an acrylic oligomer that contains pendant glycidyl groups. During melt compounding, polyester carboxyl end groups open the epoxide rings and form covalent bonds with the oligomer.

Phosphite processing stabilizer

Add 0.2 wt. % of a hindered aryl phosphite during compounding. The phosphite decomposes hydroperoxides formed during melt processing and limits oxidative degradation.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2007/0278452 A1
Published
Dec 6, 2007
Filed
Jun 6, 2006
Class
C09K 15/00
Document BUS 9,085,687 B2
Published
Jul 21, 2015
Filed
Feb 3, 2012
Class
C08L 69/00
Claim 1
Document A
Document B
1.1(A) from 40 to 70 wt. % of a polycarbonate composition comprising from 0 to 50 wt. % based on the weight of the polycarbonate composition of a first polycarbonate and from 100 to 50 wt. % of a second polycarbonate, the first polycarbonate having a higher molecular weight than the second polycarbonate;
The disclosed thermoplastic compositions generally comprise a polycarbonate component, a primary impact modifier component comprising an acrylonitrile-butadiene-styrene polymer, and at least one additional secondary impact modifier chemically different from the first acrylonitrile-butadiene-styrene component.
B · US 9,085,687 B2 · ¶ 45
1.2(B) from 10 to 40 wt. % of a polyester composition comprising from 30 to 70 wt. % based on the weight of the polyester composition of a first polyester and from 70 to 30 wt. % of a second polyester, the first polyester having a higher intrinsic viscosity than the second polyester;
Thermoplastic polyester resins suitable in the context of the present invention are characterized in that their intrinsic viscosity is at least about 0.4 and preferably about 0.6 to about 1.6 dl/gm (determined as a 1% solution in a 60:40 mixture of phenol and tetrachloroethane at 30° C.).
A · US 2007/0278452 A1 · ¶ 22
1.3(C) from 0.1 to 10 wt. % of a hydrolytic stabilizer composition comprising at least one compound containing epoxy functional groups (D) from 0 to 15 wt. % of impact modifier; and
A molding composition comprising: (i) at least one resin selected from the group consisting of polycarbonate, polyester and polyamide, (ii) a stabilizer mixture containing, A) a carbodiimide conforming to where R1-R14 independently one of the others denote a member selected from the group consisting of hydrogen, halogen, aliphatic, aromatic, cycloaliphatic and alkoxy radicals and n is 0 to 500, and B) a co-stabilizer selected from the group consisting of boehmite and pseudobo
A · US 2007/0278452 A1 · claim 17
In various aspects, the invention pertains to a process for preparing thermoplastic compositions comprising a hydrolytic stabilizer with improved electroplate adhesion, wherein the process comprises preparing a desired blend of at least one polycarbonate polymer, a first impact modifier composition, a second impact modifier composition, and adding varying amounts of, as described in the description herein, of hydrolytic stabilizer composition comprising a hydrotalcite and an
B · US 9,085,687 B2 · ¶ 124
1.4(E) from 0 to 5 wt. % of other components
The additives may be used in conventional effective amounts, preferably of from 0.01 to a total of about 30% relative to the weight of the resinous components.
A · US 2007/0278452 A1 · ¶ 54
The disclosed thermoplastic compositions can also optionally comprise one or more additives such as fillers, reinforcing agents, stabilizers, and the like, with the proviso that the additives do not adversely affect the desired properties of the polycarbonate blend compositions.
B · US 9,085,687 B2 · ¶ 125

An empty cell means only that no passage was reproduced there.

Statements in these documents
A significant disadvantage characterizing these materials is a susceptibility to deterioration upon exposure to hot water or water vapor.
A · US 2007/0278452 A1 · ¶ 2
Incorporation of carbodiimides in polyalkylene terephthalate is known to improve the resistance of this resin to hydrolysis.
A · US 2007/0278452 A1 · ¶ 3
Accordingly, there remains a need in the art for thermoplastic blends of polycarbonate and acrylonitrile-butadiene-stryrene (ABS) exhibiting improved electroplate adhesion values notwithstanding the presence of polycarbonate in the blend.
B · US 9,085,687 B2 · ¶ 5
The disclosed compositions comprise a primary and secondary impact modifier and, as such, are capable of exhibiting improved electroplate adhesion values as compared to a reference blend composition in the absence of the secondary impact modifier.
B · US 9,085,687 B2 · ¶ 6
Cite aspatent.fyi, US 2026/0357061 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357061/, SHA-256 5c49e05a408c61d90340e7401fad976156d83ff8a985216b5c52fc3d79397c6e
First published
Permanent addresshttps://patent.fyi/US20260357061/
Content fingerprint (SHA-256)5c49e05a408c61d90340e7401fad976156d83ff8a985216b5c52fc3d79397c6e