1.1Acrylic polyol binder
A water-dispersible aliphatic polyisocyanate supplies the curing component. As water evaporates, isocyanate groups react with acrylic hydroxyl groups to form a crosslinked urethane film.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A water-dispersible aliphatic polyisocyanate supplies the curing component. As water evaporates, isocyanate groups react with acrylic hydroxyl groups to form a crosslinked urethane film.
Condensation of a dimerized fatty acid with excess polyalkylene polyamine produces an amidoamine with residual primary and secondary amine groups. A portion of those groups reacts with epoxides during adduct preparation, and the remaining amine groups crosslink the binder after mixing.
The aliphatic diepoxide is added to the amine blend under agitation with an excess of amine hydrogen groups. Amine groups open the epoxide rings to form an adduct with residual amine sites for curing the binder.
The formulation uses 7 parts of adduct solids per 100 parts of mixed coating and sets the epoxy resin loading from the measured amine hydrogen and epoxide contents. The amine groups open the binder’s epoxide rings and form a crosslinked film as water evaporates.
Coarse and fine ground calcium carbonate are dispersed into the binder component to improve particle packing. A dispersant controls slurry viscosity, and the epoxy and amine components cure around the packed particles.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A waterborne epoxy binder and a separate amine functional adduct curing component form a lining for precast concrete stormwater channels. The mixed coating contains 16% by weight adduct and 25% by weight fine quartz filler, with both percentages based on total mixed mass. A roller applies the mixture to the mechanically prepared channel invert and sidewalls, and a brush works the coating into the corners. The lining cures before the channel enters service.
An aqueous dispersion of bisphenol F diglycidyl ether replaces the epoxy resin in the binder component. The separate curing component retains the amine functional adduct prepared from the three amine classes and the two epoxy resin classes. The binder and curing component are proportioned by epoxy group content and active amine hydrogen content. The finished mixture contains 16% by weight adduct and 25% by weight filler.
Ground calcium carbonate with a median particle diameter of 10–20 micrometers replaces quartz flour as the mineral filler. A high-shear disperser incorporates the calcium carbonate into the waterborne epoxy binder before the binder contacts the curing component. The finished mixture contains 25% by weight calcium carbonate and 16% by weight amine functional adduct. The filled binder and curing component are combined at application, and the epoxy and amine groups react as water leaves the applied film.
The waterborne epoxy binder and amine adduct curing component are mixed to give 16% by weight adduct and 25% by weight mineral filler. The filler has a median particle diameter of 5–10 micrometers and a 90th-percentile particle diameter below 25 micrometers. A short-nap roller applies two coats at 125–175 micrometers wet thickness per coat. The first coat reaches a tack-free state before the second coat is applied within the formulation's recoat window.
A cementitious self-leveling underlayment provides the planar base for a waterborne epoxy finish. The underlayment cures and dries, and mechanical preparation removes weak surface material before application of a compatible epoxy primer. The finish combines the epoxy binder, the separate amine adduct curing component, and mineral filler at 16% by weight adduct and 25% by weight filler in the mixed finish. A gauge rake spreads the finish over the primed underlayment, and a spiked roller releases entrained air while the film remains fluid.
Separate feed vessels hold the waterborne epoxy binder, the amine adduct curing component, and an aqueous mineral filler slurry. A controller doses each feed into a vessel on load cells using stored epoxy group content, active amine hydrogen content, adduct concentration, and slurry solids content. The controller selects feed masses that meet the specified cure ratio, 9–22% by weight adduct, and 15–35% by weight filler in the total mixture. It starts the mixer after the dosing checks pass and timestamps first contact between binder and curing component for pot-life tracking.
The binder contains a bisphenol A diglycidyl ether resin dispersed in water at 55% resin solids by weight. The resin supplies epoxide groups that react with the amine curing component after mixing.
A polypropylene glycol diamine, diethylenetriamine, and isophorone diamine form the amine feed. Polypropylene glycol diglycidyl ether and liquid bisphenol A diglycidyl ether react with that feed under an excess of amine hydrogen groups, leaving residual amine functionality for binder cure.
A curing component containing 70% adduct solids by weight contributes 20 parts per 100 parts of mixed coating. The resulting mixture contains 14 parts of active adduct per 100 parts by weight.
The mixed coating contains 25% ground calcium carbonate by weight, with 15 percentage points supplied by a grade with a median particle size of 20 micrometers and 10 by a grade with a median of 3 micrometers. The finer particles occupy spaces between coarser particles.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Provided are a resin composition for the manufacture of marble chips including a halogenated epoxy resin binder and showing high heat resistance, high chemical resistance, high impact resistance, high specific gravity and high transparency, a marble chip manufacturing method using the resin composition and an artificial marble made from marble chips.A · US 2010/0311867 A1 · abstract
An epoxy composition including a waterborne hardener component containing an amine functional adduct, which is a reaction product of at least one polyether amine, at least one polyalkylene amine, at least one arylaliphatic or cycloaliphatic amine, at least one polyether epoxy resin and at least one aromatic liquid epoxy resin, a resin component containing at least one liquid epoxy resin and mineral fillers, wherein the composition contains mineral fillers in the range of 85 tB · US 2022/0235220 A1 · abstract
The resin composition may further include a curing agent for increasing the molecular weight of the halogenated epoxy resin.A · US 2010/0311867 A1 · ¶ 17
In order to produce marble chips having a specific gravity of, e.g., from 1.70 to 1.75, about 10 to 15 wt % of curing agent is added on the basis of the total weight of the resin composition.A · US 2010/0311867 A1 · ¶ 32
The epoxy composition contains mineral fillers in the range of 85 to 95 weight-% based on the total solids of the composition.B · US 2022/0235220 A1 · ¶ 109
An empty cell means only that no passage was reproduced there.
More particularly, the present invention is directed to a resin composition for the manufacture of marble chips including a halogenated epoxy resin binder and showing high heat resistance, high chemical resistance, high impact resistance, high specific gravity and high transparency, a marble chip manufacturing method using the resin composition and an artificial marble made from marble chips.A · US 2010/0311867 A1 · ¶ 2
However, the engineered stone-based artificial marble has a drawback in that it is high in specific gravity and hard to process.A · US 2010/0311867 A1 · ¶ 8
There are no self-leveling epoxy floors on the market, which can be applied in a layer thickness of 1 to 3 mm or more and achieve both a high quality surface for decorative purpose and generate a low enough heat upon burning to fulfill the A2fl fire classification according to EN 13501-1.B · US 2022/0235220 A1 · ¶ 6
The composition according to claim 1 enables a high cure speed and long open time, low shrinkage without crack formation at high layer thickness, such as 1 to 3 mm, a good impact resistance and a glossy and even surface upon curing at ambient conditions.B · US 2022/0235220 A1 · ¶ 8
patent.fyi, US 2026/0357106 A1, claim 1, first published 2026-11-20T10:48:41-05:00, https://patent.fyi/US20260357106/, SHA-256 8180354d79f03e1211b72796119f1bf3d4668c8c759e9e2ba767589145973d18