US 2026/0357098 A1

Published
Nov 12, 2026
Filed
Oct 30, 2023
Earliest date on the face
Oct 31, 2022
Classification
C09D 123/12
First published here
Nov 20, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Covalent coupling through chain ends

What ifWhat if terminal epoxide groups on polypropylene coupled the coating to the filament through covalent bonds?
Claim language“a side chain compound capable of forming hydrogen bond”

An amino-functional silane attaches to surface hydroxyl groups on the glass through siloxane bonds. During melt coating, surface amines open epoxide rings at the polypropylene chain ends and form covalent links across the interface.

1.3Polypropylene wax for melt flow

What ifWhat if a low molecular weight polypropylene wax served as the melt-flow additive?
Claim language“a low molecular weight polyethylene”

The coating compound contains 2 wt % polypropylene wax dispersed in the polypropylene matrix. At the coating temperature, the wax melts and lowers the compound's melt viscosity, which helps the melt spread around the filament in the die.

1.4Polypropylene and elastomer blend

What ifWhat if grafted and non-grafted polypropylene together made up 75 wt % of the coating composition?
Claim language“at least 90 wt %”

The blend contains 70 wt % non-grafted polypropylene, 5 wt % maleic anhydride-grafted polypropylene, 23 wt % ethylene-octene elastomer, and 2 wt % polyethylene wax. The grafted polypropylene supplies polar groups at the glass interface, while the dispersed elastomer absorbs strain during bending.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Reinforcement for irrigation valve housings

A polypropylene irrigation valve housing contains chopped glass filaments with a polypropylene coating applied directly to each filament. The coating contains grafted polypropylene with hydrogen-bonding side groups and 2 wt % polyethylene with a number-average molecular weight of 3000 g/mol. A twin-screw extruder incorporates the chopped filaments into polypropylene pellets that feed an injection molding machine. The molded housing uses the filaments to stiffen the walls around the threaded ports.

Parameter or scale variation

Two coating thicknesses on glass

Individual glass filaments with a diameter of 17 µm receive radial coating thicknesses of 2 µm or 8 µm on separate reels. A metering pump supplies a blend of 98 wt % grafted polypropylene bearing hydrogen-bonding groups and 2 wt % polyethylene with a number-average molecular weight of 3000 g/mol to a crosshead die. The line adjusts melt delivery at a fixed take-up speed to produce outside diameters of 21 µm and 33 µm after cooling. An optical microscope measures polished cross sections to verify coating thickness and concentricity.

Combination with existing systems

Coated filaments in tape consolidation

A continuous tape line draws directly coated glass filaments from multiple reels and aligns them side by side with a comb guide. Each filament carries a coating of 98 wt % grafted polypropylene bearing hydrogen-bonding groups and 2 wt % polyethylene with a number-average molecular weight of 3000 g/mol. The line feeds the aligned filaments between two polypropylene films into a heated double-belt press. The press melts the films and coatings together under pressure and cools the consolidated tape before winding.

Automated or data-driven variant

Closed-loop control of coating thickness

A gear pump meters a coating blend of grafted polypropylene bearing hydrogen-bonding groups and 2 wt % polyethylene with a number-average molecular weight of 3000 g/mol into a die that applies the blend directly to a moving glass filament. An upstream optical gauge measures the bare filament diameter, and a downstream gauge measures the coated diameter after cooling. A controller aligns the measurements using line speed and calculates mean radial coating thickness as half the diameter difference. The controller trims pump speed to hold the thickness setpoint and flags readings outside the specified tolerance.

Component substitution

Basalt filament in polypropylene coating

A continuous melt-drawn basalt filament replaces the glass filament as the reinforcement core. A crosshead die applies a coating of 98 wt % maleic anhydride-grafted polypropylene and 2 wt % polyethylene with a number-average molecular weight of 3000 g/mol directly to the dried, unsized basalt surface. Polar groups on the grafted polypropylene interact with hydroxyl groups on the basalt surface. A cooling stage solidifies the coating before the filament is wound onto a reel.

Specific version of a part

Mechanical anchoring with surface texture

A thin layer of silica particles bonded to the glass creates recesses beneath projecting particle edges. The coating die presses molten polypropylene into the recesses, and the cooled polymer keys into the texture.

Acrylic acid grafted polypropylene

A peroxide initiator drives acrylic acid grafting onto polypropylene during reactive extrusion. The resulting pendant carboxylic acid groups form hydrogen bonds with hydroxyl groups on the glass surface.

Polypropylene with fatty amide

A twin-screw extruder disperses 0.5 wt % stearamide in non-grafted isotactic polypropylene. The stearamide carries an amide group that forms hydrogen bonds with surface hydroxyl groups where the additive contacts the glass.

Polyethylene wax at two percent

The coating compound contains 2 wt % polyethylene wax with a number average molecular weight of 2500 g/mol. The wax melts during compounding and reduces melt viscosity during filament coating.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2020/0148879 A1
Published
May 14, 2020
Filed
Nov 12, 2019
Class
C08L 67/02
Document BUS 2021/0009865 A1
Published
Jan 14, 2021
Filed
Mar 1, 2019
Class
C09J 123/26
Claim 1
Document A
Document B
1.1A) a grafted polypropylene grafted with C1) a side chain compound capable of forming hydrogen bond and/or
A wall for a package comprising a composition wherein the composition comprises: a polyester base polymer; a polyolefin polymer; a functionalized polyolefin polymer selected from the group consisting of a maleic anhdride-grafted polypropylene, a maleic anhydride-grafted polypropylene adhesive resin, an acrylic acid-grafted polyproylene, a maleic anhydride-grafted styrene-ethylene-butylene-styrene copolymer, an ethylene-butyl acrylate-maleic anhydride terpolymer, an ethylene-b
A · US 2020/0148879 A1 · abstract
The modified polypropylene-based resin (A) is a resin having a portion derived from an unmodified polypropylene-based resin (D) and a grafted portion derived from a modifying agent, and is preferably obtained by graft-polymerizing the modifying agent including an α,β-unsaturated carboxylic acid or derivative thereof in the presence of the unmodified polypropylene-based resin (D).
B · US 2021/0009865 A1 · ¶ 40
1.2B) a non-grafted polypropylene and C2) a compound capable of forming hydrogen bond,
In the following examples, various compositions of PET resin blends with varying amounts of a polypropylene resin, a polyether-PET copolymer based OS additive, and/or transition metal catalyst were fabricated into monolayer bottles via a 2-step process.
A · US 2020/0148879 A1 · ¶ 101
Provided is an adhesive composition that is characterized by containing a modified polypropylene-based resin (A), an epoxy resin (B) and an unmodified polypropylene-based resin (C), with the modified polypropylene-based resin (A) being a resin obtained by graft modifying an unmodified polypropylene-based resin (D) with a modifying agent that contains an α,β-unsaturated carboxylic acid or a derivative thereof, the content of the modified polypropylene-based resin (A) being 10
B · US 2021/0009865 A1 · abstract
1.3wherein the polypropylene composition comprises D) a low molecular weight polyethylene having number average molecular weight of at most 5000 g/mol in an amount of less than 10 wt % with respect to the polypropylene composition,
1.4wherein the total amount of A) and B) with respect to the polypropylene composition is at least 90 wt %.
In the adhesive composition according to the present invention, the total content of the modified polypropylene-based resin (A) and the unmodified polypropylene-based resin (C) is preferably 50 parts by mass or more, and more preferably 60 parts by mass or more relative to 100 parts by mass of the solid content of the adhesive composition.
B · US 2021/0009865 A1 · ¶ 71

An empty cell means only that no passage was reproduced there.

Statements in these documents
In particular, the present invention relates to stretch-blow-molded opaque polyester containers that have superior barrier properties for oxygen, carbon dioxide, and visible light.
A · US 2020/0148879 A1 · ¶ 2
Dairy products such as milk or even non-dairy products such as soy milk are not only sensitive to oxygen but also light.
A · US 2020/0148879 A1 · ¶ 4
In further detail, it relates to an adhesive composition and a laminate having an adhesive layer suitable for use in bonding electronic parts and the like, particularly for manufacturing products related to flexible printed circuits (hereinafter often referred to as “FPC”).
B · US 2021/0009865 A1 · ¶ 1
Accordingly, with the increase in signal speed and signal frequency, the adhesive for use in FPC-related products must satisfy dielectric properties that can withstand use in high frequency region (low dielectric constant and low dielectric loss tangent).
B · US 2021/0009865 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0357098 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357098/, SHA-256 cd697550b9ff96eb27c74d4ab2b50cb0bd415c7d4644ebe4efd65e61c10bbaef
First published
Permanent addresshttps://patent.fyi/US20260357098/
Content fingerprint (SHA-256)cd697550b9ff96eb27c74d4ab2b50cb0bd415c7d4644ebe4efd65e61c10bbaef