1.1Polystyrene feed produces aromatic oil
A screw feeder meters ground polystyrene into an oxygen-depleted reactor operated at 450–500 °C. Thermal decomposition releases styrene-rich vapors that condense into an aromatic oil.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A screw feeder meters ground polystyrene into an oxygen-depleted reactor operated at 450–500 °C. Thermal decomposition releases styrene-rich vapors that condense into an aromatic oil.
The vessel heats the resin in a hydrocarbon solvent with a dispersed metal sulfide catalyst under pressurized hydrogen. Cracking shortens the polymer chains, and hydrogen saturates the resulting fragments before distillation separates the oil from the circulating solvent.
A fluidized bed uses steam and a controlled oxygen feed at 850–950 °C to convert the resin into a gas containing hydrogen and carbon monoxide. A water-gas shift reactor increases the hydrogen concentration, and a pressure swing adsorption unit separates hydrogen from the shifted gas.
A heated, nitrogen-blanketed vessel shortens the polyethylene chains, and residence time controls the extent of cracking. A vacuum stripping stage removes light hydrocarbons from the melt, and a chilled belt solidifies the remaining wax.
A heated transfer line keeps condensable hydrocarbons in the vapor phase as they flow to a burner. The burner mixes the vapors with combustion air, and the hot flue gas transfers heat through the reactor wall.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A wax manufacturing plant collects low molecular weight polyethylene wax from off-specification production lots in a dedicated feed bin. A loss-in-weight screw meters solid wax granules into an indirectly heated pyrolysis reactor. A condenser cools the reactor vapors, and a sealed receiver collects the resulting hydrocarbon oil for shipment to a refinery.
An indirectly heated rotary kiln serves as the pyrolysis reactor. A sealed screw feeder delivers solid low molecular weight olefin resin into the elevated inlet of the kiln, and rotary seals maintain an inert atmosphere. The inclined drum rotates to move material toward the solids discharge while a separate vapor outlet routes the pyrolysis vapors to an oil condenser.
Four identical pyrolysis modules each receive 125 kg/h of low molecular weight olefin resin from a common feed bin, giving a total feed capacity of 500 kg/h. Each module has a dedicated loss-in-weight feeder, indirectly heated reactor, condenser, and sealed condensate receiver. A level-controlled pump transfers oil from each receiver through a check valve to a common storage tank.
An indirectly fired pyrolysis reactor receives low molecular weight olefin resin and sends product vapors to a condenser and sealed gas-liquid separator. Liquid oil drains to storage, and gas from the separator passes through a knock-out drum and a pressure regulator to a burner on the reactor furnace. The burner uses auxiliary fuel at startup and adjusts auxiliary fuel flow as recovered gas becomes available.
A pyrolysis reactor converts low molecular weight olefin resin into vapors that pass through a shell-and-tube condenser and drain as oil into a sealed receiver. A closed water loop circulates through the condenser and carries the recovered heat to a separate heat exchanger that preheats plant wash water. A temperature-controlled trim cooler removes surplus heat from the closed loop when wash-water demand falls.
A loss-in-weight feeder meters low molecular weight olefin resin into the pyrolysis reactor, and a mass flowmeter measures the oil pumped from the condensate receiver. Software integrates the measured oil flow over a rolling interval, corrects for inventory changes using the receiver level, and compares the result with resin feed measured over an interval shifted by the process delay. A supervisory controller trims the feeder setpoint within configured limits to maintain the target oil production rate, while a separate temperature loop regulates reactor heat input.
A loss-in-weight feeder meters resin granules from a nitrogen-purged hopper into a variable-speed screw. The screw pushes the granules through a cooled inlet into the heated pyrolysis chamber.
A bubbling fluidized bed holds silica sand at 480–520 °C using recycled noncondensable gas as the fluidizing medium. Contact with the hot sand melts and cracks the resin, and the gas carries the hydrocarbon vapors into the recovery train.
A hot cyclone removes entrained solids before the vapor stream enters two condensers in series. The first condenser collects heavier hydrocarbons, and the chilled second condenser collects lighter hydrocarbons in a separate receiver.
The feed consists of polyethylene granules with a weight-average molecular weight of 30,000 g/mol. High-temperature size-exclusion chromatography measures the molecular-weight distribution of the incoming resin.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Despite the order of feeding the plastic feedstock 12 and the purge gas 18 to the reaction zone 20, the plastic feedstock 12 is considered to be introduced to a hydrogen environment in the reaction zone 20 when the ambient air is purged from the reaction zone 20 by the purge gas 18 and the plastic feedstock 12 is received in the reaction zone 20.B · US 2015/0247096 A1 · ¶ 18
Catalyst likes Ti(II) ethylhexanoate (but not limited to it) is added in the reactor 2 to allow a reversed reaction (PLA→Lactide) occur with continuous depolymerization of PLA to lactide.A · US 2013/0023674 A1 · ¶ 30
Autoclave Time at >400° C. 0.8 hour 1.0 hour 1.5 hour Product Wax Recovery (% 96 94 91 of feed polyethylene) Product Wax Melting Point 112° C. 111° C. 110° C.B · US 2015/0247096 A1 · ¶
As used herein “plastic” refers to thermoplastic polyolefins. Thermoplastic polyolefins include polyethylenes, for example polyethylenes with the formula (C2H4)nH2 where n is typically from 50 to 100, and polypropylenes, such as polypropylenes with the formula (C3H6)mH2, where m is typically from 50 to 100, or a mixture of thermoplastic polyolefins.B · US 2015/0247096 A1 · ¶ 13
An empty cell means only that no passage was reproduced there.
A major component of the production cost is the cost of harvesting and transporting feed-stocks to a production facility.A · US 2013/0023674 A1 · ¶ 4
The current method avoids the cost of harvesting and transporting feed-stocks to a production facility by using feed-stocks derived from organic waste streams already present in municipal solid wastes that are already collected in centralized facilities.A · US 2013/0023674 A1 · ¶ 7
However, polyethylene waxes derived from the thermal decomposition of polyethylene resin are typically inferior in quality, e.g., they exhibit undesirable color, low molecular weight, and are inconsistent across production lots.B · US 2015/0247096 A1 · ¶ 3
Further, it is desirable to provide a method for converting waste plastic into wax with desired properties.B · US 2015/0247096 A1 · ¶ 4
patent.fyi, US 2026/0357137 A1, claim 1, first published 2026-11-20T10:48:41-05:00, https://patent.fyi/US20260357137/, SHA-256 a62db6ca803700682bc633fcd1ab8c7036ebfcd4129f8fa7a3463eaaa259ec04