Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Semiconductor emitter with a band gap
What ifWhat if the first electrode is formed from a semiconductor with a band gap rather than a first conductive material?
Claim language“a first conductive material”
A doped semiconductor wafer serves as the charge-supplying electrode, where thermal or radiative energy excites electrons across an energy band gap of 0.6 eV to 1.4 eV into the conduction band. An ohmic back contact collects return current from the external load while the semiconductor surface forms a rectifying barrier against the opposing layer. Carrier concentration is set by dopant density between 10^15 and 10^18 atoms per cubic centimeter to control internal resistance and open-circuit voltage.
1.2Micrometer vacuum gap for thermionic emission
What ifWhat if the spacing between the facing surfaces is a micrometer-scale vacuum gap larger than 200 angstroms?
Claim language“in a range of 200 angstroms or less”
Ceramic micro-spacers hold the two facing electrode surfaces 1 to 10 micrometers apart inside an evacuated enclosure maintained below 0.001 Pa. At this separation, quantum tunneling is suppressed and electrons cross the vacuum gap by thermionic emission when the emitter reaches sufficient thermal energy to overcome its surface barrier. A low-pressure alkali metal vapor fill neutralizes space charge in the interelectrode region to sustain steady current flow to the collector.
1.2Low work function collector with reversed polarity
What ifWhat if the facing surface of the second conductor has a work function below 2.0 eV?
Claim language“a work function in a range of 2.0 eV or greater”
A monolayer of alkali metal or alkaline-earth oxide lowers the facing surface of the second conductor to a work function between 1.1 eV and 1.8 eV, while the first conductor uses a high-work-function metal above 4.5 eV. The resulting contact potential difference reverses the direction of net electron flow so electrons move from the second conductor to the first conductor. External terminal connections are swapped so the load receives the required output polarity.
1.3Single inductive coil powered by magnetic fields
What ifWhat if the electrical potential is induced across the two ends of a single coiled conductor rather than between the first conductor and the second conductor?
Claim language“between the first conductor and the second conductor”
A continuous planar spiral coil of insulated wire sits inside a hermetically sealed biocompatible housing and couples inductively to an external alternating magnetic field. Time-varying magnetic flux through the coil turns induces an electromotive force between the inner and outer leads of the single winding. A rectifier bridge and smoothing capacitor convert the induced alternating voltage into a steady direct-current supply for internal circuitry.
1.4Electrochemical redox transfer through an electrolyte
What ifWhat if charge is transferred between the electrodes by electrochemical redox reactions through an ionic electrolyte rather than by quantum tunneling?
Claim language“by quantum tunneling”
A solid polymer electrolyte or liquid salt bridge fills the space between the two electrodes and conducts ions while blocking direct electronic conduction. Oxidation at the anode releases electrons into an external circuit, and reduction at the cathode consumes those electrons while ionic migration through the electrolyte maintains charge neutrality. Electrode potentials are set by the chemical half-cell reactions, producing 0.5 V to 3.6 V per cell.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Subcutaneous power module for implantable veterinary telemetry tags
An array of asymmetric work-function tunneling cells is hermetically encapsulated inside a biocompatible titanium housing with ceramic feedthroughs for subcutaneous implantation in livestock or companion animals. Each cell pairs a low-work-function cesium-coated metal emitter and a high-work-function platinum collector separated by a 5-nanometer aluminum oxide barrier layer, stacked in series-parallel groups on a silicon substrate. At a mammalian body temperature of 37 to 39 degrees Celsius, the stacked array supplies a continuous direct current output through the feedthroughs to a low-power physiological monitoring circuit and an inductive telemetry coil. The hermetically sealed titanium enclosure isolates the electrode stack from interstitial fluids while maintaining thermal equilibrium with surrounding tissue.
Component substitution
Diamond emitter and tungsten collector tunneling junction
A hydrogen-terminated, nitrogen-doped nanocrystalline diamond film replaces the metallic first conductor to provide a work function near 1.5 electronvolts on the emitting surface. A sputtered tungsten layer with a work function of 4.5 electronvolts forms the opposing second conductor, separated from the diamond film by a 3-nanometer stack of exfoliated hexagonal boron nitride sheets. The crystalline hexagonal boron nitride lattice provides a uniform tunneling barrier with high dielectric breakdown strength and low interfacial defect density. Electrons tunnel across the hexagonal boron nitride sheets from the diamond emitter into the tungsten collector under ambient thermal excitation, establishing a steady open-circuit voltage across the electrodes.
Flexible elastomer substrate with titanium carbide sheet electrodes
A flexible silicone elastomer film replaces the rigid substrate to support a conformable array of tunneling power cells for skin-mounted medical monitoring patches. Solution-processed two-dimensional titanium carbide nanosheets with a surface-terminated work function of 2.1 electronvolts form the first conductor, paired with a serpentine evaporated gold film having a work function of 5.1 electronvolts as the second conductor. An atomic-layer-deposited hafnium oxide layer measuring 4 nanometers in thickness separates the facing conductive surfaces while flexing without cracking under bending radii down to 5 millimeters. Serpentine copper-polyimide interconnects link adjacent cells across the elastomer sheet so the power patch maintains electrical continuity during skin stretching and body movement.
Parameter or scale variation
Wafer-scale cell array with sub-nanometer vacuum gap
A monolithic 100-millimeter silicon wafer integrates 10,000 planar tunneling elements arranged into 100 series-connected banks of 100 parallel cells using photolithographic metal interconnects. Each element maintains a gap of 0.8 nanometers between a barium-oxide-coated nickel emitter and a gold collector using microfabricated silicon dioxide edge spacers around an evacuated cavity. Reducing the barrier spacing to 0.8 nanometers increases the electron tunneling current density per square centimeter while keeping the active area of each cell at 50 micrometers by 50 micrometers. Across an operating temperature range of minus 40 to 125 degrees Celsius, the interconnected wafer array produces a combined output of 1.2 volts at 500 microamperes across its perimeter contact pads.
Combination with existing systems
Hybrid power module with supercapacitor and voltage regulator
A stacked array of tunneling power elements connects directly to the input of a low-voltage synchronous boost converter that steps a 150-millivolt input up to a regulated 1.8-volt rail. The boost converter charges a 50-millifarad thin-film solid-state supercapacitor that stores energy during idle periods and delivers pulsed currents up to 20 milliamperes during active load cycles. A voltage supervisor circuit monitors the supercapacitor terminal voltage and closes a field-effect transistor load switch when the stored potential reaches 1.8 volts, powering a downstream neural stimulation pulse generator or sensor transceiver. When the supercapacitor discharges to 1.2 volts, the supervisor opens the load switch so the tunneling array recharges the storage element continuously without collapsing the converter input.
Automated or data-driven variant
Closed-loop impedance matching using embedded sensor feedback
An embedded microcontroller samples output voltage, output current, and local die temperature from integrated analog-to-digital converters and a resistive temperature detector mounted on the tunneling array substrate. A firmware control loop executes a perturb-and-observe algorithm every 100 milliseconds to adjust the switching duty cycle of a programmable load-matching converter, holding the array at its maximum power point as ambient temperature shifts. A regression model stored in flash memory predicts cell degradation and series resistance drift from historical current-voltage curves and cumulative operating hours. When the model detects a bank whose internal resistance exceeds a programmed threshold, the controller actuates solid-state bypass switches to isolate the degraded bank and reconfigure the remaining series-parallel strings.
Specific version of a part
Coplanar interdigitated electrodes on one plane
Photolithography patterns alternating fingers of the first and second conductive materials on the top surface of an insulating ceramic wafer with lateral trench spacing of 50 to 500 nanometers. Charge carriers travel horizontally across the lateral gap or through a deposited surface dielectric film bridging adjacent fingers. Single-plane fabrication removes vertical wafer bonding and provides direct wire-bonding access to both electrode pads from the top side.
Alkali coated refractory metal emitter foil
A 5-micrometer tungsten foil serves as the first conductor, and a sub-monolayer of cesium is vapor-deposited onto its facing first surface under ultra-high vacuum. The alkali surface dipole layer lowers the effective work function of the first surface from 4.5 eV to a range of 1.4 eV to 1.6 eV. The opposing second surface of the tungsten foil bonds to a copper current-collecting bus bar.
Atomic layer deposited aluminum oxide barrier
A gold film with a work function of 5.1 eV forms the second conductor and faces the first conductor across a uniform dielectric spacer. Atomic layer deposition grows an amorphous aluminum oxide film between 15 and 40 angstroms thick directly onto the first conductor before metalizing the gold collector layer. The dense oxide barrier prevents direct electrical shorting while keeping the interelectrode gap within 200 angstroms.
Series stacked microcell array for implants
Multiple electrical power source elements are fabricated vertically on a biocompatible ceramic substrate and connected in series through thin-film platinum interconnects. At a mammalian body temperature of 310 K, each element produces a millivolt-level open-circuit potential that sums across the series stack to reach 1.5 V to 3.0 V. A hermetically sealed titanium enclosure houses the stack and feeds a storage capacitor for an implantable pulse generator.
Isothermal direct tunneling across asymmetric barriers
Both facing electrode surfaces remain at a uniform ambient temperature of 295 K to 315 K through thermal coupling to a common metallic heat spreader. Because the barrier thickness is held below 30 angstroms, thermally excited electrons near the highest occupied electron energy level of the lower-work-function surface tunnel directly through the trapezoidal potential barrier into unoccupied states of the higher-work-function surface. A low-leakage rectifying load circuit extracts unidirectional current from the resulting potential difference without any thermal gradient between the two conductors.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a first conductor formed of a first conductive material and having a first surface and a second surface, the first surface having a work function value;
The photodetector array comprises an array of pairs of opposing first and second electrodes; a photo-sensitive insulating material disposed between the opposing first and second electrodes of the respective pairs; an electrical circuit for detecting photo-assisted quantum tunneling currents between the opposing first and second electrode of the respective pairs.
A · US 2011/0079706 A1 · abstract
1.2a second conductor formed of a second conductive material and having a first surface and a second surface, the first surface having a work function in a range of 2.0 eV or greater, and facing the first surface of the first conductor with a gap formed between the first surface of the first conductor and the first surface of the second conductor, the gap being in a range of 200 angstroms or less;
An insulating material 308 is disposed between the substrate 302, 306, in the fixed separation distance gap between the first and second sets 102, 106 of nano wires.
A · US 2011/0079706 A1 · ¶ 40
The thickness of the tunneling/passivation layer can be between 1 and 50 angstroms, preferably between 1 and 10 angstroms.
B · US 2015/0236177 A1 · ¶ 33
1.3the electrical power source element being configured to generate an electrical potential between the first conductor and the second conductor at a temperature above absolute zero;
The electrical circuit may further comprise a source for applying a potential difference across the first and second opposing electrodes.
A · US 2011/0079706 A1 · ¶ 23
The low temperature coefficient allows the tunneling-junction solar cells to convert solar energy to electricity more efficiently in comparison with conventional solar cells at elevated temperature. For example, at an elevated temperature of 75° C., the tunneling-junction solar cells produce 12-15% more electricity than conventional solar cells with the same nameplate power.
B · US 2015/0236177 A1 · ¶ 54
1.4wherein electrons from said first surface of said first conductor are transferred to said facing first surface of said conductor by quantum tunneling without the need for said first surface of said first conductor and said facing surface of said second conductor to be at different temperatures.
In operation, photons 400 entering the photo-sensitive material 308 interact with the photo-sensitive material 308 to achieve photo-assisted quantum tunneling 401 between opposing sections 402, 404 of nano wires 300, 304 of the first and second sets of nano wires respectively.
A · US 2011/0079706 A1 · ¶ 41
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.11.4. Both have a passage for 1.21.3. Both are classified in CPC H01L.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
It is with the knowledge of this background that the present invention has been made, and example embodiments of the present invention seek to provide an alternative image sensor and a method of generating an image in view of the ongoing and increasing demand for image sensors.
A · US 2011/0079706 A1 · ¶ 4
This is undesirable because the energy-conversion efficiency of semiconductor solar cells degrades as the temperature rises.
B · US 2015/0236177 A1 · ¶ 7
Another issue with the concentration of sunlight is the current crowding effect.
B · US 2015/0236177 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0364362 A1, claim 1, first published 2026-11-23T02:02:31-05:00, https://patent.fyi/US20260364362/, SHA-256 c1348503b7bf720ebff3926f2797928c45787666ceef7b10bd877f7987b30ea0