What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Adipate polyester soft segment

What ifWhat if the first polyol were a low-glass-transition adipate polyester polyol?
Claim language“a first polyether polyol”

A hydroxyl-terminated polyester made from adipic acid and mixed glycols reacts with isocyanate to form flexible polyurethane segments. The glycol ratio limits crystallization, and the polyol blend places segmental relaxation near the foam's use temperature.

1.1Predominantly primary hydroxyl ends

What ifWhat if 90 percent of the first polyol's hydroxyl groups were primary?
Claim language“a primary hydroxyl content of 30 percent to 78 percent”

Ethylene oxide end blocks on a mixed-oxide polyether produce predominantly primary hydroxyl ends while the total ethylene oxide content stays within the specified range. A lower gelling catalyst loading offsets the faster urethane formation and gives the water–isocyanate reaction time to expand the foam.

1.2Polycarbonate diol soft segment

What ifWhat if the second polyol were an amorphous aliphatic polycarbonate diol?
Claim language“a second polyether polyol”

A mixed-diol polycarbonate with a hydroxyl number near 56 mg KOH/g reacts with isocyanate and adds flexible carbonate segments to the matrix. The first polyol supplies branching, and the polycarbonate diol fraction adjusts segmental mobility and recovery time.

1.2Mixed oxide second polyol

What ifWhat if the second polyol contained 75 wt. % propylene oxide-derived units and 25 wt. % ethylene oxide-derived units?
Claim language“90 wt. % to 100 wt. % of moieties derived from”

A mixed-oxide backbone adds ethylene oxide units that improve water compatibility. A short terminal propylene oxide block maintains predominantly secondary hydroxyl ends, and adjustment of the gelling catalyst balances network formation with gas generation.

1.3Alcohol alkoxylate cell stabilization

What ifWhat if a fatty alcohol ethoxylate–propoxylate supplied the surface activity?
Claim language“a polyether siloxane surfactant”

An alkoxylated C12–C15 alcohol adsorbs at the gas–liquid interface and reduces surface tension as carbon dioxide bubbles grow. The ethylene oxide and propylene oxide balance controls dispersibility in the polyol blend, and the gelling catalyst sets the time at which the cell walls gain strength.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Viscoelastic liners for instrument transport cases

A transport case liner uses water-blown viscoelastic polyurethane foam made from ethylene oxide-rich and propylene oxide-rich polyether polyols, a polyether siloxane surfactant, and an isocyanate. The cured foam is cut into a base pad and a lid pad, with recesses in the base pad that fit the instrument housing. The pads lightly compress when the lid closes and dissipate energy as the instrument moves under vibration.

Component substitution

Silicone surfactant with a linear architecture

A hydroxyl-free linear polyether–polydimethylsiloxane–polyether triblock replaces the silicone surfactant with pendant polyether chains. The terminal polyether blocks contain ethylene oxide and propylene oxide units and carry methyl ether end groups. The triblock is dispersed in the two-polyol blend with water before the isocyanate is added, and it stabilizes the expanding cell interfaces during the rise.

Parameter or scale variation

Slab thickness set by slicing

The two polyether polyols, polyether siloxane surfactant, and water are mixed with an isocyanate and poured into an open box with a 300 mm by 300 mm footprint. The charge is sized for a nominal free-rise height of 120 mm at the measured free-rise density. After curing, a horizontal band knife removes the surface skins and slices the core into sheets 10 mm or 25 mm thick.

Water loading below five percent

The reactive blend contains 65 wt. % ethylene oxide-rich polyether polyol, 30.5 wt. % propylene oxide-rich polyether polyol, 1 wt. % polyether siloxane surfactant, and 3.5 wt. % water. The isocyanate charge supplies 0.90 moles of isocyanate groups per mole of demand, with demand calculated as one mole per mole of hydroxyl groups plus two moles per mole of water. During free rise, the water generates carbon dioxide and the surfactant stabilizes the gas cells.

Combination with existing systems

Viscoelastic layer with powered seat ventilation

A seat cushion uses a perforated layer of the two-polyol, water-blown viscoelastic foam above a molded support pad with a recessed air plenum. An open spacer fabric sits between the foam and the perforated upholstery and distributes air across the seat surface. A centrifugal blower feeds the plenum through a duct, and the holes through the foam connect the plenum to the spacer fabric.

Automated or data-driven variant

Mass flow control for foam dispensing

Separate metering pumps feed the two polyether polyols, the polyether siloxane surfactant, and water to a premixer, and a fifth pump feeds isocyanate to the dispensing head. A controller reads mass flow meters and adjusts pump speeds to hold the selected blend fractions and the isocyanate-to-reactive-group ratio calculated from the polyol hydroxyl numbers and the water feed. The controller directs the mixed stream to a collection vessel until the measured flows stabilize within their set tolerances, then switches delivery to the mold.

Specific version of a part

Mixed oxide polyether triol

A glycerol-started polyether triol forms 65 wt. % of the isocyanate-reactive composition and contains 65 wt. % ethylene oxide-derived units. Mixed ethylene oxide and propylene oxide finishing feeds give 60 percent primary hydroxyl groups, and the chain length sets a hydroxyl number of 42 mg KOH/g.

Propylene oxide polyether triol

A glycerol-started propylene oxide polyether triol forms 30 wt. % of the isocyanate-reactive composition. Its chains terminate predominantly in secondary hydroxyl groups, with 100 wt. % propylene oxide-derived units and a hydroxyl number of 56 mg KOH/g.

Methyl capped pendant polyethers

A trimethylsiloxy-terminated dimethylsiloxane copolymer has an average of 20 dimethylsiloxane units and four pendant-bearing methylsiloxane units per chain. Each pendant contains a propyl spacer, ten ethylene oxide units and six propylene oxide units on average, and a terminal methyl ether. The surfactant forms 1.0 wt. % of the isocyanate-reactive composition.

Acetyl capped pendant polyethers

A trimethylsiloxy-terminated siloxane copolymer has an average of 30 dimethylsiloxane units and six pendant-bearing methylsiloxane units per chain. Each pendant contains a propyl spacer, twelve ethylene oxide units and eight propylene oxide units on average, and a terminal acetate ester. The surfactant forms 0.8 wt. % of the isocyanate-reactive composition.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2016/0376397 A1
Published
Dec 29, 2016
Filed
Jan 20, 2015
Class
C08G 18/4845
Document BUS 2020/0255665 A1
Published
Aug 13, 2020
Filed
Apr 12, 2017
Class
C08L 83/12
Claim 1
Document A
Document B
1.1(a) 50 to 90 weight percent (wt. %) of a first polyether polyol based on the total weight of the isocyanate reactive composition, wherein the first polyether polyol has 50 wt. % to 80 wt. % of moieties derived from ethylene oxide based on a total weight of the first polyether polyol, has a primary hydroxyl content of 30 percent to 78 percent based on a total number of hydroxyl groups in the first polyether polyol, and a hydroxyl number of 28 to 56 mg KOH/g;
Process for preparing rigid polyurethane or urethane-modified polyisocyanurate foams from polyisocyanates and polyfunctional isocyanate-reactive compounds in the presence of blowing agents wherein the polyfunctional isocyanate-reactive compounds comprise a polyether polyol having a hydroxyl number of between 50 and 650 mg KOH/g obtained by reacting a polyfunctional initiator first with ethylene oxide and subsequently with propylene oxide wherein the propoxylation degree is be
A · US 2016/0376397 A1 · abstract
1.2(b) 10 to 50 wt. % of a second polyether polyol based on the total weight of the isocyanate reactive composition, wherein the second polyether polyol has 90 wt. % to 100 wt. % of moieties derived from propylene oxide based on a total weight of the second polyether polyol, has a primary hydroxyl content of 0 percent to 40 percent based on a total number of hydroxyl groups in the second polyether polyol, and a hydroxyl number of 25 to 88 mg KOH/g;
Preferred isocyanate-reactive compounds to be used in the present invention in addition to the propylene oxide tipped ethoxylated polyether polyol are propoxylated polyethers with a functionality above 5 and an hydroxyl value above 400 mg KOH/g and aromatic polyester polyols with an hydroxyl value below 350 mg KOH/g.
A · US 2016/0376397 A1 · ¶ 38
1.3(c) 0.2 wt. % to 4.0 wt. % of a polyether siloxane surfactant, based on the total weight of the isocyanate reactive composition, of Formula (I): R1(CH3)2Si—[OSi(CH3)2]x—[OSi(CH3)(Y)]y—OSi(CH3)2R2 (Formula I)
Some representative materials are sold under the designations Niax L6100, L6900, L6917, L6887 supplied by Momentive Performance Chemicals, Dabco DC 193 supplied by Air Products, Tegostab B8534, B8461, B8490, B8476, B8460, B8486, B8466, B8484, B8470, B8487 supplied by Evonik. Typically, from about 0.5 to 5 pbw of surfactant based on isocyanate-reactive component is used.
A · US 2016/0376397 A1 · ¶ 64
The siloxane-oxyalkylene copolymer surfactants that can be used with the fatty acid esters have the general formula MDxD′yM wherein M represents (CH3)3SiO1/2 or R(CH3)2SiO1/2, D represents (CH3)2SiO2/2, D′ represents (CH3)RSiO2/2, and the value of x+y is from 50 to 220, and the ratio x/y is from 5 to 15 inclusive. In the above formulae for M and D′, R is a polyether-containing substituent.
B · US 2020/0255665 A1 · ¶ 6

An empty cell means only that no passage was reproduced there.

Statements in these documents
This invention relates to processes for the preparation of rigid polyurethane or urethane-modified polyisocyanurate foams having improved fire retardancy, to foams prepared thereby and to compositions useful in said processes.
A · US 2016/0376397 A1 · ¶ 1
Whilst well-insulated buildings are environmentally better due to energy conservation, improving the fire retardancy of said foams is often required to meet fire safety legislation.
A · US 2016/0376397 A1 · ¶ 8
The inventive surfacants are useful for making polyurethanes including polyurethane foams.
B · US 2020/0255665 A1 · ¶ 1
Moreover, flexible polyurethane slabstock foams produced with the surfactant of the present invention showed better foam heights, while maintaining finer cell structures, than foams produced with other conventional siloxane-oxyalkylene copolymer surfactants.
B · US 2020/0255665 A1 · ¶ 4
Cite aspatent.fyi, US 2026/0357065 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357065/, SHA-256 1ba3dab2a1e8f30d1ea11ff223fea0d8088019dd31a5ed0dc30514ece763da51
First published
Permanent addresshttps://patent.fyi/US20260357065/
Content fingerprint (SHA-256)1ba3dab2a1e8f30d1ea11ff223fea0d8088019dd31a5ed0dc30514ece763da51
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi