Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Nonporous beads with gel shells
What ifWhat if solid glass beads carry a thin cationic gel shell?
Claim language“a porous support”
A cross-linked gel bearing quaternary ammonium groups coats each bead, and a covalently attached anionic polymer covers the gel exterior. Small acidic proteins diffuse through the outer layer and bind in the gel, while larger protein assemblies flow between the beads.
1.1Anionic gel in the pores
What ifWhat if a cross-linked anionic gel fills the support pores?
Claim language“a first cationic polymer”
A sulfonated acrylamide gel fills the pores of a polymethacrylate bead and binds small basic proteins at a pH below their isoelectric points. The gel mesh limits entry of larger assemblies, and a salt gradient releases the bound proteins.
1.1Linear chains on pore walls
What ifWhat if individually tethered linear cationic chains line the pores?
Claim language“which is cross-linked”
One end of each linear poly(methacryloyloxyethyltrimethylammonium chloride) chain attaches to a pore wall, and the hydrated chains extend into the pore liquid. The pore openings restrict entry of large protein assemblies, while smaller acidic proteins enter and bind to the quaternary ammonium groups.
1.2Neutral exterior polymer brush
What ifWhat if a neutral polyethylene glycol brush covers the bead exterior?
Claim language“a second anionic polymer”
Polyethylene glycol chains attach covalently to reactive groups on the outer face of the gel-filled bead. The hydrated brush limits surface adsorption of large protein assemblies, while small acidic proteins diffuse into the underlying gel and bind to cationic sites.
1.2Electrostatically adsorbed exterior layer
What ifWhat if electrostatic attraction holds an anionic polymer on the bead exterior?
Claim language“is covalently bonded”
High-molecular-weight poly(styrene sulfonate) adsorbs to exposed cationic sites at the bead surface, and its coil size limits penetration into the filled pores. The bed operates at low ionic strength to retain the adsorbed layer while small acidic proteins enter the pores and bind to the cationic gel.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Dye removal from textile rinse water
A packed column contains porous beads filled with a cross-linked cationic polymer and bearing a covalently attached sulfonated polymer on their exterior. Screened textile rinse water flows through the bed, and dissolved anionic dye molecules enter the pores and bind to the cationic network. A concentrated sodium chloride rinse displaces the retained dye into a separate collection tank.
Component substitution
Phosphonate polymer as the exterior layer
Poly(vinylphosphonic acid) replaces the exterior anionic polymer and supplies phosphonate groups at neutral pH. Porous silica beads contain a cross-linked cationic network, and vinyl groups are tethered to the bead exterior through silane linkages. Radical copolymerization of vinylphosphonic acid with the tethered vinyl groups forms the covalently attached exterior layer, and a water rinse removes soluble polymer.
Ceramic honeycomb as the porous support
A porous alumina honeycomb replaces a bed of individual porous beads. Its channel walls contain a cross-linked cationic polymer, and a sulfonated polymer is covalently grafted to the exposed channel faces through surface-bound silane linkers. A gasket seals the honeycomb into a housing so liquid travels along the channels and dissolved solutes diffuse into the wall pores.
Parameter or scale variation
Adjustable depth cartridge for adsorption trials
A column with a 25 mm internal diameter holds porous beads filled with a cross-linked cationic polymer and coated on the exterior with a covalently attached anionic polymer. A movable outlet frit sets the packed bed depth to 20, 40, or 80 mm, and a metering pump supplies liquid at 5 mL/min. The three settings give empty-bed contact times of approximately 2, 4, and 8 minutes for comparing solute breakthrough.
Combination with existing systems
Adsorption upstream of reverse osmosis
A cartridge packed with porous beads containing a cross-linked cationic network and a covalently attached exterior anionic polymer sits between a sediment filter and the high-pressure pump of a reverse osmosis system. The cationic network captures dissolved anions that bind under the feed conditions, and the pump sends cartridge effluent to the membrane module. Isolation valves direct cartridge regeneration liquid and the subsequent water rinse to a separate drain.
Automated or data-driven variant
Optical breakthrough control for twin beds
Two parallel columns contain porous beads filled with a cross-linked cationic polymer and bearing a covalently attached exterior anionic polymer. A controller reads optical absorbance from the common inlet and the active column outlet at the absorption maximum of the dissolved dye. When the outlet signal reaches 10% of the inlet signal for 30 seconds, actuated valves route the feed through the second column. A separate pump regenerates the first column with brine and rinses it with water until the outlet conductivity returns to its pre-service value.
Specific version of a part
Quaternary ammonium acrylamide gel
An aqueous mixture of acrylamide, a quaternary ammonium acrylamide comonomer, and methylenebisacrylamide fills the pores of a polymethacrylate bead. Radical polymerization forms a hydrated, cross-linked gel with fixed positive charges.
Cross-linked cationic dextran gel
Dextran bearing quaternary ammonium groups infiltrates the interconnected pores of a cellulose bead. A water-soluble diglycidyl ether links dextran chains through hydroxyl groups to form a cationic gel inside the support.
Amide-linked polyacrylate surface layer
Activated carboxyl groups on high-molecular-weight poly(acrylic acid) react with primary amines exposed on the exterior of the gel-filled bead to form amide bonds. The polymer coil exceeds the accessible gel mesh size, and unreacted carboxyl groups carry negative charge at neutral pH.
Epoxide-linked sulfonated polymer layer
An amine-terminated poly(styrene sulfonate) chain opens an epoxide at the outer face of the gel-filled bead and forms a covalent linkage. The chain size limits entry into the filled pores, and the pendent sulfonate groups carry negative charge across a broad pH range.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a porous support being filled with a first cationic polymer which is cross-linked, and
The method also includes filling pores of the porous dielectric material with a metal-containing material using an atomic layer deposition (ALD) process.
B · US 2019/0252313 A1 · abstract
1.2a second anionic polymer which is covalently bonded to the external surface of the cross-linked polymer-filled porous support.
The second component is an anionic polymer layer, which is coated onto the substrate comprising the therapeutic agent (e.g., coated over the therapeutic agent).
A · US 2005/0266072 A1 · ¶ 20
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.2. Only Document B has a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
There exists a need in the art to develop controlled release pharmaceutical formulations wherein the active ingredient in the formulation does not migrate through the controlled release coating during the manufacturing process and/or upon storage prior to administration of the formulation.
A · US 2005/0266072 A1 · ¶ 6
It is an object of the present invention to provide an oral controlled release pharmaceutical formulation having an improved stability of the therapeutic agent in the formulation by the inclusion of an anionic polymer in the formulation.
A · US 2005/0266072 A1 · ¶ 7
When patterning extremely small vias with extremely small pitches by such lithographic processes, several challenges present themselves, especially when the pitches are around 70 nanometers (nm) or less and/or when the critical dimensions of the via openings are around 35 nm or less.
B · US 2019/0252313 A1 · ¶ 5
Another such challenge is that the critical dimensions of the via openings generally tend to scale faster than the resolution capabilities of the lithographic scanners.
B · US 2019/0252313 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0364565 A1, claim 1, first published 2026-11-23T04:01:59-05:00, https://patent.fyi/US20260364565/, SHA-256 17faa2c70f32ed33900c19beff9d7962934250ab8b7a78a26e2036cfb0a518a1