Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Extruded microporous film sheet without fibers
What ifWhat if the antimicrobial barrier is a continuous extruded microporous thermoplastic film with no polymeric fibers?
Claim language“polymeric fibers”
A molten blend of polyethylene, calcium carbonate filler at 40 to 55 percent by weight, and antimicrobial additive is cast into a flat film 25 to 60 micrometers thick. The cast film is stretched biaxially at 80 to 110 degrees Celsius, pulling the polymer away from the mineral filler to create interconnected sub-micrometer pores. The resulting non-fibrous sheet transmits water vapor while blocking liquid droplets and inhibiting microbes on the film surface.
1.2Metallic alloy microfilaments without a polymer
What ifWhat if the antimicrobial fibers are formed from drawn copper-nickel alloy microfilaments with no polymer?
Claim language“a polymer”
A copper-nickel alloy rod containing 70 to 90 percent copper by weight is bundle-drawn through sequential tungsten carbide dies into flexible microfilaments with diameters of 8 to 20 micrometers. The metallic filaments are spun into conductive yarns and knitted into a breathable mesh fabric. Upon contact with moisture, the metallic surface directly oxidizes to release antimicrobial copper ions while maintaining mechanical flexibility.
1.3Covalently bonded organic ammonium salt
What ifWhat if the fibers carry covalently bonded quaternary ammonium organic molecules with no antimicrobial metal compound?
Claim language“antimicrobial metal compound”
A trialkoxysilyl quaternary ammonium compound is grafted onto hydroxyl-functional fiber surfaces through hydrolysis and condensation at 110 to 130 degrees Celsius. The positively charged nitrogen groups remain permanently bound to the fiber rather than leaching into surrounding liquid. When negatively charged microbial cell membranes contact the surface, electrostatic attraction and the long alkyl chains puncture the lipid bilayer.
What ifWhat if the particles generate reactive oxygen species under visible light rather than release antimicrobial ions upon contact with a fluid?
Claim language“release antimicrobial ions upon contact with a fluid”
Nitrogen-doped titanium dioxide particles with diameters of 20 to 80 nanometers are dispersed in the fiber at 1 to 3 percent by weight. Illumination from ambient visible light between 400 and 500 nanometers excites electrons across the narrowed semiconductor band gap. The excited charge carriers react with adsorbed oxygen and surface humidity to produce hydroxyl radicals and superoxide anions that oxidize microbial cell walls.
1.4Solid organic acid particles for acidification
What ifWhat if the fibers contain solid organic carboxylic acid particles with no boric compounds?
Crystalline fumaric acid or citric acid particles with diameters below 5 micrometers are compounded into the molten polymer at 0.5 to 2.5 percent by weight. When moisture contacts the fiber surface, trace amounts of the solid organic acid dissolve and buffer the immediate surface film to a pH between 3.5 and 4.5. This localized acidic environment disrupts microbial membrane proton gradients and accelerates ion dissociation from the antimicrobial particles.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Antifouling aquaculture netting from copper and borate filaments
Extruded high-density polymer monofilaments containing dispersed cuprous oxide and zinc borate particles form knotted or knotless netting panels for marine and freshwater fish cages. When submerged in seawater or brackish water, continuous fluid contact dissolves trace copper ions and borate ions at the filament surface. The released ions inhibit the settlement of algae, barnacles, and bacterial biofilms on the mesh openings, maintaining water exchange through the enclosure. Twine diameters between 1.5 mm and 4.0 mm provide the tensile strength required to withstand tidal currents and net-washing operations.
Antimicrobial woven groundcover for livestock barn flooring
Heavy-duty woven geotextile fabric constructed from polypropylene tapes loaded with water-insoluble copper compound and borate particles forms a permeable liner beneath bedding material in dairy and poultry barns. Urine, washdown water, and ambient moisture permeate the woven structure and contact the embedded particles along the tape surfaces. The resulting release of antimicrobial metal ions and borate ions reduces ammonia-producing bacteria and hoof-infection pathogens within the damp bedding layer. The permeable weave allows liquid drainage to sub-floor collection channels while resisting tearing from animal hooves and mechanical scrapers.
Component substitution
Biodegradable polylactic acid fibers with zinc oxide
Melt-spun polylactic acid resin replaces conventional petrochemical polymers as the fiber matrix, with finely milled zinc oxide particles substituted for copper or silver salts alongside dispersed boric acid particles. The dry resin pellets and mineral powders are compounded in a twin-screw extruder at 185 to 200 degrees Celsius and drawn into staple fibers or spunbond nonwovens. Upon exposure to moisture in soil or humid air, the zinc oxide releases zinc ions while the boric acid lowers local surface pH and supplies borate species that disrupt microbial cell walls. After the service period ends, the polylactic acid backbone undergoes hydrolytic degradation in industrial composting conditions.
Parameter or scale variation
Bicomponent fibers with high-loading thin outer sheath
A co-extrusion spinneret forms bicomponent filaments having an additive-free structural polymer core that accounts for 75% to 85% of the fiber cross-sectional area and a concentric outer sheath measuring 2 to 5 micrometers thick. The outer sheath contains 6% to 12% by weight of water-insoluble copper oxide particles sized between 0.2 and 1.0 micrometer and 3% to 6% by weight of zinc borate particles sized below 2.0 micrometers. Concentrating the active particles within the thin sheath reduces total additive mass per kilogram of fabric by more than half while preserving surface ion-release flux during fluid contact. The unloaded core retains fiber tenacity above 4.0 grams per denier across spinning speeds of 2500 to 3500 meters per minute.
Combination with existing systems
Antimicrobial nonwoven liners integrated into hydroponic drip trays
A needle-punched nonwoven mat made from polymer fibers containing embedded cuprous oxide and borate particles sits directly beneath growing media inside a recirculating hydroponic channel. Nutrient solution flows laterally through the fibrous mat at a controlled irrigation rate, maintaining continuous liquid contact with the embedded particles. The slow release of copper and borate ions at the mat interface suppresses fungal root-rot pathogens and algae accumulation inside the drainage trough without clogging emitter nozzles. Conventional inline mechanical filters and nutrient dosing pumps downstream of the tray operate unchanged while the mat serves as a replaceable passive barrier.
Automated or data-driven variant
Sensor-guided melt extrusion for uniform particle dispersion
An inline optical turbidity sensor and a near-infrared spectrometer mounted at the extruder die head continuously sample the molten polymer stream carrying antimicrobial metal compound and borate particles. A programmable logic controller compares real-time spectral absorbance and melt pressure against target concentration and viscosity profiles at 10 Hz intervals. When particle agglomeration or concentration drift occurs, a trained regression model adjusts gravimetric side-feeder rates, screw speed, and barrel zone temperatures automatically to restore uniform dispersion. The control loop logs batch-level concentration maps synchronized with yarn bobbin identifiers for downstream weaving allocation.
A bicomponent spinneret co-extrudes a plain polyester core surrounded by a concentric sheath layer containing 2 to 5 percent by weight of antimicrobial and borate particles. The sheath accounts for 20 to 35 percent of the fiber cross-sectional area, concentrating the active particles near the outer fiber surface while preserving the tensile strength of the core. Post-spinning drawing at a draw ratio of 3.0 to 4.5 orients the polymer chains and yields continuous filaments with linear densities of 1.5 to 3.0 decitex.
The fiber matrix uses isotactic polypropylene homopolymer with a melt flow index between 18 and 35 grams per 10 minutes at 230 degrees Celsius. The polymer is compounded with a hindered amine light stabilizer at 0.2 percent by weight and melt-spun at 220 to 250 degrees Celsius through multi-hole spinnerets. Its hydrophobic backbone limits bulk water absorption while allowing surface-adjacent particles to interact with external fluids.
Micronized cuprous oxide ceramic particles
Cuprous oxide powder is jet-milled to a median particle diameter between 0.5 and 2.0 micrometers and dried to a moisture content below 0.1 percent by weight before compounding. The water-insoluble inorganic particles are dispersed into a carrier masterbatch at 15 to 25 percent by weight and let down into the spinning melt to a final fiber loading of 1 to 3 percent. When aqueous fluid contacts exposed particles at the fiber surface, slow surface oxidation releases monovalent and divalent copper ions at controlled rates.
Anhydrous calcium borate mineral particles
Finely milled anhydrous calcium borate particles with a median diameter of 1 to 3 micrometers are compounded into a polymer masterbatch via a co-rotating twin-screw extruder at 230 to 260 degrees Celsius. The anhydrous crystal structure remains thermally stable during melt spinning without releasing water vapor that causes filament breakage. Embedded within the solidified polymer, the sparingly soluble particles gradually hydrate upon contact with moisture and supply borate species at the fiber surface.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Accordingly, fibers and fabrics have been produced with anti-microbial alloys in various synthetic polymers such as polyester, polypropylene, nylon, rayon, and polylactic acid (PLA).
B · US 10,506,805 B2 · ¶ 3
1.2wherein the antimicrobial fibers comprise: a polymer
In another embodiment, the present invention comprises a synthetic fiber comprising a polymer, an anti-microbial agent, and a cationic pigment.
B · US 10,506,805 B2 · ¶ 9
1.3particles comprising water insoluble antimicrobial metal compound that release antimicrobial ions upon contact with a fluid
A method for treating diaper rash, leg ulcers and bed sores using super hydrated bacteriostatic topical preparation with a stable acid pH 5.82, by applying this topical application, which is a mixture of anhydrous lanolin (USP), water, boric acid powder (USP), edible corn starch, white petrolatum, cosmetic grade, and zinc oxide ointment (USP 20% zinc oxide) mixed in a paddle mixer at a temperature of about 100° F. to 107° F. then applying topically, the super hydrated bacteri
A · US 7,824,713 B1 · abstract
An anti-microbial agent may be any suitable anti-microbial, such as silver, copper, zinc and/or gold in metallic forms (e.g., particulates, alloys and oxides), salts (e.g., sulfates, nitrates, acetates, citrates, and chlorides) and/or in ionic forms. In some embodiments, the anti-microbial agent is an anti-microbial alloy powder with a particle size of less than 1 micron, and preferably 0.3 to 0.6 micron.
B · US 10,506,805 B2 · ¶ 17
1.4particles comprising boric compounds embedded in the polymer.
The method of preparation of this salve is critical, and is not merely mixing the ingredients but includes special steps' of adding warm water at about 100° F. to 107° F. to anhydrous lanolin (USP) and mixing in a paddle mixer to obtain water saturation of the anhydrous lanolin then boric acid powder (USP) grade is added to the anhydrous lanolin—water mix and dispersed therein by the mixing apparatus, then edible corn starch is added, mixed into the anhydrous lanolin-water bo
A · US 7,824,713 B1 · ¶ 22
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.4. Only Document B has a passage for 1.11.2. Both have a passage for 1.3.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
There has been much study and effort to date to eliminate this problem and present studies indicate that in many cases the rash is due to a yeast/bacterial growth in a neutral or alkaline environment and by lowering the pH along with a mild antiseptic, in an aqueous environment, stops the yeast/bacterial growth.
A · US 7,824,713 B1 · ¶ 1
An object of this invention is to create a topical preparation, in an aqueous environment among components that are aqua-phobic, which is accomplished by super-hydrating lanolin (wool fat) to create an environment that approximates ten percent water
A · US 7,824,713 B1 · ¶ 8
Thus the need exists for an anti-microbial fabric that will resist the destructiveness of washing in chlorine bleach and maintain its color and efficacy against pathogens.
B · US 10,506,805 B2 · ¶ 6
One skilled in the art can recognize that there are numerous modifications, equivalents and alternative constructions that fall within the spirit and scope of the invention as expressed in the claims.
B · US 10,506,805 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0363248 A1, claim 1, first published 2026-11-22T11:54:49-05:00, https://patent.fyi/US20260363248/, SHA-256 48e106c434003178fcb2e8f64bea6f037b57bf55e0335fa491d156fa2c4e2803