Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Unsupported cobalt powder
What ifWhat if the cobalt precursor is a self-supporting powder dispersed in liquid wax?
Claim language“disposed on a support”
Precipitation and calcination produce cobalt oxide particles without a separate carrier. Hydrogen reduction forms metallic cobalt, and recirculating wax keeps the particles suspended while gas bubbles supply the reactants.
1.2Wax barrier for handling
What ifWhat if a solid wax coating protects the cobalt surface during handling?
Claim language“contacting the first catalyst material with carbon monoxide”
Reduced cobalt catalyst granules receive a molten paraffin coating under nitrogen, and the coating solidifies on cooling. A hot paraffin flush under nitrogen melts and removes the coating before hydrogen conditioning.
1.2Hot carbon monoxide conditioning
What ifWhat if carbon monoxide conditioning takes place above 300 °C?
Claim language“T1 is at most 300 °C”
A fixed bed at 320 °C receives a short pulse of carbon monoxide diluted in nitrogen at 1.2 bar absolute. The pulse forms carbon-containing surface species on the cobalt precursor, and hydrogen treatment converts those species and restores metallic cobalt sites.
1.3Hydrogen reduction at low pressure
What ifWhat if hydrogen reduction takes place at 2 bar absolute?
Claim language“P2 is at least 10 bara”
After carbon monoxide conditioning at 1 bar absolute, flowing dry hydrogen reduces cobalt oxide at 290 °C and 2 bar absolute. The gas stream carries water out of the bed, and the reactor is pressurized for synthesis after reduction.
1.3Higher temperature hydrogen activation
What ifWhat if hydrogen activation takes place at 350 °C?
Claim language“T2 is at most 300 °C”
A supported cobalt oxide bed receives flowing hydrogen at 350 °C and 15 bar absolute after carbon monoxide conditioning at 5 bar absolute. Hydrogen converts cobalt oxide to metallic cobalt, and the bed cools under hydrogen before synthesis gas enters.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Associated gas conversion at oil fields
A field skid connects a gas cleanup unit and compact reformer to a fixed-bed synthesis reactor containing supported cobalt oxide. A separate carbon monoxide manifold supplies the passivation gas, and a hydrogen manifold supplies the reducing gas at a pressure of at least 10 bara and at least the passivation pressure. After reduction, the skid feeds reformer synthesis gas to the bed and collects condensable hydrocarbons in a cooled separator.
Component substitution
Silicon carbide foam catalyst support
An open-cell silicon carbide foam with a porous silica washcoat supports the cobalt oxide. The washcoat is impregnated with aqueous cobalt nitrate, dried and calcined to form cobalt oxide, and the foam is sealed around its perimeter in a tubular reactor so gas flows through the cells. The gas manifold supplies carbon monoxide for passivation, hydrogen at a pressure of at least 10 bara and at least the passivation pressure for reduction, and then a hydrogen and carbon monoxide mixture for synthesis.
Parameter or scale variation
Numbered up parallel catalyst tubes
A pilot reactor contains 24 parallel tubes with a 20 mm internal diameter and a 1 m packed length, each filled with 1 mm supported cobalt oxide pellets. Calibrated inlet orifices distribute gas across the tubes, and a circulated heat-transfer fluid controls the shell-side temperature. The common manifold supplies carbon monoxide at 15 bara and 210 °C for passivation, hydrogen at 20 bara and 275 °C for reduction, and then a hydrogen and carbon monoxide mixture for synthesis.
Combination with existing systems
Hydrogen recovery from synthesis tail gas
A pressure swing adsorption unit connects to the synthesis tail-gas line downstream of a cooled separator and a coalescing filter. During steady operation, the unit recovers hydrogen from the dry tail gas, and a compressor fills a buffer vessel that supplies the catalyst reduction manifold. During a subsequent startup, carbon monoxide passivates the supported cobalt bed, stored hydrogen reduces it at a pressure of at least 10 bara and at least the passivation pressure, and synthesis gas then enters the activated bed.
Synthesis heat recovery for gas preheating
A shell-side steam drum on a multitubular synthesis reactor supplies steam to an indirect heater on the activation gas manifold. Separate carbon monoxide and hydrogen inlet lines feed the heater through interlocked valves, and an electric trim heater brings each selected gas to its passivation or reduction setpoint. An auxiliary steam header supplies heat during a cold start, and steam from an operating reactor supplies the common header during catalyst activation in a parallel train.
Automated or data-driven variant
Reduction endpoint from outlet gas analysis
A programmable controller reads bed thermocouples, a pressure transmitter and a water vapor analyzer on a heated outlet sampling line. The controller records the inlet hydrogen moisture baseline, passivates the bed with carbon monoxide, purges the manifold with nitrogen and starts hydrogen reduction at a pressure of at least 10 bara and at least the passivation pressure. After the outlet water signal rises and returns within a commissioned band around the inlet baseline for a preset hold time, the controller verifies bed temperature and pressure and ramps in the synthesis gas feed.
Specific version of a part
Cobalt oxide on porous alumina
An aqueous cobalt nitrate solution fills the pore volume of porous alumina extrudates. Drying and air calcination convert the nitrate to cobalt oxide distributed along the pore walls.
Dilute carbon monoxide passivation
A fixed bed receives 5 mole percent carbon monoxide in nitrogen at 200 °C and a total pressure of 5 bar absolute. Carbon monoxide contacts the supported cobalt precursor, and a nitrogen purge clears the gas phase before reduction.
Pressurized flowing hydrogen reduction
Following passivation at 5 bar absolute, dry hydrogen flows through the catalyst bed at 280 °C and 15 bar absolute. The hydrogen reduces cobalt oxide, and continuous flow removes water from the bed.
Synthesis in cooled catalyst tubes
A mixture with a hydrogen to carbon monoxide molar ratio near 2 to 1 enters tubes packed with activated cobalt catalyst at 220 °C and 25 bar absolute. Boiling water on the shell side removes reaction heat, and downstream cooling condenses liquid hydrocarbons and water.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1(a) providing a first catalyst material comprising cobalt (e.g., in the form of oxide) disposed on a support;
The process of making supported cobalt oxide catalysts comprises: impregnation of cobalt compounds on a substrate; the formation of cobalt oxide by thermal decomposition of the cobalt compounds.
A · US 2007/0004582 A1 · ¶ 7
Cobalt oxide supported on titanium dioxide was manufactured as a catalyst by impregnating titanium dioxide powder with an aqueous solution of cobalt nitrate hexahydrate, followed by extrusion of the formed paste, and then drying and calcining to yield catalyst extrudates with a cobalt loading of 10% by weight of catalyst and a manganese loading of 1% by weight of catalyst. 0.25 g of the catalyst was loaded into the quartz u-tube reactor of a TPR unit and subjected to reductio
B · US 2017/0368546 A1 · ¶ 36
1.2(b) contacting the first catalyst material with carbon monoxide at a first pressure (P1) and a first temperature (T1) to provide a passivated catalyst material, wherein P1 is at least 1 bara and at most 50 bara, and T1 is at most 300 °C;
1.3(c) contacting the passivated catalyst material with a reducing agent at a second temperature (T2) and a second pressure (P2) to form an activated catalyst material, wherein P2 is at least 10 bara, and wherein P2 is greater than or equal to P1, and wherein T2 is at most 300 °C; and
The surface activation is engaged by immersion of the catalyst in a metal borohydride solution for 5˜30 minutes.
A · US 2007/0004582 A1 · ¶ 27
This aspect may also desirably include a step of pre-treating a catalyst composition comprising titanium dioxide support and oxidic cobalt (e.g. cobalt oxide) or a cobalt compound decomposable thereto by reduction to produce the catalyst above.
B · US 2017/0368546 A1 · ¶ 3
1.4(d) contacting the activated catalyst material with a mixture of hydrogen and carbon monoxide.
As indicated above, the present invention provides, in a first aspect, a process for the conversion of a feed comprising a mixture of hydrogen and carbon monoxide, preferably in the form of a synthesis gas mixture, to hydrocarbons, which process comprises contacting the feed with a reductively activated catalyst composition as hereinbefore described.
B · US 2017/0368546 A1 · ¶ 25
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document B has a passage for 1.4. Both have a passage for 1.11.3. Both are classified in CPC B01J, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The catalyst employed in the present invention may be obtained by pre-treating a catalyst composition comprising titanium dioxide support and oxidic cobalt or a cobalt compound decomposable thereto, with a reducing agent.
B · US 2017/0368546 A1 · ¶ 6
Related claim parts: 1.11.3
From a practical point of view, a high performance catalyst for hydrogen generation having low production cost is highly desirable.
A · US 2007/0004582 A1 · ¶ 5
The invention also relates to a method of making, sintering, activating a cobalt oxide catalyst, regenerating a deactivated cobalt oxide catalyst, and the use of the catalyst for oxidative reaction on various chemical systems.
A · US 2007/0004582 A1 · ¶ 1
Surprisingly, it has now been found that a limited degree (or extent) of reduction of a titanium dioxide supported cobalt catalyst, i.e. reduction achieved to a lower level, (commensurately the degree of reduction of the catalyst when it is subsequently exposed to the feed), may be utilised while still achieving at least acceptable, and even enhanced, catalyst activity and C5+ selectivity in an FT process.
B · US 2017/0368546 A1 · ¶ 2
The reducing gas referred to above may particularly be carbon monoxide or hydrogen.
B · US 2017/0368546 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0364575 A1, claim 1, first published 2026-11-23T04:01:59-05:00, https://patent.fyi/US20260364575/, SHA-256 6f81dae127ee7f3229f66f58ed6c3aa1f22d0d4dabc5bed12a6de830359af55c