1.1Polycarbonate film as support
Melt extrusion forms a clear polycarbonate sheet that carries the coating and provides dimensional support. Corona treatment raises the surface energy before a waterborne polyurethane primer is coated and dried.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Melt extrusion forms a clear polycarbonate sheet that carries the coating and provides dimensional support. Corona treatment raises the surface energy before a waterborne polyurethane primer is coated and dried.
Marked film strips are heated at 120 °C for 10 minutes and cooled to room temperature. The percentage length change along each direction measures dimensional stability under the specified thermal cycle.
A pressure-sensitive adhesive strip is rolled onto the coated surface and conditioned for 24 hours at 23 °C. A tensile tester pulls the strip back at 180° and 300 mm/min, and the average steady-state force per unit width measures adhesion to the coating.
A focused pulsed ion beam rasters a 10 μm × 10 μm region and ejects secondary ions. Mass-resolved counts for characteristic molecular fragments form maps of the lateral distribution of selected primer constituents.
The phase samples in each evaluation region form an empirical distribution. Subtracting its 10th percentile from its 90th percentile gives the central phase span in degrees.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A biaxially oriented polyester web carries an adhesion-promoting coating on its print face. A resin thermal-transfer ribbon contacts the coating, and a thermal printhead transfers plant identifiers and barcodes onto the coated face. A rotary die cuts the printed web into individual tags and forms a slot for attaching each tag to a plant support.
A biaxially drawn polyethylene naphthalate film replaces a polyethylene terephthalate film beneath the adhesion-promoting layer. A corona discharge treats one face before a gravure roll applies a waterborne polyurethane dispersion. A hot-air oven removes the water and coalesces the polyurethane particles into a continuous primer.
A phase-mode atomic force microscope records a 20 μm × 20 μm map at 512 × 512 pixels. Software subtracts the map mean and divides the centered map into 25 equal tiles arranged in a 5 × 5 grid, with nominal tile dimensions of 4 μm × 4 μm. It calculates the root mean square divided by the mean absolute phase deviation for each tile whose mean absolute deviation is positive, then reports the median of those ratios and the number of tiles included.
A roll-to-roll label converter feeds the coated polyester web with its adhesion-promoting face toward a transfer adhesive carried on a silicone-coated release liner. A nip presses the adhesive onto the primer and leaves the release liner in place. A rotary die cuts the polyester and adhesive to label shape while the liner remains continuous, and a stripping roll removes the surrounding waste.
A motorized sample stage positions film coupons taken from the two edges and center of a coated web under a phase-mode atomic force microscope. The acquisition software records a 10 μm × 10 μm map on each coupon and centers the phase values by subtracting the map mean. It extracts seven 2 μm × 2 μm windows at fixed coordinates, divides the root mean square by the mean absolute phase deviation in each window, and averages the middle five ratios after sorting. It stores the result with the roll identifier and cross-web position and flags maps with a zero denominator for review.
Near-infrared reflectance sensors view the same cross-web position upstream of the primer applicator and downstream of the drying oven. A web encoder aligns readings from the same segment, and a calibration against gravimetric samples converts the difference in absorbance at a primer-sensitive band into dry coat weight. A controller adjusts the speed of the metering pump feeding the slot die to hold coat weight at its setpoint.
A biaxially stretched polyethylene terephthalate film carries a waterborne aliphatic polyurethane primer. A gravure roll meters the dispersion onto the film, and a hot-air dryer removes water to form a continuous coating.
Polarized measurements at 589 nm give refractive indices of 1.665 in the machine direction, 1.675 in the transverse direction, and 1.500 through the thickness. The mean of the two in-plane indices minus the thickness index gives a plane orientation degree of 0.170.
An atomic force microscope scans a 10 μm × 10 μm area on a 512 × 512 pixel grid using an oscillating silicon cantilever. The phase detector records the lag between the drive and cantilever response in degrees at each pixel.
Seven 2 μm × 2 μm regions are centered at the four combinations of X and Y equal to 2 or 8 μm, and at (5, 2), (5, 5), and (5, 8) μm, with coordinates measured from a scan corner. The procedure computes δq/δa for each region, discards the smallest and largest values, and averages the remaining five.
patent.fyi, US 2026/0357112 A1, claim 1, first published 2026-11-20T10:48:41-05:00, https://patent.fyi/US20260357112/, SHA-256 ead5736e11bae967e50c694a9991b8bcd8417385958cd200862ada32eef1eae6