Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
What ifWhat if magnesium oxide replaces a K oxide (K2O) as the basic promoter in the copper-silica catalyst?
Claim language“a K oxide (K2O)”
Magnesium oxide introduces surface basic sites that neutralize excess surface acidity on the support and suppress carbon-carbon bond cleavage to ethylene glycol and methane. During synthesis, magnesium nitrate and copper nitrate co-precipitate onto the silica carrier, followed by drying at 110 degrees Celsius and calcination at 450 degrees Celsius. Under glycerol hydrogenolysis at 200 degrees Celsius and 4 megapascals of hydrogen, the magnesium-promoted copper phase dehydrates glycerol to acetol and hydrogenates acetol to propylene glycol.
1.1Unpromoted binary copper and silica catalyst
What ifWhat if the catalyst omits a K oxide (K2O) and operates as a binary copper oxide and silica formulation?
Claim language“a K oxide (K2O)”
A binary copper oxide and silica catalyst prepared by ammonia evaporation forms copper phyllosilicate layers that yield dispersed metallic copper nanoparticles after hydrogen reduction at 300 degrees Celsius. The high copper surface area and interfacial copper-silanol sites catalyze glycerol dehydration to acetol and rapid hydrogenation to propylene glycol without an alkali modifier. Operating the fixed-bed reactor at 195 degrees Celsius with a liquid hourly space velocity of 1.0 per hour limits over-hydrogenolysis and maintains selectivity toward propylene glycol.
1.2Ruthenium metal active phase replaces copper
What ifWhat if metallic ruthenium nanoparticles replace a Cu oxide (CuO) as the active hydrogenation component?
Claim language“a Cu oxide (CuO)”
Ruthenium chloride is impregnated onto potassium-modified silica at a 3 weight percent metal loading, dried at 120 degrees Celsius, and reduced in flowing hydrogen at 350 degrees Celsius to form metallic ruthenium nanoparticles. The ruthenium surface dissociates molecular hydrogen and cleaves the terminal carbon-oxygen bond of glycerol at 170 degrees Celsius and 5 megapascals of hydrogen pressure. Surface potassium species moderate the hydrogenolysis activity of ruthenium so that carbon-carbon bond scission remains low and propylene glycol forms as the primary liquid product.
1.3Porous activated carbon replaces silica support
What ifWhat if porous activated carbon replaces silica (SiO2) as the high-surface-area support?
Claim language“silica (SiO2)”
Acid-washed activated carbon granules with a specific surface area above 800 square meters per gram resist hydrothermal leaching in hot aqueous glycerol solutions where oxide supports gradually dissolve. Copper nitrate and potassium carbonate are loaded onto the carbon surface via incipient wetness impregnation, dried under nitrogen at 110 degrees Celsius, and thermally decomposed in inert gas at 350 degrees Celsius to prevent carbon oxidation. The resulting carbon-supported copper and potassium catalyst operates in aqueous glycerol at 200 degrees Celsius and 4 megapascals of hydrogen to produce propylene glycol.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Hydrogenation of furfural using potassium copper silica catalyst
A packed-bed stainless steel reactor holds a reduced potassium oxide, copper oxide, and silica catalyst bed to hydrogenate biomass-derived furfural into furfuryl alcohol. Liquid furfural dissolved in isopropanol at 15 wt % enters the top of the reactor alongside compressed hydrogen gas at 3.0 MPa and 160 °C. The alkaline potassium oxide sites suppress furan ring hydrogenation and polymerization while the reduced copper crystallites selectively hydrogenate the aldehyde carbonyl group. The effluent passes through a gas-liquid separator to recover unreacted hydrogen for recycle and deliver crude furfuryl alcohol to a distillation column.
Component substitution
Alumina support replacing silica in potassium copper catalyst
Gamma-alumina powder with a specific surface area of 180 m2/g replaces silica as the structural support for the potassium oxide and copper oxide active phases. Sequential wet impregnation loads the gamma-alumina with aqueous copper nitrate and potassium carbonate solutions, followed by drying at 110 °C and calcination at 500 °C in air. During glycerol hydrogenolysis at 220 °C and 4.0 MPa hydrogen pressure, electron-accepting acid sites on the alumina surface promote glycerol dehydration to acetol while dispersed copper particles hydrogenate acetol to propylene glycol. The potassium oxide component neutralizes strong acid sites on the alumina to limit coke deposition and side-product formation.
Cesium oxide replacing potassium oxide as alkali promoter
Cesium oxide replaces potassium oxide as the alkali metal oxide promoter within the copper oxide and silica nanocomposite framework. Coprecipitation of copper nitrate, cesium nitrate, and colloidal silica using aqueous ammonium carbonate yields a precursor gel that undergoes washing, drying at 120 °C, and calcination at 450 °C for 4 hours. The larger ionic radius and stronger basicity of cesium ions modify the electronic density of adjacent metallic copper sites after reduction in flowing hydrogen at 280 °C. In a trickle-bed reactor fed with aqueous glycerol, the cesium-promoted copper surface accelerates carbon-oxygen bond cleavage while maintaining copper particle dispersion over extended operating cycles.
Parameter or scale variation
Pelletized catalyst bed for high-pressure continuous glycerol hydrogenolysis
The potassium oxide, copper oxide, and silica powder blends with 2 wt % graphite binder and compresses into cylindrical extrudates measuring 3 mm in diameter and 5 mm in length for fixed-bed continuous operation. A tubular reactor of 250 mm internal diameter holds 45 kg of the pelletized catalyst with a combined potassium oxide and copper oxide loading of 35 wt % and a silica support balance of 65 wt %. Neat glycerol preheated to 240 °C enters the reactor with hydrogen at 6.5 MPa, a hydrogen-to-glycerol molar ratio of 12:1, and a liquid hourly space velocity of 1.5 h-1. The pellet geometry keeps the pressure drop across the 2.5 m catalyst bed below 80 kPa while sustaining continuous propylene glycol production at 65 kg/h.
Combination with existing systems
Integrated biodiesel transesterification and glycerol hydrogenolysis process unit
The potassium oxide, copper oxide, and silica hydrogenolysis reactor connects directly downstream of a continuous vegetable oil transesterification unit and a vacuum methanol stripping column. Crude glycerol exiting the biodiesel phase separator undergoes acidification with phosphoric acid, filtration to remove precipitated fatty acid salts, and ion-exchange polishing to reduce sodium and chloride concentrations below 10 ppm. The purified glycerol stream dilutes to 40 wt % with process condensate and flows through a feed-effluent heat exchanger into the hydrogenolysis reactor containing the reduced catalyst. A three-column distillation train downstream of the reactor separates water, unreacted glycerol for recycle, and refined propylene glycol, using low-pressure steam recovered from the exothermic hydrogenolysis jacket to reboil the methanol recovery column.
Automated or data-driven variant
Closed-loop reactor control using inline infrared spectroscopy
An inline mid-infrared spectrometer with a diamond attenuated total reflectance probe mounts in the liquid outlet line of the potassium oxide, copper oxide, and silica hydrogenolysis reactor to measure glycerol, acetol, and propylene glycol concentrations every 30 seconds. Thermocouples spaced at 20 cm intervals along the catalyst bed and a thermal mass flow meter on the hydrogen inlet transmit real-time process readings to a model predictive controller. The controller runs a kinetic deactivation model that tracks copper sintering and adjusts the reactor jacket temperature setpoint between 190 °C and 235 °C and the liquid feed rate to hold glycerol conversion above 92 %. When the model detects selectivity loss below a programmed threshold, the control system initiates an automated nitrogen purge and switches flow to a parallel standby reactor for catalyst regeneration.
Specific version of a part
Potassium oxide from carbonate impregnation
Potassium oxide is introduced at 1 to 3 weight percent loading by incipient wetness impregnation of an aqueous potassium carbonate solution onto a preformed copper-silica precursor. Drying at 110 degrees Celsius for 12 hours followed by calcination in flowing air at 450 degrees Celsius decomposes the carbonate salt into finely dispersed potassium oxide species across the pore walls. This controlled alkali loading neutralizes acidic silanol groups without blocking the exposed copper active surface.
Nanoscale copper oxide via ammonia evaporation
Copper oxide is formed at 20 to 35 weight percent loading by dissolving copper nitrate in aqueous ammonia to generate a copper-ammonia complex, mixing with colloidal silica, and evaporating ammonia at 80 degrees Celsius until the pH reaches 7. Calcination of the precipitated copper phyllosilicate at 450 degrees Celsius produces copper oxide crystallites smaller than 5 nanometers that resist sintering during hydrogen reduction. The uniform copper dispersion maximizes exposed copper metal surface area per gram of catalyst.
Ordered mesoporous silica with uniform channels
The silica carrier consists of hydrothermally synthesized mesoporous silica particles with hexagonal pore channels of 6 to 8 nanometers in diameter and a nitrogen physisorption surface area of 500 to 700 square meters per gram. The wide, uniform pore geometry accommodates viscous aqueous glycerol feeds and facilitates diffusion of propylene glycol away from active copper sites before secondary dehydration occurs. Thick amorphous silica pore walls provide mechanical crush strength and resistance to structural collapse under elevated temperature and water vapor pressure.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
TABLE 1 Mass of the alkali compounds on a 0.3 mol X to 1 mol Mo ratio at 5.00 grams of ATM. (X = alkali metal) Compound Mass (grams) Potassium Carbonate 0.40 g Lithium Hydroxide 0.14 g Cesium Acetate 1.10 g ATM 5.00 g
A · US 10,316,254 B2 · ¶ 49
1.2a Cu oxide (CuO); and
In particular, supported CuO catalysts that include modified support, promoters or co-active phases, or combinations thereof, provide supported catalysts with increased activity and selectivity at lower reaction temperatures.
B · US 10,906,852 B2 · ¶ 6
1.3silica (SiO2).
The catalyst support can include alumina, carbon, silica, zirconia, or combinations thereof.
B · US 10,906,852 B2 · ¶ 7
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.1. Only Document B has a passage for 1.21.3.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
There remains a need for additional catalysts and methods to producing such catalyst for Fischer-Tropsch processes.
A · US 10,316,254 B2 · ¶ 2
It is contemplated that any embodiment discussed herein can be implemented with respect to any method or composition of the invention, and vice versa.
A · US 10,316,254 B2 · ¶ 6
In particular, supported CuO catalysts that include modified support, promoters or co-active phases, or combinations thereof, provide supported catalysts with increased activity and selectivity at lower reaction temperatures.
B · US 10,906,852 B2 · ¶ 6
Further the supported catalysts and process conditions can be fine-tuned to increase the efficiency of specific feedstock compositions arising from particular commercial processes (e.g., DCPD isoprene co-extraction process, etc.).
B · US 10,906,852 B2 · ¶ 6
This approach has been common over the past decade, with examples such as potassium catalyzed soot oxidation supported by TiO2, ZrO2, Al2O3, SiO2, etc.
C · US 9,592,490 B2 · ¶ 4
Related claim parts: 1.3
Document C: US 9,592,490 B2, published Mar 14, 2017. Cited for this statement only.
Cite aspatent.fyi, US 2026/0364572 A1, claim 1, first published 2026-11-23T04:01:59-05:00, https://patent.fyi/US20260364572/, SHA-256 5508731c4ad6652575516c801cd9c267cc97a1ed3bb44a732350c7e3111faf53