patent.fyi
Applications  /  US 2026/0364541
United States Patent Application Publication

US 2026/0364541 A1

Published
Nov 19, 2026
Filed
Nov 21, 2023
Earliest date on the face
Nov 30, 2022
Classification
B01D 71/34
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Polyethersulfone membrane matrix

What ifWhat if polyethersulfone forms the membrane matrix?
Claim language“a PVDF polymer”

Polyethersulfone dissolves in a pyrrolidone-rich casting liquid and forms a thin layer on a porous backing. Immersion in water exchanges the casting liquid for water and precipitates the polyethersulfone as a porous solid.

1.1Lithium chloride pore modifier

What ifWhat if dissolved lithium chloride controls pore formation?
Claim language“water soluble polymer and/or hydrogel”

Lithium chloride dissolves in the casting liquid and changes the dope viscosity and its demixing behavior during water coagulation. A water rinse extracts the salt and residual solvent from the precipitated PVDF matrix.

1.1Dimethylacetamide as the primary solvent

What ifWhat if dimethylacetamide serves as the primary solvent in a blend with methyl lactate?
Claim language“comprising N-butylpyrrolidone and”

Dimethylacetamide dissolves PVDF, and methyl lactate forms part of the casting liquid. In a water bath, solvent leaves the cast layer and water enters, causing PVDF to separate into a polymer-rich matrix and a liquid-rich pore phase.

1.1Dimethyl sulfoxide as co-solvent

What ifWhat if dimethyl sulfoxide serves as the water-miscible co-solvent?
Claim language“water soluble lactate acid derivative”

Dimethyl sulfoxide blends with N-butylpyrrolidone in the PVDF dope. The dimethyl sulfoxide fraction changes the exchange between the casting liquid and the water bath, which changes the rate of phase separation and the resulting pore structure.

1.2Forty percent n-butylpyrrolidone blend

What ifWhat if N-butylpyrrolidone makes up 40 wt % of the solvent blend?
Claim language“at least 50 wt % or greater of N-butylpyrrolidone”

The solvent blend contains 40 wt % N-butylpyrrolidone, 40 wt % dimethyl sulfoxide, and 20 wt % methyl lactate. Dimethyl sulfoxide contributes to PVDF dissolution, and a water bath precipitates the cast polymer layer as the mixed solvent diffuses out.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Textile rinse water recovery

A flat-sheet PVDF membrane cast from a dope containing a water-soluble polymer and a solvent blend of N-butylpyrrolidone and a water-soluble lactate derivative is installed in a crossflow module. N-butylpyrrolidone makes up at least 50 wt % of the total solvent. A lint screen upstream of the module captures fibers, and the membrane retains suspended fines and colloids. The permeate feeds the first rinse stage, and a bleed from the recirculating retentate loop limits solids buildup.

Component substitution

Polyvinyl alcohol as pore former

Partially hydrolyzed polyvinyl alcohol serves as polymer H in place of polyvinylpyrrolidone. The polyvinyl alcohol is dissolved in a small amount of heated water, cooled, and metered into the stirred PVDF solution below the dope's cloud point. The solvent blend contains a water-soluble lactate derivative, and N-butylpyrrolidone accounts for at least 50 wt % of the total solvent, including the added water. The dope is cast as a film, immersed in a water bath, and rinsed to extract solvent and the water-soluble fraction of the additive.

Parameter or scale variation

Thin film casting on fabric

A doctor blade meters a 150 to 250 µm wet layer onto a polyester nonwoven at a web speed of 0.5 to 2 m/min. The dope contains PVDF and a water-soluble polymer, with N-butylpyrrolidone at 55 to 65 wt % of the total solvent and a water-soluble lactate derivative making up the balance. The coated web enters an 18 to 22 °C water bath within 3 seconds of casting. The supported sheet then passes through two fresh-water rinse stages to extract residual solvent.

Two-stage coagulation for flat sheets

A 200 µm wet film is cast from a dope containing PVDF and a water-soluble polymer, with N-butylpyrrolidone at 60 wt % of total solvent and a water-soluble lactate derivative making up the balance. The film enters a first bath at 20 °C containing 10 wt % of the same organic solvent blend in water. After 15 seconds it transfers to a fresh-water bath at 25 °C for at least 5 minutes. The dissolved solvent in the first bath reduces the initial solvent exchange rate, and the second bath continues precipitation and solvent extraction.

Combination with existing systems

Immersed module for activated sludge

A PVDF dope containing a water-soluble polymer is spun through an annular spinneret using water as the bore fluid and an external water bath for coagulation. The solvent blend contains at least 50 wt % N-butylpyrrolidone and a water-soluble lactate derivative. The rinsed hollow fibers are potted with open lumens at a permeate header and sealed at their opposite ends, then submerged in an activated sludge tank. A pump withdraws permeate through the lumens while a diffuser beneath the bundle scours the fiber surfaces with rising air bubbles.

Automated or data-driven variant

Feedback control of coagulation bath

A continuous casting line feeds a PVDF dope containing a water-soluble polymer into a water coagulation bath, with N-butylpyrrolidone accounting for at least 50 wt % of the dope solvent and a water-soluble lactate derivative present as a cosolvent. A probe in the bath recirculation loop measures near-infrared absorbance, and a calibration based on bath samples converts the spectra to dissolved organic solvent concentration. A controller increases fresh-water makeup when solvent concentration exceeds the setpoint, and an overflow maintains bath level. A separate temperature loop regulates the recirculating bath through a heat exchanger.

Specific version of a part

Polyvinylpyrrolidone as pore modifier

A casting dope contains 17 wt % PVDF and 2 wt % polyvinylpyrrolidone, with the balance supplied by an N-butylpyrrolidone and methyl lactate blend. Polyvinylpyrrolidone changes the dope viscosity, and a portion diffuses into the water during coagulation and rinsing.

Methyl lactate co-solvent

Methyl lactate serves as the lactic acid ester in a binary solvent blend with N-butylpyrrolidone. During immersion in water, solvent diffuses out of the cast film and PVDF precipitates around the liquid-rich regions that form the pores.

Seventy percent n-butylpyrrolidone blend

A 100 g solvent charge contains 70 g N-butylpyrrolidone and 30 g methyl lactate. The solvent charge sets the 70 wt % fraction before PVDF and the water-soluble polymer are added.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2015/0057375 A1
Published
Feb 26, 2015
Filed
Jan 17, 2013
Class
A01N 25/02
Document BUS 2020/0216599 A1
Published
Jul 9, 2020
Filed
Mar 16, 2020
Class
C08G 18/0871
Claim 1
Document A
Document B
1.1a PVDF polymer, water soluble polymer and/or hydrogel “polymer H”, a solvent mixture comprising N-butylpyrrolidone and at least one water soluble lactate acid derivative, and optional additives
The method according to claim 22 wherein the second solvent is selected from the group consisting of N-ethyl-2-pyrrolidone (NEP), 1,5-dimethyl-pyrrolidone (DMP), dipropyleneglycol dimethyl ether (DPGDME), a mixture of ethyl lactate with a methyl ester derived from soya bean oil or corn oil, poly(ethylene glycol)dimethyl ether (commonly called “polyglyme”), diethylene glycol diethyl ether (commonly called “ethyl diglyme”), 1,3-dioxolanes, dimethyl sulphoxide (DMSO) and methyl-
A · US 2015/0057375 A1 · claim 23
In spite of the extremely high viscosity of the prepolymer (P), the N-n-butylpyrrolidone co-solvent demonstrated excellent solubilizing effect of the prepolymer (P) solids and allowed easy flow and incorporation of the hydrophobic prepolymer into the water phase.
B · US 2020/0216599 A1 · ¶ 255
1.2wherein the solvent mixture comprises at least 50 wt % or greater of N-butylpyrrolidone based on total weight of solvent.
Most preferably, the solvent mixture comprises at least 50 vol % of one or more of the pyrrolidones according to the invention.
A · US 2015/0057375 A1 · ¶ 29

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2. Both have a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The present invention is concerned with the use of selected pyrrolidones as solvent replacements in specific applications wherein N-methylpyrrolidone (NMP), N-ethyl-2-pyrrolidone (NEP), dimethyl formamide (DMF), N,N-dimethyl acetamide (DMAc), and mixtures thereof, is the appropriate solvent to be used.
A · US 2015/0057375 A1 · ¶ 1

Related claim parts: 1.1

This being said, the selection and the relative amounts of the polyurethane (PU) constitutional components (i.e. isocyanate, polyol component, chain extenders, emulsifiers, in particular internal emulsifiers, organic solvents, water, etc.), in the PUD formulation are thereby important for the targeted coating properties.
B · US 2020/0216599 A1 · ¶ 8

Related claim parts: 1.2

Therefore, there is a need for NMP to be substituted in many applications on medium term.
A · US 2015/0057375 A1 · ¶ 7
The present invention relates to aqueous polyurethane dispersions using at least a N—(C4-alkyl)-pyrrolidone as a prepolymer diluent, a dispersing agent and a coalescing agent wherein said aqueous polyurethane dispersions are very useful for the manufacture of films and coatings.
B · US 2020/0216599 A1 · ¶ 1
Pages 1 (11) to 11 (11)) that the pre-polymer mixing process is a versatile and straightforward process for the preparations for PUDs, thereby permitting a great variation in PU formulations.
B · US 2020/0216599 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0364541 A1, claim 1, first published 2026-11-23T03:43:43-05:00, https://patent.fyi/US20260364541/, SHA-256 072021687bdf13ed300a0c1ea54c7142c280d864554a82ffa8cadd64f2b51c81
First published
Permanent addresshttps://patent.fyi/US20260364541/
Content fingerprint (SHA-256)072021687bdf13ed300a0c1ea54c7142c280d864554a82ffa8cadd64f2b51c81
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi