1.1Self-supporting cobalt oxide granules
Compacted cobalt oxide powder forms porous granules that retain their shape in a fixed bed. Flowing hydrogen penetrates the connected pores and reduces exposed oxide to metallic cobalt.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Compacted cobalt oxide powder forms porous granules that retain their shape in a fixed bed. Flowing hydrogen penetrates the connected pores and reduces exposed oxide to metallic cobalt.
A heated fixed bed holds cobalt oxide on silica while dry hydrogen flows through it at 350 °C. The gas stream carries away water formed as the oxide reduces to metallic cobalt.
Molten paraffin wax coats the reduced cobalt particles under inert gas and solidifies on cooling. The receiving vessel remelts and drains the bulk wax, then hydrogen treatment restores the active surface.
An inert gas purge clears residual carbon monoxide before hydrogen enters the bed. The second hydrogen flow at 300 °C removes adsorbed carbon monoxide through desorption and hydrogenation.
Hydrogen partially reduces the supported iron oxide, and subsequent carbon monoxide exposure forms iron carbide. The carbide sites convert hydrogen and carbon monoxide into hydrocarbons through surface chain growth.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A steelworks conversion unit uses carbon monoxide recovered from furnace offgas and hydrogen supplied through a separate header. A scrubber removes particulates, and a gas separation train recovers carbon monoxide and removes sulfur compounds before the gas enters a buffer vessel. The unit reduces a supported cobalt bed, passivates it with carbon monoxide from the buffer vessel, and reduces it a second time. A mixing header then combines the purified carbon monoxide with hydrogen for conversion over the activated bed.
A silicon carbide honeycomb with a porous silica washcoat serves as the cobalt support. Cobalt nitrate solution impregnates the washcoat, and drying and calcination form cobalt oxide on the channel walls. A pressure shell holds the monolith and seals its perimeter to direct gas through the channels. The same channels carry the first reducing gas, carbon monoxide for passivation, the second reducing gas, and the hydrogen and carbon monoxide feed in sequence.
Four parallel pressure vessels each hold 25 kilograms of supported cobalt catalyst and have separate feed selection valves and backpressure regulators. Each vessel undergoes first reduction at 240 °C, carbon monoxide passivation at 180 °C and 12 bara, and second reduction at 220 °C. The vessels enter the sequence at 60-minute intervals to spread demand on the shared gas headers. Each vessel switches to the hydrogen and carbon monoxide feed after completing its own activation sequence.
A multitubular reactor holds supported cobalt pellets inside tubes surrounded by a boiling water circuit connected to a steam drum. A separate thermal fluid circuit preheats the incoming gases during first reduction, carbon monoxide passivation, and second reduction. During hydrocarbon synthesis, water on the shell side absorbs reaction heat and returns to the drum as a steam and water mixture. The drum separates steam for a plant heating header and returns liquid water to the reactor shell.
A supported cobalt reactor carries out first reduction, carbon monoxide passivation, and second reduction before receiving the hydrogen and carbon monoxide feed. A heated high-pressure separator collects the heavy hydrocarbon liquid from the synthesis effluent and sends it through a heated transfer line. The liquid mixes with hydrogen upstream of a trickle-bed hydrocracker containing nickel and tungsten on an acidic silica-alumina support. A downstream fractionator separates the upgraded products and recycles the heavy fraction to the hydrocracker.
A programmable controller reads bed thermocouples, inlet and outlet flow meters, an outlet moisture analyzer, and a gas analyzer that measures carbon monoxide and methane. During first reduction, the controller tracks the decline in outlet moisture above the inlet baseline, and during passivation it calculates carbon monoxide uptake from the inlet and outlet molar flows. During second reduction, it tracks the return of methane and moisture to their commissioned endpoint thresholds. The controller sequences the gas valves through inert purges and admits synthesis gas when the final endpoint and the bed temperature and pressure conditions are satisfied.
An iron-based catalyst promotes reverse water-gas shift, generating carbon monoxide and water inside the bed. Iron carbide sites use the generated carbon monoxide and hydrogen to form hydrocarbons.
A measured volume of aqueous cobalt nitrate fills the pores of silica pellets. Drying and calcination in air convert the deposited salt to cobalt oxide within the pellets.
Dry hydrogen flows through a fixed bed of supported cobalt oxide at 240 °C and 3 bara. An outlet moisture analyzer tracks the water released during oxide reduction.
After reduction at 240 °C, an inert gas purge clears hydrogen from the bed and the bed cools to 180 °C. A back-pressure regulator holds the carbon monoxide exposure at 8 bara while the gas contacts the reduced cobalt surface.
A manifold distributes hydrogen and carbon monoxide at a 2:1 molar ratio to parallel tubes packed with activated cobalt catalyst. Shell-side coolant removes reaction heat, and a downstream separator collects condensed hydrocarbons and water.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
In a further embodiment, the present invention relates to a method for preparing the catalyst composition as described herein, wherein said method comprises the steps of: (a) preparing a mixture comprising activated carbon support particles having a BET surface area of 700-1500 m2/g and a solution comprising soluble Co- and Mo-comprising salts;A · US 2016/0271593 A1 · ¶ 25
Cobalt oxide supported on titanium dioxide was manufactured as a catalyst by impregnating titanium dioxide powder with an aqueous solution of cobalt nitrate hexahydrate, followed by extrusion of the formed paste, and then drying and calcining to yield catalyst extrudates with a cobalt loading of 10% by weight of catalyst and a manganese loading of 1% by weight of catalyst.B · US 2018/0037825 A1 · ¶ 29
In the reducing step (d) or (d2) as described herein, the calcined catalyst precursor is contacted with a reducing agent. This is to reduce the comprised Co and Mo to its metallic state and results in the formation of metallic Co and Mo as comprised in the catalyst composition as defined herein.A · US 2016/0271593 A1 · ¶ 41
Each channel of the microreactor underwent the same drying procedure in parallel, before the catalysts were activated according to the following protocols under 100% H2 gas at a GHSV of 3800 h−1 and pressure of 1 atm: Example 1 (inventive): From room temperature ramped to 150° C. at a rate of 2° C./min, then ramped to 200° C. at a rate of 1° C./min, before dwelling at 200° C. for 15 hours.B · US 2018/0037825 A1 · ¶ 29
In a further embodiment, the present invention relates to a process for producing a product stream comprising alcohols comprising contacting the catalyst composition as described herein with a gaseous mixture comprising hydrogen and carbon monoxide (syngas mixture).A · US 2016/0271593 A1 · ¶ 48
This invention relates to Fischer-Tropsch (FT) processes for the conversion of a feed comprising a mixture of carbon monoxide gas and hydrogen gas (e.g. synthesis gas (syngas)) to hydrocarbons over a cobalt catalyst comprising a titanium dioxide (titania) support, catalysts therefor and uses of/processes to produce said catalysts.B · US 2018/0037825 A1 · ¶ 1
An empty cell means only that no passage was reproduced there.
Both have a passage for 1.1 1.2 1.5.
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Gaseous mixtures comprising hydrogen (H2) and carbon monoxide (CO) can be converted into a hydrocarbon product stream by a catalytic process known as Fischer-Tropsch synthesis (F-T synthesis).A · US 2016/0271593 A1 · ¶ 2
Related claim parts: 1.5
A major drawback of conventional catalysts for producing alcohols by F-T synthesis is that the selectivity of the process for alcohols is relatively low.A · US 2016/0271593 A1 · ¶ 5
It was surprisingly found that the selectivity for alcohols can be increased by using the carbon supported cobalt molybden urn catalyst as described herein in a process for producing alcohols from a feed stream comprising hydrogen and carbon monoxide.A · US 2016/0271593 A1 · ¶ 1
It has thus been thought desirable to reduce as much of the cobalt present as possible in order to improve the activity of the resultant catalyst, requiring harsh conditions, such as high temperature.B · US 2018/0037825 A1 · ¶ 2
Surprisingly, it has now been found that, provided a hydrogen gas reduction step is used, milder reduction conditions (e.g. lower temperature) may be utilised while still achieving at least acceptable, and even enhanced, catalyst activity and C5+ selectivity in an FT process.B · US 2018/0037825 A1 · ¶ 2
patent.fyi, US 2026/0364574 A1, claim 1, first published 2026-11-23T04:01:59-05:00, https://patent.fyi/US20260364574/, SHA-256 483cbbb4c8726ea262ecc7b779a28e2b9b2d1ce0153fe4caebe367db81c2476e