Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Straightening wire with rotary rollers
What ifWhat if the smooth wire is straightened mechanically without passing an electrical current through it?
Claim language“passing an electrical current”
A rotary arbor equipped with offset tungsten carbide dies spins around the smooth wire as a capstan pulls it forward under tension. The alternating bending stresses exceed the yield strength of the alloy in multiple planes, removing coil curvature and residual bow. A pair of pinch rollers at the exit maintains linear alignment before cutting.
1.1Starting with pre-textured wire stock
What ifWhat if the starting feedstock is a wire with preformed surface knurling rather than smooth wire?
Claim language“smooth wire”
Continuous wire stock is drawn through a patterned carbide die that impresses longitudinal micro-grooves along the circumference prior to straightening. The textured wire is clamped between tensioning jaws and straightened by controlled axial stretching beyond its elastic limit. Subsequent forming operations act on the pre-textured profile to retain surface engagement features.
1.2Omitting the wire flattening step
What ifWhat if the straightened wire is not flattened before forming the pin?
Claim language“flattening the straightened wire”
The straightened round wire is cut to pin length and cold-worked by axial drawing to achieve the required spring temper. During assembly, the cylindrical pin is inserted into a hollow post and bent slightly so its elastic curvature presses against opposite points of the inner post wall. Friction from the spring-loaded contact points retains the pin without flat surfaces.
1.2Swaging a stepped retention taper
What ifWhat if the straightened wire is radially swaged into a tapered profile?
Claim language“to create a flattened wire”
Rotating hammers inside a rotary swaging machine strike the straightened wire radially as it feeds through a converging die set. The process reduces the wire diameter in a controlled taper toward the tip while increasing material density and hardness along the shaft. The tapered cylindrical pin wedges into a matching bore to create an interference fit.
1.3Crimping periodic waves along the pin
What ifWhat if the flattened wire is crimped into a sinusoidal wave pattern without twisting?
Claim language“twisting the flattened wire”
A pair of intermeshing toothed gears feeds the flattened wire through their nip point to impress regular, planar undulations along the pin axis. The alternating bends increase the effective outer envelope of the flattened section and work-harden the crests. When inserted into a cylindrical post, the wave crests compress elastically against the bore wall to hold the pin in place.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Modular electrical pin terminals for miniature connectors
The straightened, flattened, and twisted pin structure serves as a removable male contact pin in miniature board-to-board or sensor connectors. A beryllium-copper round wire is resistance-straightened, rolled to a rectangular cross section, and twisted along its longitudinal axis to form helical contact ridges. When inserted into a tubular female receptacle socket, the helical ridges press against the inner bore wall at multiple angular points and maintain electrical continuity under vibration. The spring-back elasticity from cold-working holds the pin in place without solder or locking clips, allowing tool-free replacement during field maintenance.
Component substitution
Niobium wire flattened by opposing carbide dies
Annealed niobium wire and a pair of opposing tungsten-carbide flatting dies mounted in a bench press replace the gold wire and rolling mill. The niobium wire is clamped under axial tension while a direct-current power supply passes current through it to remove curvature and relieve internal stress. The straightened wire is compressed between the parallel carbide dies to produce a uniform flat ribbon profile without rotational roller slippage. Twisting the flattened niobium ribbon forms helical ridges along its surface, increasing surface hardness and creating a biocompatible friction pin suitable for nickel-sensitive wearers.
Induction heating coil for non-contact wire straightening
A high-frequency induction heating coil surrounding the wire path between two ceramic guide bushings replaces the direct electrical contact clamps. As the round wire is drawn continuously under axial tension through the induction coil, eddy currents heat the metal uniformly without leaving clamp marks or arc pits on the wire surface. Downstream of the coil, a forced-air cooling nozzle brings the straightened wire back to ambient temperature before it enters the flattening rollers. Because the wire remains free of surface scoring from electrical contacts, the subsequent twisting step produces smooth helical ridges that resist galling inside a hollow post.
Parameter or scale variation
Heavy-gauge pin fabrication with pulsed current straightening
The process scales to 1.02 mm diameter wire cut into 300 mm lengths for large-format piercing posts and heavy clasp assemblies. A pulsed direct-current source delivers 24 volts at 15 amperes in 50-millisecond pulses with 100-millisecond cooling intervals to prevent surface oxidation during straightening. The wire passes through a rolling mill set to a 0.65 mm gap to reduce thickness by 36 percent, followed by 4.5 full axial turns per 25 mm of length. The resulting thicker twisted pin generates higher radial interference force inside a 1.2 mm inner-diameter hollow post.
Combination with existing systems
Inline laser welding to decorative jewelry heads
The pin-forming station integrates directly upstream of a pulsed-laser micro-welder and a vibratory bowl feeder that supplies cast decorative bezel settings. After the straightened and flattened wire is twisted and sheared into individual 10 mm pin segments, a pneumatic pick-and-place arm transfers each pin vertically into a ceramic fixture aligned beneath a bezel base. A focused laser pulse joins the butt end of the twisted pin to the underside of the bezel without heating or annealing the helical ridges along the shaft. An optical camera inspects concentricity between the bezel and the pin before ejecting the finished threadless stud into a sorting tray.
Specific version of a part
Resistive heating with tensioned brass clamps
A length of 24-gauge titanium alloy wire is gripped between two spring-loaded brass electrode clamps spaced 300 millimeters apart. A regulated low-voltage direct current pulse heats the wire by resistive joule heating to approximately 550 degrees Celsius while a pneumatic cylinder applies 15 newtons of axial tension. Controlled cooling under tension locks the crystal structure into a straight alignment without mechanical die marks.
Precision two-high rolling mill flattening
The straightened 0.51-millimeter round wire passes through the gap between two hardened tool-steel cylindrical rollers arranged in a two-high rolling mill. Micrometer-adjusted bearing blocks set the roll gap to 0.36 millimeters, compressing the wire into an oval-edged flat strip with a 30 percent thickness reduction. Cold rolling increases the surface hardness while preserving a smooth, burr-free edge profile.
Dual-chuck torsion with axial tension control
Both ends of the flattened wire are secured in precision collet chucks, with one chuck fixed to a load cell and the other driven by a stepper motor. The motor rotates the flattened strip through 3.5 full turns per centimeter of length while a linear actuator maintains constant axial tension to prevent helical buckling. The resulting uniform pitch forms angled ridges along the pin that interlock with the inner wall of a hollow post.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1electrically straightening lengths of smooth wire by passing an electrical current through the smooth wire;
1.2flattening the straightened wire to create a flattened wire; and
Flattened wires are (1) round wires that have been compressed, preferably cold compressed, or (2) drawn into the desired flattened shape.
A · US 8,893,894 B2 · ¶ 16
Examples of methods that can be used to increase the potential contact area of the contacting regions of the wire of the woven mesh or expanded mesh electrodes 112, 122, e.g., to flatten portions of the wire, include, but are not limited to mechanical modification of the wire, including by abrasion (e.g., sanding, milling, grinding, etc.) or plastically deforming and flattening the wires at the apexes using compressive loading.
B · US 2023/0243046 A1 · ¶ 45
1.3twisting the flattened wire to create a single twisted wire.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.2.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
As a result, self-cleaning screens are desired that include the benefits of polymer support members, but not the shortcomings of woven perpendicular wires, and which take less time, material, and cost to manufacture than screens which include both woven wires and polymer support strips.
A · US 8,893,894 B2 · ¶ 6
Thus, what is, needed a method an apparatus for creating a self-cleaning screen which includes polymer support means and which does not require pre-weaving of other wires, and does not require pre-formed polymer bars or strips.
A · US 8,893,894 B2 · ¶ 6
Therefore, there is a need for cost-competitive and environmentally friendly methods of hydrogen gas producing electrolysis systems and methods.
B · US 2023/0243046 A1 · ¶ 3
The present disclosure describes systems and methods that can provide for more environmentally friendly and lower-cost production of hydrogen gas via electrolysis of water.
B · US 2023/0243046 A1 · ¶ 4
Cite aspatent.fyi, US 2026/0363400 A1, claim 1, first published 2026-11-22T12:53:29-05:00, https://patent.fyi/US20260363400/, SHA-256 08f438a2209b7063c33ffde0bc73e8b9b4e68fe788a3808f37cb4bfab7e08a54