Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Carrierless adhesive transfer film
What ifWhat if the installed sheet consisted of adhesive alone?
Claim language“a substrate”
A removable release liner supports a crosslinked acrylic pressure-sensitive film during handling and placement on polytetrafluoroethylene. After the liner comes off, a secondary lining panel contacts the exposed adhesive face and the installed film contains no carrier.
1.2Fusion welded fluoropolymer sheet
What ifWhat if fusion welds joined the sheet to the tank lining?
Claim language“an adhesive layer (Y1)”
The sheet and tank lining both use melt-processable perfluoroalkoxy fluoropolymer. A heated tool melts the mating surfaces along the sheet perimeter, and pressure brings the melts together until the joint cools.
1.3Embossed solid polymer backing
What ifWhat if a continuous embossed polymer film carried the adhesive?
Claim language“a non-woven fabric”
A thin, solid polyether ether ketone film carries the fluoropolymer-facing adhesive. Molded ribs on the opposite face increase contact area for a secondary epoxy bond, and plasma treatment promotes wetting of that face by the epoxy.
1.3Solid foil with formed ribs
What ifWhat if an unperforated metal foil provided dimensional support?
Claim language“a metal mesh”
A thin stainless steel foil carries the fluoropolymer-facing adhesive, and shallow stamped ribs stiffen the foil without opening holes. Abrasion and a metal adhesion primer prepare the exposed foil face for a secondary adhesive.
1.3Closed-cell foam backing
What ifWhat if a closed-cell foam provided cushioning and conformed to surface irregularities?
Claim language“a foam having an open-cell structure”
A crosslinked closed-cell polyethylene foam compresses around shallow surface irregularities and supports the fluoropolymer-facing adhesive. Corona treatment promotes adhesion between the foam skin and a tie coating on the opposite face.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Mounting for conveyor guide strips
An adhesive sheet with a glass cloth backing mounts polytetrafluoroethylene guide strips on packaging conveyors. The adhesive face bonds to the untreated underside of each guide strip, and a two-part epoxy wets the exposed cloth and bonds it to the conveyor rail. Recessed rail shoulders support the strip edges and take lateral loads from passing packages. The adhesive face provides a 180° peel force of at least 5.0 N per 25 mm on untreated polytetrafluoroethylene at 23 °C.
Component substitution
Perforated film backing for mechanical anchoring
A 125 μm polyethylene terephthalate film with 0.4 mm punched holes on a 1.5 mm square pitch replaces the porous backing. A pressure-sensitive adhesive covers one face, and a release liner supports the adhesive across the holes during handling. During mounting, epoxy applied to the exposed film face enters the holes and cures against the adhesive, forming discrete anchors through the film. The adhesive face provides a 180° peel force of at least 5.0 N per 25 mm on untreated polytetrafluoroethylene at 23 °C.
Fluorinated film as the bonding surface
A fluorinated ethylene propylene film replaces polytetrafluoroethylene as the exposed facing on a removable splash panel. A fluoropolymer-bonding pressure-sensitive adhesive on a carbon cloth backing bonds to the untreated film under a nip roller. A curable epoxy wets the exposed cloth and secures it to the rigid panel, which supports the film during cleaning. Peel testing on the fluorinated ethylene propylene film at 180° and 23 °C measures the bond to the substituted facing.
Parameter or scale variation
Narrow strips for curved mounting channels
A nonwoven-backed adhesive web is slit into 8 mm strips for mounting a polytetrafluoroethylene wear liner in a curved channel with a 30 mm inside radius. Three strips lie side by side with 2 mm gaps so each strip follows the curvature independently. A compliant roller presses the adhesive faces onto the untreated liner, and a curable bedding resin wets the exposed nonwoven faces when the liner seats in the channel. A 25 mm coupon cut from the unslit web provides a 180° peel force of at least 5.0 N at 23 °C.
Combination with existing systems
Adhesive mounting in a vacuum fixture
A glass cloth-backed adhesive sheet mounts a polytetrafluoroethylene facing on a zoned vacuum fixture. The adhesive face bonds to the untreated facing, and epoxy bonds the exposed cloth to a rigid platen. Matching openings cut through the facing and adhesive sheet align with the platen ports, and perimeter gaskets isolate the vacuum zones. The ports draw sheet stock against the facing while the platen supports the machining load.
Automated or data-driven variant
Feedback control for adhesive coating
A slot die coats adhesive onto a release liner, and a heated nip transfers the adhesive to one face of a moving nonwoven web. A scanning gauge measures coat mass per unit area, and a controller adjusts the metering pump relative to web speed to maintain the setpoint. An automated tester laminates 25 mm coupons to untreated polytetrafluoroethylene panels and measures 180° peel at 23 °C after a fixed dwell. The controller marks the associated web interval when the measured peel force falls below 5.0 N.
Specific version of a part
Spunbond polyester carrier
A 100 g/m² web of continuous polyester filaments forms the substrate. Thermal point bonds stabilize the web during coating and die cutting.
Transfer coated silicone adhesive
A 75 µm dry layer of silicone pressure-sensitive adhesive forms on a removable release liner. A roller laminates the dried adhesive onto one face of the substrate under light nip pressure.
Plain weave glass cloth
Continuous glass yarns form a plain weave with interstices between the yarn bundles. A nip roller presses the adhesive into the interstices on the coating face and leaves the opposite yarn crowns exposed for secondary bonding.
Seven newton peel setting
The fluoropolymer-facing adhesive has a target peel force of 7.0 N/25 mm on untreated polytetrafluoroethylene. A 25 mm wide strip bonds to a flat panel, and a tensile tester pulls it back through 180° at 23 °C to measure the steady peel force.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The substrate layer 5 comprises a single or two or more of thin layers, and constituent component thereof can be selected from any material such as a synthetic resin, a natural resin and the like without restriction, as far as the material has both stretchability and strength.
A · US 2008/0185700 A1 · ¶ 108
The seed germination sheet 340 is composed of a pulp layer 345 on which seeds are spread and a coir mattress 330 integrated with a top surface of the pulp layer 345 including the seeds.
B · US 2021/0029895 A1 · ¶ 66
1.2an adhesive layer (Y1) on one surface of the substrate,
By laminating at room temperature under atmospheric pressure using a laminator (FIG. 4), an adhesive film comprising an adhesive layer (A) and a substrate functioning, which functions as a dicing tape with a die attach film, comprising a protecting film, a die attach film (adhesive layer (B)) and a dicing tape substrate (adhesive layer (A)+substrate layer), was obtained.
A · US 2008/0185700 A1 · ¶ 147
1.3the substrate including at least one selected from the group consisting of a non-woven fabric, a glass cloth, a carbon cloth, a metal mesh, and a foam having an open-cell structure,
Outer wire mesh nonwoven fabric along the inner surface of the outer wire mesh covers the outer wire mesh.
B · US 2021/0029895 A1 · abstract
1.4the adhesive sheet having a 180° peeling force at 23 °C for polytetrafluoroethylene of 5.0 N/25 mm or greater on an adhesive layer (Y1) side of the adhesive sheet.
Further, as the constituent component of the adhesive layer (A), using a mixed resin comprising the above-described α-olefin copolymer and the thermoplastic elastomer is favorable from the viewpoint that the glass transition temperature, shear/peel strength and Young's modulus E′ can be regulated in a suitable range, and the 180° peel adhesion required for over the temperature range of from room temperature (about 20° C.) to high temperature (about 80° C.) can be improved.
A · US 2008/0185700 A1 · ¶ 102
An empty cell means only that no passage was reproduced there.
Statements in these documents
However, these dicing tapes with die attach film fail to fully satisfy the requirement to have sufficient adhesion to the wafer chip during dicing, and be easily peeled off at the time of pickup.
A · US 2008/0185700 A1 · ¶ 2
The present inventors have conducted extensive studies and, as a result, have found that the above object could be solved by controlling the adhesive strength between an adhesive layer (B), functioning as a die attach film, and an adhesive layer (A), functioning as a dicing tape.
A · US 2008/0185700 A1 · ¶ 14
However, such a quadrangular wire net type mattress construction entails a problem that, although vegetation is possible, a sewing process of each vegetation bag and a process of putting multiple vegetation bags one by one inside the quadrangular wire net are required, thus causing increase in working time and costs.
B · US 2021/0029895 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0357111 A1, claim 1, first published 2026-11-20T10:48:41-05:00, https://patent.fyi/US20260357111/, SHA-256 fc776f2593de8275c2a91b4fbf95d4b575dbd0739861078972d6676741b0c383