patent.fyi
Applications  /  US 2026/0357088
United States Patent Application Publication

US 2026/0357088 A1

Published
Nov 12, 2026
Filed
Jun 25, 2026
Earliest date on the face
May 29, 2020
Classification
C09D 5/29
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Cholesteric liquid crystal reflector

What ifWhat if a cholesteric liquid crystal provides the temperature response?
Claim language“vanadium (IV) oxide”

Cholesteric liquid crystal domains sit in a transparent polymer binder. Temperature changes the helical pitch of the liquid crystal and shifts the wavelength band that the domains reflect.

1.1Micrometer thick particle coating

What ifWhat if the thermochromic coating is 5 micrometers thick?
Claim language“between 50 nm and 500 nm thickness”

A drawdown bar deposits a dilute dispersion of vanadium (IV) oxide nanoparticles in an acrylic binder, and drying forms a 5 micrometer film. Low particle loading limits visible absorption, while the particles change near-infrared transmission as they heat through their phase transition.

1.1Lower visible transmission glazing

What ifWhat if the thermochromic layer has a visible light transmission of 45%?
Claim language“and Tvis≥60%”

A neutral gray pigment dispersed in the coating binder sets the visible light transmission to 45%. Vanadium (IV) oxide particles in the same binder regulate near-infrared transmission as their temperature changes.

1.2Reflected color difference metric

What ifWhat if the temperature response is reported as a reflected color difference?
Claim language“% visible light transmission”

A reflectance spectrophotometer records the coating on an opaque panel at 25 °C and 80 °C under the same illumination and viewing geometry. The difference between the two sets of lightness and chromaticity coordinates quantifies the visible change on heating.

1.2Single wavelength transmission change

What ifWhat if the switching response is reported as the transmission change at 1,550 nm?
Claim language“% solar modulation”

A narrowband infrared source illuminates the coating, and a photodiode measures transmitted power at 25 °C and 90 °C. The difference between the normalized readings gives the transmission change in percentage points at 1,550 nm.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Thermochromic glazing for greenhouse roofs

A single 200 nm layer containing vanadium (IV) oxide particles in a transparent silica binder coats the interior face of a glass greenhouse roof panel. When sunlight warms the panel through the oxide transition, the layer transmits less near-infrared radiation. Panel qualification uses visible transmission and solar modulation measured through the coated glass, with a separate measurement of photosynthetically active radiation for crop lighting.

Component substitution

Tungsten substituted vanadium oxide coating

A tungsten-substituted vanadium dioxide solid solution replaces the vanadium (IV) oxide as the active particulate material. The particles contain tungsten at 1 atomic percent of the metal sites and disperse in a transparent silica binder to form a single 200 nm dry layer on glass. Tungsten substitution lowers the transition temperature, and a heating and cooling scan of the coated glass measures the resulting transition and solar modulation.

Parameter or scale variation

Thickness series for optical tuning

A series of glass coupons carries single layers of the same vanadium (IV) oxide and silica formulation at dry thicknesses of 100, 200, 300, and 400 nm. A variable-gap applicator sets the wet thickness, and step-height profilometry verifies the dry thickness after cure. Spectral transmission measurements at 25 °C and 90 °C provide the visible transmission and the difference in solar-weighted transmission in percentage points. The selected thickness gives the highest product of those two values among coupons with visible transmission of at least 60% and a product greater than 600.

Combination with existing systems

Thermochromic layer in insulated glazing

A single 200 nm vanadium (IV) oxide composite layer coats the cavity-facing surface of the outer pane of a double-pane insulating glass unit. A sealed gas gap separates the coated pane from an inner pane that carries a low-emissivity film on its cavity-facing surface. The thermochromic layer reduces near-infrared transmission when the outer pane heats, and the low-emissivity film reduces long-wave radiative exchange across the gap. Hot and cold transmission measurements through the assembled unit quantify the combined optical response.

Automated or data-driven variant

Sensor controlled two stage curing

A programmable chamber cures a glass-supported vanadium (IV) oxide and silica precursor film in two stages under separate oxygen setpoints. An oxygen analyzer measures the chamber atmosphere, and a controller adjusts the nitrogen and oxygen flows through mass-flow controllers. The controller starts each timed hold after chamber oxygen and substrate temperature enter their programmed bands, and it records both signals throughout the hold. Post-cure hot and cold transmission measurements link the recorded cure conditions to visible transmission and solar modulation.

Optical feedback for continuous coating

A slot die deposits a vanadium (IV) oxide particle dispersion in a transparent binder onto a moving transparent polymer web, and a dryer forms a single layer. A downstream spectral reflectometer estimates dry thickness using calibration coupons, and a controller adjusts the feed pump to maintain a 250 nm setpoint at the current web speed. A thinned film increases the commanded feed rate, and a thickened film decreases it. Hot and cold spectral transmission measurements on finished web samples verify visible transmission and solar modulation.

Specific version of a part

Separate optical and switching layers

A sputtered vanadium (IV) oxide film changes near-infrared transmission across its phase transition. Silicon dioxide layers above and below the film reduce visible reflection through thin-film interference.

Sputtered oxide on glass

Reactive sputtering deposits a single 60 nm vanadium oxide film on glass, and a controlled oxygen anneal forms the vanadium (IV) oxide phase. Visible and solar transmission measurements verify at least 60% visible transmission and a product of visible transmission and solar modulation greater than 600 using percentage values.

Oxide particles in silica

A bar coater applies a dispersion of vanadium (IV) oxide nanocrystals in a silica sol, which dries to a single 350 nm layer on glass. Particle loading sets the optical density, and transmission measurements verify at least 60% visible transmission and a product of visible transmission and solar modulation greater than 600 using percentage values.

Photopic weighted visible transmission

A spectrophotometer measures transmission from 380 nm to 780 nm. Integration against the daylight spectrum and the photopic sensitivity curve gives the percentage of incident visible light transmitted, weighted for human vision.

Solar weighted transmission difference

A temperature-controlled spectrophotometer records transmission from 300 nm to 2,500 nm at 25 °C and 90 °C. Each spectrum is weighted by the same incident solar irradiance spectrum, and the cold value minus the hot value gives solar modulation in percentage points.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 6,933,553 B2
Published
Aug 23, 2005
Filed
Dec 30, 2003
Document BUS 2013/0164511 A1
Published
Jun 27, 2013
Filed
Dec 21, 2012
Class
C09D 1/00
Claim 1
Document A
Document B
1.1vanadium (IV) oxide and exhibiting SSFcoating=Tvis*ΔTsol>600 and Tvis≥60% when applied as a single layer of between 50 nm and 500 nm thickness
Referring to FIGS. 1 through 3, a vanadium dioxide (VO2) thin film 120 having a thickness of about 700-1000 Å and having a square pattern with an area of several μm is disposed on a single crystal sapphire (Al2O3) substrate 110.
A · US 6,933,553 B2 · ¶ 27
FIG. 4 is a graph depicting the transmittances of a vanadium dioxide (VO2) thin film, a photochromic thin film, and a multilayer film, which includes a VO2 thin film and a photochromic thin film stacked on the VO2 thin film, according to an embodiment of the invention; and
B · US 2013/0164511 A1 · ¶ 27
1.2wherein Tvis is the % visible light transmission and ΔTsol is the % solar modulation.
The transition of the VO2 thin film 300 occurs at a predetermined temperature, at which the crystalline structure of VO2 changes due to the thermochromic phenomenon, so that the physical properties (electrical conductivity and infrared radiation transmittance) of the VO2 thin film drastically change. As a result, the VO2 thin film 300 blocks near IR radiation and IR radiation while allowing visible light to pass through.
B · US 2013/0164511 A1 · ¶ 37

An empty cell means only that no passage was reproduced there.

Statements in these documents
Therefore, when Mott-Hubbard field effect transistors are applied to ultra-small devices, they suffer a problem in that the amount of current decreases due to reduction in the area of devices.
A · US 6,933,553 B2 · ¶ 7
The present invention provides a field effect transistor which induces a sharp metal-insulator transition by adding low-density holes to a vanadium dioxide thin film to control a large current even in devices having small areas.
A · US 6,933,553 B2 · ¶ 8
The application of smart windows to vehicles or buildings may be very effective in saving energy.
B · US 2013/0164511 A1 · ¶ 6
However, as a drawback, when the thermochromic glass is applied to the construction industry, the thermochromic glass using the VO2 thin film is not compliant with consumers' demands, since consumers prefer greenish, bluish or grayish colors.
B · US 2013/0164511 A1 · ¶ 10
Cite aspatent.fyi, US 2026/0357088 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357088/, SHA-256 15843418a8ce5cc09a63f8977f1272a81e2d34bfe7d70905fb2c169a9f81d938
First published
Permanent addresshttps://patent.fyi/US20260357088/
Content fingerprint (SHA-256)15843418a8ce5cc09a63f8977f1272a81e2d34bfe7d70905fb2c169a9f81d938
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi