Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Three terminal acrylate groups

What ifWhat if compound A has three terminal acrylate groups per molecule?
Claim language“having at most two (meth)acrylate groups”

Grow trimethylene ether arms from a glycerol core and esterify the three terminal hydroxyl groups with acrylic acid. During ultraviolet exposure, radicals add to the terminal acrylates and tie the three arms into the cured network.

1.1Longer polyether precursor chains

What ifWhat if the glycol precursor has a number average molecular weight of 1,000 g/mol?
Claim language“from 350 to 600 g/mol”

Esterify the terminal hydroxyl groups of the 1,000 g/mol glycol with acrylic acid to produce a difunctional polyether acrylate. Blend it with the unsaturated oligomer and a radical photoinitiator so ultraviolet exposure incorporates the longer polyether chains into the film network.

1.2Lower viscosity reactive oligomer

What ifWhat if compound B has a viscosity of 2 Pa s at 25 °C?
Claim language“a viscosity at 25 °C of more than 5 Pa s”

Use a short aliphatic polyester diacrylate with a neat viscosity of 2 Pa s at 25 °C. The oligomer flows during coating application, and its terminal acrylates copolymerize with compound A during ultraviolet exposure.

1.2Cationically cured epoxy oligomer

What ifWhat if the second oligomer is an epoxide-terminated polyether with saturated end groups?
Claim language“an ethylenically unsaturated oligomer compound B”

Blend the epoxide-terminated polyether with compound A, a radical photoinitiator, and a photoacid generator. Ultraviolet exposure initiates acrylate polymerization and epoxide ring opening, forming interlaced polymer networks in the film.

1.3Waterborne coating viscosity control

What ifWhat if water supplies the viscosity reduction for coating application?
Claim language“a low molecular weight ethylenically unsaturated monomer compound C”

Disperse compounds A and B in water using a nonionic surfactant and adjust the water content to set the application viscosity. Evaporate the water from the applied layer and expose the coalesced film to ultraviolet light to cure the acrylates.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Clear coating for decorative paper

The coating contains 55 wt % biobased poly(trimethylene ether) diacrylate made from a glycol with a number average molecular weight of 500 g/mol, 42 wt % urethane acrylate oligomer with a viscosity above 5 Pa·s at 25 °C, and 3 wt % ultraviolet photoinitiator. A reverse gravure roll applies the mixture to sealed, printed decorative paper at a wet thickness of 8 to 12 µm. A nitrogen-shrouded ultraviolet lamp cures the wet layer into a clear wear surface over the print.

Component substitution

Polycaprolactone diacrylate as reactive diluent

Polycaprolactone diacrylate made from a polycaprolactone diol with a number average molecular weight of 530 g/mol replaces the poly(trimethylene ether) diacrylate at 40 wt % of the formulation. A urethane acrylate oligomer with a viscosity above 5 Pa·s at 25 °C supplies 57 wt %, and a phosphine oxide photoinitiator supplies 3 wt %. The mixture is blended at 40 °C, applied with a drawdown bar, and exposed to ultraviolet radiation to copolymerize the acrylate groups.

Parameter or scale variation

Two stage ultraviolet exposure schedule

A blend of biobased poly(trimethylene ether) diacrylate, a urethane acrylate oligomer with a viscosity above 5 Pa·s at 25 °C, and a phosphine oxide photoinitiator is cast at a wet thickness of 25 µm. A first 395 nm lamp delivers 75 mJ/cm² at the coating plane to partially gel the film. A second 395 nm lamp delivers 750 mJ/cm² under nitrogen within 5 seconds of the first exposure to complete the cure.

Combination with existing systems

Extrusion line with inline coating

A flat-die extrusion line forms a rigid thermoplastic sheet, and chill rolls support and cool the sheet before it passes through a corona treatment station. A downstream roll coater applies a blend of biobased poly(trimethylene ether) diacrylate, a urethane acrylate oligomer with a viscosity above 5 Pa·s at 25 °C, and an ultraviolet photoinitiator. A shielded ultraviolet station cures the coating on the moving sheet before a crosscut saw cuts the sheet to length.

Microtexture replication with a transparent belt

A roll coater deposits a mixture of biobased poly(trimethylene ether) diacrylate, a urethane acrylate oligomer with a viscosity above 5 Pa·s at 25 °C, and an ultraviolet photoinitiator onto a moving film. A nip presses the wet coating against an ultraviolet-transparent embossing belt bearing an inverse surface texture. A lamp exposes the coating through the belt while the resin fills the texture, and a peel roll separates the belt from the cured film.

Automated or data-driven variant

Closed loop wet film thickness control

A gear pump feeds a slot die with a blend of biobased poly(trimethylene ether) diacrylate, an ethylenically unsaturated oligomer with a viscosity above 5 Pa·s at 25 °C, and an ultraviolet photoinitiator. A spectral reflectance gauge between the die and the curing station calculates wet thickness from reflections at the air–coating and coating–substrate interfaces using a calibrated optical model. The controller uses web speed and target thickness to set pump flow, then trims pump speed from the measured thickness error before the film reaches the ultraviolet station.

Specific version of a part

Biobased polyether terminal diacrylate

Esterify both terminal hydroxyl groups of a biobased poly(trimethylene ether) glycol with acrylic acid and remove the water formed during esterification. Use a glycol with a number average molecular weight of 500 g/mol and incorporate the resulting diacrylate at 40 wt % of the total coating.

Viscous aliphatic urethane diacrylate

React a polyester diol with an aliphatic diisocyanate and cap the terminal isocyanate groups with hydroxyethyl acrylate. Use the resulting urethane diacrylate at 55 wt % of the total coating and select an oligomer with a neat viscosity of 20 Pa s at 25 °C.

Isobornyl acrylate reactive diluent

Add 4 wt % isobornyl acrylate to reduce the viscosity of the uncured blend. Its single acrylate group copolymerizes with the acrylate groups of the other components during ultraviolet exposure.

Saturated polyester film modifier

Dissolve 5 wt % of an adipate polyester prepared from adipic acid and neopentyl glycol in the reactive blend. The polyester increases the uncured film viscosity and remains physically dispersed in the cured network.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2012/0004340 A1
Published
Jan 5, 2012
Filed
Sep 14, 2011
Class
C09D 175/16
Document BUS 2016/0168413 A1
Published
Jun 16, 2016
Filed
Dec 15, 2014
Class
C09D 133/12
Claim 1
Document A
Document B
1.1from 10 wt % to 90 wt %, based on the total weight of the coating composition, of a poly(trimethylene ether) (meth)acrylate compound A having at most two (meth)acrylate groups obtainable by a condensation reaction of biobased 1,3 poly(trimethylene ether) glycol and an (meth)acrylate compound selected from the group consisting of (meth)acrylic acid, (meth)acryloyl chloride, and/or alkylesters thereof, wherein the biobased 1,3 poly(trimethylene ether) glycol has a number average molecular weight Mn of from 350 to 600 g/mol, more preferably from 400 to 550 g/mol;
Acrylated polyether oligomers, useful in the present invention, have at least two or more acryloyl or methacryloyl groups and a polyether core.
A · US 2012/0004340 A1 · ¶ 14
1.2from 10 wt % and 89.99 wt %, based on the total weight of the coating composition, of an ethylenically unsaturated oligomer compound B different from compound A, wherein compound B has a viscosity at 25 °C of more than 5 Pa s;
In certain other embodiments the gel is comprised of 60-70% by weight an aliphatic polyester based urethane diacrylate oligomer, 5-10% by weight 2-hydroxyethyl methacrylate (HEMA), 5-10% by weight isobornyl methacrylate, and up to 1% by weight hydroxycyclohexyl phenyl ketone.
A · US 2012/0004340 A1 · ¶ 21
1.3optionally, a low molecular weight ethylenically unsaturated monomer compound C;
The method of claim 1 wherein the gel composition comprises monomer selected from hydroxyethyl (meth)acrylate, hydroxypropyl (meth)acrylate, trimethylolpropane tri (meth)acrylate, and isobornyl (meth)acrylate.
A · US 2012/0004340 A1 · claim 12
The reactive diluent has at least one ethylenically unsaturated functional group, no additional functionality, and a boiling point of greater than 100° C.
B · US 2016/0168413 A1 · abstract
1.4optionally, a further compound D which is a polymer without a reactive ethylenically unsaturated group.
The organic liquid may also comprise non-reactive polymer, filler, and dispersant. For example, the organic liquid may comprise as non-reactive polymers nitrocellulose, cellulose acetate propionate, cellulose acetate butyrate, and similar cellulose-based polymers and other synthetic non-reactive polymers, with or without solvent.
A · US 2012/0004340 A1 · ¶ 22
Suitable epoxy-functional polymers can be saturated or unsaturated, cyclic or acyclic, aliphatic, alicyclic, aromatic or heterocyclic.
B · US 2016/0168413 A1 · ¶ 64

An empty cell means only that no passage was reproduced there.

Statements in these documents
It has been a long felt need in this art to provide integrally colored artificial nails which have a reproducible, predictable color when cured.
A · US 2012/0004340 A1 · ¶ 7
There is also a need for an improved method to produce color containing UV-curable gels which give high color density.
A · US 2012/0004340 A1 · ¶ 8
Sprayable coatings which are capable of being applied by robotics are desirable to provide for labor and cost savings, and flexibility in design specifications for imparting desired sound and vibration damping properties.
B · US 2016/0168413 A1 · ¶ 3
According to the present invention, a method for providing sound and vibration damping through a substrate comprises: applying the coating composition described above to the substrate; and at least partially curing the coating composition.
B · US 2016/0168413 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0357102 A1, claim 1, first published 2026-11-20T10:10:52-05:00, https://patent.fyi/US20260357102/, SHA-256 82a40956dacb1e76b6d30a1b42f96038130bfff904cb6a36912f47e83d0fb048
First published
Permanent addresshttps://patent.fyi/US20260357102/
Content fingerprint (SHA-256)82a40956dacb1e76b6d30a1b42f96038130bfff904cb6a36912f47e83d0fb048
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi