Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Non-porous corrugated metal substrate
What ifWhat if the composite uses a non-porous corrugated metal sheet as the support?
Claim language“a porous support”
A stamped stainless-steel or aluminum foil is folded into fluted channels with a pitch of 1 to 3 millimeters to provide high geometric surface area without internal pores. Abrasive grit blasting roughens the dense metal surface to an average roughness of 2 to 5 micrometers so subsequent coatings adhere mechanically. Air flows along the open channels across the coated metal faces with low pressure drop.
1.2Dry thermal spray phosphor deposition
What ifWhat if dry phosphor powder is thermally sprayed onto the support without a liquid slurry?
Claim language“using a long-lasting phosphor slurry”
Dry aluminate phosphor powder with a particle size of 10 to 40 micrometers feeds through a carrier gas stream into an oxygen-fuel flame spray torch. Partially molten droplets impact the support surface and solidify on contact to build a 20 to 60 micrometer coating without wet drying steps. Dry deposition prevents hydrolysis of moisture-sensitive phosphor grains during application.
1.2Bulk-embedded phosphor in support body
What ifWhat if the phosphor particles are blended into the support bulk material so no phosphor coating layer is formed on the surface?
Claim language“a long-lasting phosphor coating layer on a surface”
Phosphor powder at 10 to 25 percent by weight is mixed directly into a translucent ceramic or polymer feedstock prior to extrusion or molding. After shaping and consolidation, the luminescent particles sit distributed throughout the porous walls and emit stored light outward through the translucent matrix. Monolithic integration eliminates separate coating and drying stages for the phosphor.
1.3Vapor-grown alumina barrier layer
What ifWhat if an aluminum oxide barrier layer is grown by atomic layer deposition with no silica layer?
Claim language“using a silica sol, a silica (SiO2) coating layer”
Alternating vapor pulses of trimethylaluminum and water vapor react sequentially on the phosphor surface at 150 to 250 degrees Celsius inside a vacuum chamber. Each cycle deposits approximately 0.1 nanometers of amorphous aluminum oxide until a pinhole-free 10 to 30 nanometer film forms. The transparent alumina film shields the phosphor from moisture and reactive radicals while transmitting excitation and emission light.
1.3Direct photocatalyst coating without barrier
What ifWhat if the intermediate silica coating step is omitted and the photocatalyst is applied directly onto a water-insoluble phosphor layer?
Claim language“forming, using a silica sol, a silica (SiO2) coating layer”
A non-hygroscopic nitride or silicate phosphor is fixed onto the support with an inorganic phosphate binder that resists acidic or alkaline photocatalyst suspensions. The photocatalyst dispersion is applied directly over the phosphor surface and calcined at 350 to 450 degrees Celsius to bond the two layers together. Omitting the intermediate oxide film reduces optical reflection losses and shortens the manufacturing sequence by one coating and curing cycle.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Wastewater treatment reactor with submerged luminescent ceramic media
A packed-bed aqueous photoreactor contains porous ceramic beads coated sequentially with a strontium aluminate phosphor layer, a dense silica barrier layer, and an anatase titanium dioxide photocatalyst layer. The silica intermediate layer isolates the water-sensitive aluminate phosphor from direct contact with the aqueous effluent while transmitting afterglow light at 480 to 530 nanometers to the outer catalyst layer. Ultraviolet light-emitting diode arrays housed in submerged quartz sleeves pulse on for 10 minutes and off for 20 minutes to charge the phosphor and maintain continuous hydroxyl radical generation at the catalyst-water interface. Dissolved organic dyes and phenolic compounds oxidize as wastewater circulates through the packed bed at a superficial liquid velocity of 0.5 to 2.0 centimeters per second.
Component substitution
Alumina intermediate barrier replacing the silica coating layer
An optically transparent aluminum oxide layer replaces the silica intermediate layer between the long-lasting phosphor coating and the outer photocatalyst coating on a porous cordierite honeycomb support. The barrier layer forms by vacuum-assisted slip casting of an aqueous boehmite sol at 5 weight percent solids, followed by drying at 110 degrees Celsius and calcination at 500 degrees Celsius to produce a gamma-alumina film 0.8 to 1.5 micrometers thick. The gamma-alumina layer blocks chemical diffusion between the alkaline-earth aluminate phosphor and the outer titanium dioxide catalyst while maintaining high optical transmittance across 400 to 550 nanometers. Its alkali resistance reduces interfacial degradation when the composite operates in humid gas streams containing ammonia or volatile amines.
A monoclinic tungsten trioxide photocatalyst layer replaces an ultraviolet-active titanium dioxide catalyst on the outer surface of the silica-coated phosphor composite. A peroxotungstic acid sol with a tungsten concentration of 0.2 molar is deposited over the silica layer by ultrasonic mist deposition and calcined at 450 degrees Celsius in air for 3 hours. Because monoclinic tungsten trioxide has a band gap near 2.7 electron volts, the outer layer absorbs blue-green afterglow photons emitted around 450 to 520 nanometers by a europium- and dysprosium-doped strontium aluminate underlayer. Electron-hole pairs generated by the persistent luminescence drive continuous oxidation of acetaldehyde and formaldehyde in dark enclosures without ultraviolet excitation.
Parameter or scale variation
High cell density monolith with submicron coating layers
A porous ceramic monolith with 400 to 600 square channels per square inch and wall thicknesses of 0.15 to 0.25 millimeters serves as the support structure. The long-lasting phosphor layer is deposited at a dry thickness of 8 to 15 micrometers using phosphor particles milled to a median diameter of 1.5 micrometers to prevent channel blockage. A silica barrier layer of 150 to 300 nanometers and a photocatalyst layer of 200 to 400 nanometers are applied by controlled-withdrawal dip coating at a pull speed of 2 millimeters per second, followed by rapid thermal annealing at 550 degrees Celsius for 20 minutes. The narrow channel geometry increases the geometric surface-to-volume ratio above 2500 square meters per cubic meter while keeping the pressure drop below 180 pascals at a face velocity of 1.5 meters per second.
Combination with existing systems
Integration with a building ventilation heat recovery unit
A replaceable filter cartridge containing the multilayer phosphor, silica, and photocatalyst porous composite mounts downstream of the coarse particulate prefilter inside a building enthalpy heat recovery ventilation unit. Light-emitting diode strips emitting at 365 to 405 nanometers are mounted along the plenum wall facing the upstream side of the composite cartridge to charge the phosphor layer during intermittent illumination intervals. Incoming outdoor air passes through the heat exchanger core, enters the composite bed where volatile organic compounds decompose into carbon dioxide and water vapor, and exits into the supply ductwork. During intervals when the light-emitting diodes power down, stored luminescence in the phosphor layer sustains photocatalytic oxidation across the composite surface.
Automated or data-driven variant
Automated coating line with inline optical thickness control
An automated manufacturing line applies the phosphor slurry, silica sol, and photocatalyst sol onto porous ceramic supports using programmable robotic spray nozzles and servo-driven dip-coating stages. Inline spectroscopic reflectometers and fluorescence intensity sensors measure wet-film thickness and luminescence emission uniformity after each deposition station and transmit the readings to a supervisory controller. A regression model trained on historical thickness, viscosity, and post-calcination photocatalytic activity data adjusts spray atomization pressure, nozzle traverse speed, and sol withdrawal rate in real time to hold each layer within plus or minus 5 percent of its target thickness. An automated conveyor kiln then executes a closed-loop thermal profile based on infrared pyrometer feedback from the coated supports.
Specific version of a part
Reticulated ceramic foam support preparation
An open-cell polyurethane sponge with 20 to 40 pores per inch is impregnated with an aqueous alumina-cordierite ceramic slurry and compressed through rollers to clear blocked cells. The coated sponge is dried at 110 degrees Celsius and sintered at 1300 to 1400 degrees Celsius to burn out the polymer template and fuse the ceramic struts. The resulting rigid porous skeleton provides interconnected gas passages with 80 to 85 percent open porosity.
Dip-coated strontium aluminate phosphor slurry
Europium- and dysprosium-doped strontium aluminate powder with a median diameter of 15 to 25 micrometers is dispersed at 30 to 40 percent solids in an ethanol solvent containing an inorganic silicate binder. The porous support is immersed in the agitated slurry for 30 to 60 seconds, drained, and blown with compressed air to clear excess suspension from pore throats. Drying at 80 degrees Celsius followed by heat treatment at 300 degrees Celsius cures the 30 to 50 micrometer luminescent layer.
Acid-catalyzed alkoxide silica sol coating
Tetraethyl orthosilicate is hydrolyzed in an ethanol-water mixture acidified with nitric acid to a pH of 2 to 3 and aged at 25 degrees Celsius for 12 hours to form a polymeric silica sol. The phosphor-coated support is dip-coated in the sol at a withdrawal speed of 2 to 5 millimeters per second to deposit a uniform wet gel film. Drying at 100 degrees Celsius and calcining at 400 degrees Celsius converts the gel into a dense 100 to 200 nanometer amorphous silica layer.
Peptized titanium dioxide sol spray
Titanium tetraisopropoxide is hydrolyzed in deionized water and peptized with acetic acid at 70 degrees Celsius to produce a translucent colloidal anatase sol with 5 to 15 nanometer crystallites. A pneumatic atomizing nozzle sprays the sol onto the silica-coated support at a pressure of 0.2 to 0.3 megapascals while the support rotates to coat all exposed surfaces. Calcination at 450 degrees Celsius for 2 hours removes organic residues and bonds a porous 200 to 500 nanometer titanium dioxide layer.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.2forming, using a long-lasting phosphor slurry, a long-lasting phosphor coating layer on a surface of the porous support;
1.3forming, using a silica sol, a silica (SiO2) coating layer on a surface of the long-lasting phosphor coating layer; and
1.4forming, using a photocatalyst sol, a photocatalyst coating layer on a surface of the silica coating layer.
As a method which uses a sol containing a photocatalyst (and which, hence, does not require a step for forming crystalline microparticles of a photocatalyst), Unexamined Japanese Patent Application Laid-Open Specification No. 6-278241 discloses a method for immobilizing a photocatalyst on the surface of a substrate, in which a water-peptized sol of titanium dioxide is coated on the surface of a substrate.
A · US 7,030,058 B1 · ¶ 20
The action of “immersing” in the invention is put the adsorbent material into the photocatalyst sol and letting the adsorbent material be coated with photocatalyst sol; “agitating” means homogenizing the adsorbent material in the photocatalyst sol by means of manual/mechanical agitation or ultrasonic vibration.
B · US 2007/0149397 A1 · ¶ 22
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.4. Both are classified in CPC B01J.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
For enabling such applications, the method for immobilizing photocatalysts on the surface of various substrates has a great importance.
A · US 7,030,058 B1 · ¶ 9
Related claim parts: 1.4
Thus the development of technology that can maintain the activity of photocatalyst after immobilization, while maintaining the property of substrate has become an important direction in the field of photocatalyst application.
B · US 2007/0149397 A1 · ¶ 7
Related claim parts: 1.4
Further, the above-mentioned film exhibits excellent properties with respect to transparency, durability, staining resistance, hardness and the like.
A · US 7,030,058 B1 · ¶ 2
Therefore, the above-mentioned modified photocatalyst sol and modified photocatalyst composition are extremely useful for, e.g., preventing dirt from adhering to the surfaces of various substrates, and preventing fogging from occurring on the surfaces of various substrates.
A · US 7,030,058 B1 · ¶ 2
To address the drawbacks of prior arts, the object of the present invention is to provide a photocatalytic composite material and a method for immobilizing photocatalyst with adsorbent materials without high energy consumption or use of adhesive agent, thereby maintaining the activity and adsorbent property of photocatalyst.
B · US 2007/0149397 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0364498 A1, claim 1, first published 2026-11-23T03:00:22-05:00, https://patent.fyi/US20260364498/, SHA-256 d2313e47784211037ddb15662c96843dbb197886f6497c7cdf6600896c729376