Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Continuous stiff rib network
What ifWhat if a continuous network of stiff ribs provided the modulus contrast within the soft coating?
Claim language“hard particulate phase”
A patterned deposition step forms a connected epoxy grid, and a silicone topcoat buries the grid just below the exposed surface. Under ice loading, the silicone deflects more between ribs than over them, concentrating stress at the ice interface near the rib edges.
1.2Oil infused ceramic matrix
What ifWhat if an oil infused porous ceramic formed the continuous matrix?
Claim language“soft resin”
A sintered porous alumina layer holds silicone oil by capillary action and feeds a thin liquid film at the surface. The liquid film separates the ice from the ceramic and provides a low shear interface for release.
1.3Dry thermal particle cure
What ifWhat if dry thermal curing formed the hard polysilazane particles before blending into the coating?
Claim language“the aqueous phase in emulsion paint”
An organic polysilazane with vinyl and silicon hydride groups cross-links through platinum-catalyzed addition during heating under dry nitrogen. The cured solid is milled and classified, then dispersed into an uncured silicone matrix that deforms around the stiff particles during ice loading.
1.4Two particle size bands
What ifWhat if the hard particles occupied two distinct size bands within the soft matrix?
Claim language“uniform particle size”
Air classification separates cured particles into 5–8 μm and 15–20 μm fractions, which are blended into the same silicone paint. Both fractions create local changes in stiffness, and the larger particles perturb the stress field over a greater distance under ice loading.
1.4Ordered particle rows
What ifWhat if the hard particles occupied regularly spaced rows within the soft matrix?
Claim language“randomly distributed”
A microperforated transfer plate places individual particles at 50 μm center spacing before a silicone overcoat embeds them. Each row creates a repeating series of stress concentrations as an ice interface crack crosses it.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Coating for freezer evaporator drain pans
A sloped metal drain pan beneath a freezer evaporator carries a spray-applied coating with a soft hydrophobic resin matrix and randomly dispersed hard particles. The particles form where organic polysilazane resin cross-links at the surfaces of aqueous droplets in the paint. During a defrost cycle, warming at the pan reduces the bonded area, and the slope directs released ice fragments and meltwater toward the drain.
Coated gutters for greenhouse roofs
Removable gutter liners on sloped greenhouse roofs carry a spray-applied soft hydrophobic coating with randomly distributed hard polysilazane particles. During film formation, organic polysilazane cross-links at water droplet interfaces to create the hard phase. The modulus contrast concentrates stress near particle-bearing regions as ice bends over the discharge lip, and released ice and meltwater enter a collection trough.
Component substitution
Fluoroelastomer binder for the soft matrix
A low-hardness, peroxide-curable vinylidene fluoride copolymer forms the continuous hydrophobic matrix. A compatible solvent carries the copolymer and organic polysilazane resin, and an emulsifier stabilizes dispersed water droplets in the paint. After spraying, the polysilazane cross-links at the droplet interfaces, the solvent flashes off, and a thermal cure sets the fluoroelastomer around the randomly distributed hard particles.
Parameter or scale variation
Thicker film with smaller hard particles
The coating has a dry thickness of 80–100 μm and contains randomly distributed hard particles with diameters of 2–4 μm. Membrane emulsification controls the water droplet size before spraying, and expansion or shrinkage during cure is accounted for by adjusting the membrane pore size against measured dry particle diameters. A traversing spray gun builds the film with overlapping passes while the preceding pass is still wet, and interfacial cross-linking fixes the particle distribution within the soft matrix.
Combination with existing systems
Particle filled coating over foil heaters
An etched resistive foil heater sits beneath an electrically insulating outer skin, and the particle-filled hydrophobic coating covers the exposed face of the skin. The outer coating contains hard particles formed by organic polysilazane cross-linking at aqueous droplet interfaces. A temperature controller pulses the heater to warm the ice–coating interface, and gravity or airflow loads the ice as debonding propagates across the coated surface.
Automated or data-driven variant
Image feedback for emulsion droplet sizing
Metering pumps feed the water phase and the soft resin phase containing organic polysilazane into a variable-speed inline mixer. A flow-cell microscope just upstream of the spray gun measures droplet size, and a controller adjusts mixer speed to hold a target median diameter of 10 μm. The gun deposits the emulsion, and cross-linking at the droplet interfaces forms hard particles that remain randomly distributed as the matrix cures.
Specific version of a part
Silicone with silazane particles
A hydrophobic silicone matrix surrounds densely cross-linked silazane particles in a dry film about 50 μm thick. The silicone deforms under ice loading, while the harder inclusions produce local stress concentrations near the ice interface.
Low modulus silicone resin
A vinyl-terminated silicone resin cures with a multifunctional silicon hydride cross-linker to form a hydrophobic elastomer. Long silicone chains between cross-links give the continuous matrix a low modulus.
Aqueous cure of silazane droplets
High-shear mixing disperses organic polysilazane droplets in the aqueous phase of the paint emulsion. Water reacts at the droplet interfaces, and hydrolysis and condensation build a densely cross-linked network that hardens each droplet.
Narrow droplet size distribution
Membrane emulsification meters organic polysilazane into droplets sized to yield cured particles near 10 μm. Interfacial cross-linking hardens the droplets, and gentle mixing maintains their random dispersion until the soft matrix sets.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1soft and hydrophobic coating matrix and hard particulate phase with high cross-linking density within the coating
1.2wherein the soft and hydrophobic coating matrix is soft resin
1.3the hard particulate phase with high cross-linking density within the coating is formed by a cross-linking reaction between organic polysilazane resin (OPSZ) and the aqueous phase in emulsion paint
The excess organic solvent is then removed and a surfactant, a monomer, an initiator and a cross-linker are added to form an activated seed particle in an aqueous vehicle. The monomer, initiator and cross-linker diffuse into the activated seed particles to form an aqueous dispersion of swollen seed particles, which initiates the polymerisation of the monomer and cross-linker in the swollen seed particles.
A · US 2022/0403084 A1 · ¶ 5
D7 (20 mg, 5% wt. related to oil phase) was dissolved in 3.6 mL of deionized water (aqueous phase, 90% wt.) in a 8 mL glass vial, to this solution 0.4 g of fish oil (oil phase, 10% wt.) were added.
B · US 12,427,109 B2 · ¶ 315
1.4the hard particle phase generated by the cross-linking reaction has uniform particle size and is randomly distributed within the soft and hydrophobic coating matrix.
In an embodiment of the invention, highly monodisperse polystyrene particles (or polystyrene beads) having a particle size of from 100 to 370 nm are prepared via a one-pot synthesis involving water as the sole solvent, styrene monomers 40, and a hydrophilic macroradical 100 formed by mixing a water-soluble initiator 20 and hydrophilic polymer stabilizer 30, as depicted in the schematic representation of FIG. 1.
A · US 2022/0403084 A1 · ¶ 165
An empty cell means only that no passage was reproduced there.
Statements in these documents
This invention relates to highly monodisperse polymer particles useful in biological assays and other applications.
A · US 2022/0403084 A1 · ¶ 1
For immunodiagnostic applications, the diameter of the particles is required to be about half of the visible light wavelength, which is around 100 nm to 370 nm, and the monodispersity (in terms of coefficient of variation) is preferably below 5%.
A · US 2022/0403084 A1 · ¶ 3
Therefore, from what is known in the art, it is derived that there is still the need of providing an efficient polysaccharide-based emulsion stabilizer useful in biomedical applications.
B · US 12,427,109 B2 · ¶ 7
In particular, the inventors have surprisingly found that polysaccharides modified by the introduction of methacrylate or acrylate groups which have a surface tension equal to or lower than 63 mN/m have the appropriate amphiphilic nature for being use as oil-in water emulsion stabilizers with esterase enzyme response.
B · US 12,427,109 B2 · ¶ 8
Cite aspatent.fyi, US 2026/0357084 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357084/, SHA-256 40112758f4e5dd7a84ee72e15c75627cdb45710f26109bd58c453a302d64479e