Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Covalently crosslinked polyurethane network
What ifWhat if permanent junctions in a low-glass-transition polyurethane network supply elastic recovery?
Claim language“soft and hard segmented”
An isocyanate-terminated polyether prepolymer reacts with a trifunctional polyether to form a lightly crosslinked network. Flexible chains stretch between covalent junctions and retract when the load is released.
1.1Crystalline polyester junctions
What ifWhat if a segmented copolyester supplies elastic recovery?
Claim language“polyurethanes or polyurethaneureas”
Melt polycondensation combines polyether glycol with aromatic polyester-forming reactants to produce a copolyester. Crystalline polyester domains anchor the flexible polyether segments, which extend under load and retract on unloading.
1.1Crystalline polyamide junctions
What ifWhat if a polyether block amide supplies elastic recovery?
Claim language“polyurethanes or polyurethaneureas”
Carboxyl-terminated polyamide blocks react with hydroxyl-terminated polyether blocks to form a block copolymer. Polyamide crystallites provide physical junctions, and the polyether blocks deform between those junctions.
1.1Higher hard segment content
What ifWhat if the polyurethane contains 10 wt% hard segments?
Claim language“HSWT % less than 7.8%”
A long-chain polyether diol reacts with a diisocyanate and a short diol, with feed proportions set to give 10 wt% hard segments. The hard domains anchor the elastic chains, and the polyether chains provide extension.
1.1Lower segment molecular weight ratio
What ifWhat if the soft-to-hard segment molecular weight ratio is 10?
Claim language“segment molecular weight ratio (SSMW/HSMW) larger than 12.0”
A polyurethane formulation targets nominal average molecular weights of 4,000 g/mol for soft segments and 400 g/mol for hard segments. A low-glass-transition polyether supplies chain mobility, and hydrogen bonding groups urethane-rich segments into physical junctions.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Compliant facing for acoustic panels
A segmented polyurethane with a hard-segment weight fraction below 7.8% and a soft-to-hard segment molecular weight ratio above 12.0 forms a perforated facing for a porous acoustic panel. The facing is cast as a sheet, dried, and perforated before it is clamped around the perimeter of a frame that holds an open-cell absorber. The perforations admit air motion into the absorber, where viscous losses dissipate acoustic energy.
Component substitution
Polycarbonate diol as soft segment
An aliphatic polycarbonate diol replaces the polyether glycol in a segmented polyurethane formulation. The dried diol reacts with 4,4′-methylenediphenyl diisocyanate to form an isocyanate-terminated prepolymer, which is then chain-extended with 1,4-butanediol. The formulation balances hydroxyl and isocyanate groups and sets the diol molecular weight and reactant proportions to yield a hard-segment weight fraction below 7.8% and a soft-to-hard segment molecular weight ratio above 12.0.
Parameter or scale variation
Segment targets for cast films
A solution-cast segmented polyurethane formulation targets 6.0 wt% hard segment and a soft-to-hard segment molecular weight ratio of 16.0. An adjustable blade coats the solution on a release liner, with the wet gap calibrated separately for dry film thicknesses of 50 and 150 micrometers. Staged drying removes the solvent, and a thickness gauge verifies each film before the liner is peeled away.
Continuous casting on a narrow web
A segmented polyurethaneurea solution with a hard-segment weight fraction below 7.8% and a soft-to-hard segment molecular weight ratio above 12.0 feeds a 300 mm slot die above a moving release liner. At a web speed of 0.5 m/min, a metering pump delivers 30 mL/min to lay down a nominal 200 micrometer wet film across the full width. The coated liner passes through a ventilated drying tunnel, and the dried film is wound with the liner after an exit check confirms the residual solvent level meets the process limit.
Combination with existing systems
Diaphragm for a pneumatic valve
A cast segmented polyurethane diaphragm has a hard-segment weight fraction below 7.8% and a soft-to-hard segment molecular weight ratio above 12.0. Its perimeter is clamped between the valve body and bonnet, and its center is captured between two plates attached to a spring-loaded valve stem. Pilot air pressure deflects the diaphragm to move the stem, and the spring returns the stem when the pilot chamber vents.
Automated or data-driven variant
Sensor feedback for prepolymer production
Metering pumps feed dried glycol and diisocyanate to a heated prepolymer reactor, and an inline infrared probe tracks residual isocyanate using a calibration against titration results. A controller adjusts the diisocyanate feed for subsequent batches and meters the chain extender against the measured residual isocyanate for the current batch. The recipe software uses glycol lot data and recorded reactant masses to estimate the hard-segment weight fraction and soft-to-hard segment molecular weight ratio, and flags estimates at or above 7.8% or at or below 12.0, respectively.
Specific version of a part
Polyether polyurethane with diol extension
Hydroxyl-terminated poly(tetramethylene ether) reacts with an aromatic diisocyanate and is extended with 1,4-butanediol. The formulation targets 6.0 wt% hard segments and nominal average soft and hard segment molecular weights of 6,000 and 380 g/mol, giving a ratio of about 15.8.
Polyether polyurethaneurea with diamine extension
An aromatic diisocyanate caps a long-chain polyether glycol, and ethylenediamine extends the prepolymer in solution to form urea linkages. The formulation targets 7.0 wt% hard segments and nominal average soft and hard segment molecular weights of 5,600 and 420 g/mol, giving a ratio of about 13.3.
Polyester polyurethane with diol extension
A hydroxyl-terminated copolyester made from adipic acid and mixed aliphatic diols supplies the soft segments, and an aliphatic diisocyanate and 1,4-butanediol supply the hard segments. The formulation targets 5.5 wt% hard segments and nominal average soft and hard segment molecular weights of 6,300 and 365 g/mol, giving a ratio of about 17.3.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1soft and hard segmented polyurethanes or polyurethaneureas with an HSWT % less than 7.8% and a segment molecular weight ratio (SSMW/HSMW) larger than 12.0.
The number average molecular weight of the urethane moieties, the number average molecular weight of the urea moieties, and the hard segment content of the polyurethaneurea were calculated to be 3850, 820, and 17.6%, respectively.
A · US 2014/0005348 A1 · ¶ 101
As it has been well established, segmented polyurethanes are one family of long chain polyurethanes including hard and soft segments by step polymerization of a hydroxyl-terminated polymeric glycol, a diisocyanate and a low molecular weight chain extender.
B · US 2016/0122907 A1 · ¶ 41
An empty cell means only that no passage was reproduced there.
Statements in these documents
The present invention relates to a novel elastic polyurethane fiber having a high recovery stress, a low hysteresis loss, and a high heat resistance.
A · US 2014/0005348 A1 · ¶ 1
In other words, an elastic polyurethane fiber, having a high recovery stress and a low hysteresis loss after stretch and recovery is demanded.
A · US 2014/0005348 A1 · ¶ 4
The nylon fabrics containing such spandex fibers have enhanced stretch performance and improved surface appearance after heat treatment to activate the fusing and bonding between nylon fibers and spandex fibers.
B · US 2016/0122907 A1 · ¶ 2
Accordingly, an elastomeric fiber or spandex fiber that can withstand the heat treatment under nylon fabric heat setting conditions without excessive loss of recovery power and which is capable of bonding to the nylon fiber for enhanced fabric power and appearance is still needed.
B · US 2016/0122907 A1 · ¶ 10
Cite aspatent.fyi, US 2026/0357064 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357064/, SHA-256 5c7f9d787a4da55be661508ac02393754acfcf31e31ef44cf5ce2082cecce6d3