1.1Heated jaw sealing
Opposed heated jaws clamp the overlapping edges of heat-sealable polyvinyl alcohol films. Heat and pressure soften the facing layers and bring them into intimate contact, and the seam sets as it cools.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Opposed heated jaws clamp the overlapping edges of heat-sealable polyvinyl alcohol films. Heat and pressure soften the facing layers and bring them into intimate contact, and the seam sets as it cools.
A metering roller feeds a thin layer of sealing liquid onto the raised lands of a transfer roller. The lands wet the seam pattern by direct contact with the first film, and a nip presses the second film against the wetted pattern.
A backing roll holds the film at a fixed 15 mm standoff from a narrow fan nozzle. The nozzle dispenses a metered spray onto the seam band, and a downstream nip joins the films while the band remains wet.
A collimated laser beam crosses the spray 100 mm below the outlet, and a detector array records scattered light intensity by angle. A scattering model converts the angular signal into a volume-weighted size distribution and reports its median diameter.
A pulsed backlight and a side-view camera capture droplet silhouettes in a thin measurement region 5 mm above the film. Calibrated image analysis converts silhouette areas to diameters and calculates the median at that location.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A seed packaging line places premeasured seed portions in pockets formed in a lower polyvinyl alcohol film. A single nozzle sprays an aqueous sealing liquid onto the flat rim of each pocket at an 80 mm standoff while a mask shields the seeds. A second polyvinyl alcohol film covers the pocket, and a platen with a raised perimeter presses the two films together along the wetted rim.
An engraved gravure wheel replaces the spray nozzle and transfers sealing liquid directly onto the first polyvinyl alcohol film. The wheel rotates through a liquid reservoir, and a doctor blade wipes excess liquid from the wheel surface. A backing roller holds the first film against the engraved band, which deposits a narrow stripe. A downstream nip brings the second film into contact with the stripe and presses the films together.
A conveyor moves the first film at 12 m/min beneath a nozzle positioned 80 mm above its surface. A sliding carriage positions the contact nip 40 to 160 mm downstream of the spray footprint center, giving a transit time of 0.2 to 0.8 seconds. A guide roller on the carriage feeds the second film into the nip with its sealing face against the wetted first film.
A rotary vacuum thermoforming drum draws the first polyvinyl alcohol film into cavities while leaving flat sealing lands around each pocket. A metering station fills the pockets, and a fixed nozzle sprays sealing liquid through a shield onto the lands as the drum indexes. A compliant roller presses a flat cover film onto the wetted lands while the drum supports the pockets. A downstream die cuts the sealed packets from the web.
A photoelectric sensor reads registration marks on the first film, and an encoder measures web travel between the sensor and the nozzle. A controller uses the sensor offset and the measured delay from valve actuation to droplet arrival to time a fast liquid valve. The valve opens as each seam band passes beneath the nozzle and closes as the band leaves the spray footprint. A downstream nip presses the second film against the wetted bands.
A motorized slide moves the downward-facing nozzle between the sealing station and a test station with a liquid catch pan. A backlit camera views the spray from the side at a plane 100 mm below the outlet, and software measures droplet diameters using a calibrated image scale. The controller adjusts atomizing air flow at a fixed liquid flow until the measured median diameter reaches a 110 micrometer target within a 10 micrometer tolerance. The slide returns the nozzle to the sealing station while the controller retains the calibrated flow settings.
A nozzle wets the seam band on the first side of the second film. A pressure roller brings that band against the dry first side of the first film, where the transferred liquid softens the opposing surface and the joint sets as moisture redistributes.
A nozzle applies deionized water to a 4 mm seam band on the first side of a water-soluble polyvinyl alcohol film. The water hydrates and softens the surface before the second film enters the nip.
A rubber-covered roller presses the first side of the second film against the sprayed band on the first film. A rigid backing roller supports the films while the compliant cover distributes pressure across the seam.
A hydraulic flat fan nozzle sits 100 mm above the supported first film and directs the spray toward its seam band. The liquid pressure and outlet geometry produce a spray with a measured d50 of 120 micrometers before deposition.
The nozzle sprays vertically downward, and a pulsed backlight illuminates droplets 100 mm below its outlet along the line perpendicular to the outlet plane. A side-view camera captures droplet silhouettes perpendicular to their motion, and calibrated image analysis calculates d50 from the measured diameters.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Steps may be taken to treat the inside surface of the film, for example by coating it with an agent such as PVDC (poly (vinylidene chloride)) or PTFE (polytetrafluoroethylene), or to adapt the composition to ensure that it does not dissolve the film.A · US 7,906,471 B2 · ¶ 25
A preferred method of making the water-soluble unit dose article according to the present invention comprises the steps of moulding the first water-soluble film in a mould to form an open cavity, filling the cavity with the detergent composition, laying the second film over the first film to close the cavity, and sealing the first and second films together preferably through solvent sealing, the solvent preferably comprising water, to produce the water-soluble unit dose articB · US 11,078,451 B2 · ¶ 102
It may therefore be appropriate to use the film material of the invention as part of a laminate of two or more layers, as pinholes are unlikely to coincide in two layers of material.A · US 7,906,471 B2 · ¶ 23
An empty cell means only that no passage was reproduced there.
However, the performance of the different film-forming materials on usage with detergent material, and in particular in an environment such as an automatic dishwashing cycle, is sub-optimal.A · US 7,906,471 B2 · ¶ 4
We have now surprisingly discovered that ethoxylated poly (vinylalcohols), i.e. materials obtainable by grafting ethylene oxide on at least some of the hydroxyl groups of poly (vinylalcohol), provide significantly improved characteristics for the indicated purposes in several aspects.A · US 7,906,471 B2 · ¶ 6
Some water-soluble polymeric films that are used to make water-soluble unit dose articles will incompletely dissolve during a wash cycle, leaving film residue on items within the wash.B · US 11,078,451 B2 · ¶ 3
It has been found that water-soluble unit dose articles according to the present disclosure exhibit optimal water solubility, seal strength, and pouch strength.B · US 11,078,451 B2 · ¶ 7
patent.fyi, US 2026/0357165 A1, claim 1, first published 2026-11-20T11:28:11-05:00, https://patent.fyi/US20260357165/, SHA-256 30369a8cedefd752bf812ad796426cc74d4ca6f1b8586b3c302be0000488607b