1.1Colloidal silica filler
An aqueous silica sol supplies nanoscale silicon dioxide particles and mixes with dissolved boric acid. Drying packs the particles, and baking consolidates them into an electrically insulating oxide film.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
An aqueous silica sol supplies nanoscale silicon dioxide particles and mixes with dissolved boric acid. Drying packs the particles, and baking consolidates them into an electrically insulating oxide film.
A stirred bath suspends ground gibbsite with a median particle diameter near 1 micrometer and a specific surface area of 5 to 10 square meters per gram. Roll coating deposits the suspension, and baking dehydrates the gibbsite while a borate-bearing phase binds the packed solids.
A dispersant and continuous agitation suspend submicrometer alpha alumina in the boric acid bath. Baking dehydrates the boric acid into a boron oxide phase that binds the refractory particles at their contact points.
A dilute acetic acid feed sets the bath to pH 5.0, and an adsorbed nonionic dispersant limits particle agglomeration. An inline mixer feeds the suspension to the coating rolls, and baking removes water and the organic additives while consolidating the inorganic film.
A silicone resin dissolved in an organic solvent carries the two powders as suspended solids. Flash-off and thermal curing leave a crosslinked insulating film, with resin cure controlling film formation.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Prepare an aqueous aluminum hydroxide and boric acid slurry at pH 5.8 with an aluminum hydroxide specific surface area of at least 20 m²/g. Apply a 5 to 8 µm wet layer and dry it at 110 to 130 °C until it is tack-free. Apply a second 5 to 8 µm wet layer over the first, dry it, and bake the two layers together to form the insulating film.
Circulate the aluminum hydroxide and boric acid slurry from an agitated supply tank through a flow-through pH probe with temperature compensation. Set the controller to pH 5.8 and pulse dilute aqueous ammonia into the recirculation line when the measured pH falls below 5.7. Wait one measured loop circulation time after each pulse before sampling again, and hold slurry delivery to the coater whenever the pH falls below 5.5.
A high-shear mixer disperses micronized gibbsite in water. A separate tank dissolves boric acid in warm water and feeds that solution into the stirred gibbsite dispersion.
Fine gibbsite crystallites form porous aggregates with a nitrogen adsorption specific surface area of 35 to 50 square meters per gram. Roll coating deposits the aggregates, and heat drives off bound water as the borate-bearing phase consolidates the film.
Dilute aqueous ammonia enters the stirred coating bath until a calibrated electrode reads pH 6.5 at 25 degrees Celsius. An inline pH sensor controls further ammonia additions during recirculation.
Dissolved boric acid and a metered dose of potassium hydroxide establish a boric acid and borate buffer at pH 8.5. The buffer limits pH drift as fresh slurry enters the recirculation tank.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
A second subject of the invention relates to a process for obtaining an aluminum-based filler according to the invention, comprising: (i) reacting an aqueous solution of a Brönsted base under stirring with an aqueous solution of an aluminum salt in order to precipitate the aluminum salt in a suspension of aluminum hydroxide;A · US 7,425,313 B2 · ¶ 14
A chromium-free insulation coating composition includes 100 parts by weight of a phosphate solution, 1-5 parts by weight of molybdate, 50-150 parts by weight of silica sol, 3-13 parts by weight of selenium dioxide, 1-10 parts by weight of metal oxide and/or metal hydroxide, 5-15 parts by weight of organic acid, 1-6 parts by weight of boric acid, and 100-300 parts by weight of water.B · US 10,301,480 B2 · abstract
The filler comprises an aluminum (oxide-)hydroxide corresponding, with the exception of any impurities and the water of hydration, to the general Formula I (a and b being real numbers): Al(OH)aOb, where: 0<a≦3 and b=(3−a)/2, (I) the specific BET surface area of which is between 30 and 400 m2/g, the average particle size (by mass) dw of which is between 20 and 400 nm and the disagglomeration rate, α, of which, measured via the ultrasound disagglomeration test, at 100% power ofA · US 7,425,313 B2 · ¶ 11
An empty cell means only that no passage was reproduced there.
The present invention relates to diene rubber compositions reinforced with white fillers, which can be used for the manufacture of tires or semi-finished products for tires and, in particular, tire treads.A · US 7,425,313 B2 · ¶ 3
However, it also results in an unacceptable decline in the wear resistance because these conventional white fillers do not have sufficient reinforcement ability with respect to such rubber compositions.A · US 7,425,313 B2 · ¶ 7
While if the hexavalent chromium in the coating is recovered, cost will be greatly increased.B · US 10,301,480 B2 · ¶ 3
Therefore, the prior art, in particular, the chromium-free insulation coating with good performance has yet to be improved and developed.B · US 10,301,480 B2 · ¶ 4
patent.fyi, US 2026/0357077 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357077/, SHA-256 19ac8040719615b541c0031861092a41c13a407ba4c09e39bb4fe69d8a30b272