Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Dry unfilled pores before metal application
What ifWhat if the pores remain dry and unfilled before metal application?
Claim language“introducing a medium into pores”
Dry porous support particles enter a rotating drum without prior introduction of a pore-filling liquid or solid. An atomized mist of metal precursor sprays onto the tumbling exterior surfaces at a liquid-to-solid ratio below 20 percent of the total pore volume. Rapid thermal drying at 120 degrees Celsius fixes the active metal near the outer shell before deep capillary migration occurs.
1.1Pellets larger than two millimeters
What ifWhat if the starting porous supports are extruded cylinders with diameters between 2 mm and 5 mm?
Claim language“a diameter of less than 1 mm”
Porous oxide paste passes through a die plate with 3 mm circular orifices and undergoes cutting to 4 mm lengths before calcination at 550 degrees Celsius. The resulting millimeter-scale pellets pack into a stationary catalytic bed downstream of a regenerator flue gas outlet. Flue gas containing carbon monoxide flows through the packed bed at a gas hourly space velocity of 20,000 per hour, where the external surface oxidizes carbon monoxide to carbon dioxide with low pressure drop.
1.1Continuous honeycomb monolith support structure
What ifWhat if the catalyst carrier is a single extruded ceramic honeycomb monolith with straight parallel channels?
Claim language“plurality of starting porous particles”
An extruded cordierite honeycomb block with 400 cells per square inch serves as a stationary substrate in the flue gas exhaust duct. A thin catalytic washcoat containing noble metal deposits onto the channel walls by dip coating followed by air-knife clearing and calcination at 500 degrees Celsius. Exhaust gas streams laminarly through the parallel channels, diffusing carbon monoxide to the coated walls for oxidation without particle entrainment.
1.2Vapor-phase organometallic metal deposition
What ifWhat if the metal precursor is delivered as a dry vapor in a carrier gas stream?
Claim language“an aqueous salt solution”
A volatile organometallic noble metal complex sublimes at 150 degrees Celsius into a dry nitrogen carrier gas stream inside a fluidized-bed reactor. The vapor contacts the heated porous particles at 250 degrees Celsius and reacts with surface hydroxyl groups to form a uniform monolayer of metal complexes. A subsequent oxidative calcination step at 450 degrees Celsius removes the organic ligands and leaves dispersed metallic crystallites on the particle surface.
1.2Copper and cerium oxide active phase
What ifWhat if the active oxidation catalyst consists of copper oxide and cerium oxide?
Claim language“one or more Group VIII noble metals”
Porous support particles undergo impregnation with a solution containing copper nitrate and cerium nitrate at a molar ratio of 1 to 4. Drying at 110 degrees Celsius and calcination at 600 degrees Celsius convert the nitrates into dispersed copper oxide clusters anchored on fluorite-structured cerium oxide. Under regenerator temperatures between 650 and 730 degrees Celsius, lattice oxygen from the cerium-copper interface oxidizes carbon monoxide to carbon dioxide and replenishes from molecular oxygen in the air stream.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Volatile organic compound oxidation catalyst for industrial exhaust
Porous alumina-silica microspheres with diameters of 200 to 600 micrometers are pre-filled with a non-polar aliphatic hydrocarbon liquid via incipient wetness addition in a rotary drum mixer. The pre-filled microspheres are contacted with an aqueous palladium nitrate solution to deposit palladium near the outer shell of each particle, followed by drying at 120 degrees C and calcination at 500 degrees C in air. The resulting eggshell-impregnated particles are packed into a perforated annular cartridge installed inside a thermal recuperative exhaust duct for solvent-laden air streams from coating ovens. During operation at 250 to 400 degrees C, volatile organic compounds diffuse into the outer active shell and oxidize to carbon dioxide and water with reduced pressure drop and low noble metal loading.
Component substitution
Ceria-zirconia particles impregnated with copper and manganese salts
Porous ceria-zirconia mixed oxide microspheres with diameters of 50 to 150 micrometers replace the silica-alumina support and are tumbled in a double-cone blender while a low-viscosity dimethylpolysiloxane fluid is sprayed to fill 70 percent of the internal pore volume. The oil-loaded microspheres are contacted with an aqueous solution of copper(II) nitrate and manganese(II) nitrate in place of a Group VIII noble metal salt solution, confining the transition metal precursors to the outer 15 micrometers of each particle. After draining excess liquid on a vacuum belt filter, the solids undergo thermal treatment at 550 degrees C in flowing air to decompose the nitrates and remove the silicone pore-filling medium. This configuration produces a noble-metal-free oxidation promoter with an active mixed-oxide shell supported on an oxygen-storing core.
Molten paraffin wax medium for selective pore blocking
Spray-dried zeolite-alumina microspheres with diameters of 70 to 120 micrometers are heated to 75 degrees C in a jacketed ribbon blender and mixed with molten paraffin wax having a melting point of 58 degrees C to fill the interior pore network. The mixture cools to 30 degrees C under continuous agitation so the wax solidifies inside the inner pores while leaving the outer pore mouths accessible. The wax-filled particles are slurried in an aqueous solution of ruthenium(III) chloride and palladium(II) chloride at 25 degrees C, depositing the Group VIII noble metals onto the unblocked exterior shell. Subsequent heating in a fluidized-bed furnace at 480 degrees C under flowing air volatilizes and oxidizes the solid wax while converting the metal salts into dispersed catalytic metal oxide clusters.
Parameter or scale variation
Millimeter-scale porous pellets with short-contact eggshell impregnation
Cylindrical gamma-alumina extrudates measuring 2.5 millimeters in diameter and 4.0 millimeters in length are pre-saturated to 85 percent of their 0.65 cubic centimeters per gram pore volume with deionized water at 25 degrees C. The hydrated pellets pass through a vibrating perforated trough for a residence time of 45 seconds while sprayed with an aqueous chloroplatinic acid solution heated to 60 degrees C at a platinum concentration of 1.2 grams per liter. Rapid capillary exchange limits platinum penetration to an outer ring thickness of 120 to 180 micrometers before the pellets enter a continuous belt dryer operating at 140 degrees C for 20 minutes. Calcination in a rotary kiln at 520 degrees C for 2 hours yields fixed-bed oxidation pellets containing 0.15 weight percent platinum concentrated at the exterior surface.
Combination with existing systems
Inline impregnation unit coupled to spray-drying and calcination
A spray dryer producing 60 to 100 micrometer clay-alumina microspheres discharges directly into a pneumatic cyclone separator feeding a twin-shaft paddle mixer. Inside the first zone of the mixer, ultrasonic atomizing nozzles inject a hydrophobic paraffinic pore-filling liquid into the warm particles, while the second zone sprays an aqueous tetraammineplatinum(II) nitrate solution onto the conditioned bed. The impregnated wet cake drops through a rotary airlock into a multi-stage fluidized-bed dryer and calciner operating at 150 degrees C in the drying stage and 600 degrees C in the calcining stage. Off-gas from the calciner routes through a condenser and activated-carbon recovery unit that captures vaporized paraffin for recirculation to the first mixing zone.
Automated or data-driven variant
Closed-loop sensor control of pore filling and impregnation
A programmable logic controller regulates the pore-filling and noble-metal impregnation sequence using inline near-infrared moisture sensors, vibrating-tube mass flow meters, and an automated X-ray fluorescence analyzer positioned downstream of the drying stage. Before each batch enters the rotary impregnator, an automated nitrogen-physisorption sampling loop measures particle pore volume and feeds the value to a regression model that computes the required pore-filling medium dose and aqueous platinum salt flow rate. During spraying, the near-infrared probe tracks surface wetness in real time and adjusts nozzle air pressure and drum rotation speed to maintain uniform coating without agglomeration. After drying, the X-ray fluorescence analyzer verifies metal loading and shell distribution, updating the model parameters automatically for subsequent batches.
Specific version of a part
Water pore pre-filling of alumina microspheres
Spray-dried gamma-alumina microspheres with a mean particle diameter of 70 micrometers and a pore volume of 0.45 milliliters per gram tumble in a rotary cone blender. Deionized water sprays onto the moving bed in an amount equal to 85 percent of the measured nitrogen pore volume to fill the interior pore network through capillary suction. A 15-minute aging interval at ambient temperature equilibrates liquid distribution inside the particle cores before metal impregnation.
Clay-alumina microspheres with aqueous organic medium
Starting porous particles consist of 50 weight percent kaolin clay, 35 weight percent pseudo-boehmite alumina, and 15 weight percent silica sol formed by spray drying to a particle size distribution between 45 and 90 micrometers. An aqueous solution containing 10 weight percent citric acid enters the particle pores by vacuum-assisted spraying at 50 kilopascals absolute pressure. The organic medium occupies the internal mesopores and buffers the local pore pH prior to noble metal contact.
An aqueous solution of tetraammineplatinum nitrate containing 500 parts per million platinum by weight is adjusted to pH 9.5 with ammonium hydroxide. Fine spray nozzles atomize the salt solution onto the pre-filled porous particles inside a fluidized-bed coater at 30 degrees Celsius to deposit 300 to 800 parts per million platinum on a dry catalyst basis. The impregnated particles dry at 120 degrees Celsius for 2 hours and undergo air calcination at 540 degrees Celsius to form dispersed platinum crystallites.
Bimetallic platinum and palladium immersion contacting
Pre-filled porous particles immerse in an agitated aqueous bath containing both palladium nitrate and platinum nitrate at a palladium-to-platinum weight ratio of 3 to 1. Gentle stirring at 40 degrees Celsius for 30 minutes promotes electrostatic adsorption of the noble metal cations onto the outer surface regions of the particles. Vacuum filtration separates the loaded solids from the supernatant liquid, followed by thermal drying at 130 degrees Celsius and calcination at 500 degrees Celsius.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1(a) introducing a medium into pores of a plurality of starting porous particles, wherein each starting porous particle has a diameter of less than 1 mm and independently comprises one or more of silica, alumina, zeolite, silica sol, alumina sol, pseudo-boehmite alumina, and/or a clay-based matrix;
Further, water content in the noble metal salt solution A in step (1) is 90% to 100% (by weight) of the water absorption capacity of the added modified alumina. The water absorption capacity refers to the amount of water required for making La—Al2O3 or γ-Al2O3 containing Al or rare earth modified alumina powder just become viscous after water adding.
B · US 2017/0216820 A1 · ¶ 29
1.2(b) contacting the plurality of porous particles with an aqueous salt solution of one or more Group VIII noble metals.
When loading the noble metal on the oxide powder, it can be carried out by impregnating a predetermined amount of the oxide powder with a predetermined amount of the noble metal salt aqueous solution and drying and calcining it.
A · US 2006/0105908 A1 · ¶ 25
A platinum salt solution and a palladium salt solution (containing 0.6666 g of Pt and 3.3334 g of Pd) are respectively weighed and added to 800 g of deionized water, and stirred until uniform. 980 g of La—Al2O3 powder is added to a palladium nitrate solution, which is rapidly stirred until uniform and then stands for 1 hour.
B · US 2017/0216820 A1 · ¶ 41
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document B has a passage for 1.1. Both have a passage for 1.2. Both are classified in CPC B01J, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The present invention relates to a catalyst for purifying exhaust gases of internal combustion engines for automobiles and the like, and a process for producing the same.
A · US 2006/0105908 A1 · ¶ 1
Related claim parts: 1.1
The present invention relates to a method for preparing a noble metal catalyst, in particular to preparation of a catalyst containing a platinum-based noble metal and a lanthanum-based rare earth.
B · US 2017/0216820 A1 · ¶ 1
Related claim parts: 1.2
Accordingly, the temperature of catalysts for purifying exhaust gases has rose remarkably as well in service, compared with that of conventional ones, and consequently it has become difficult to inhibit the granular growth of noble metal even when the solid solution of CeO2—ZrO2 system composite oxides is used.
A · US 2006/0105908 A1 · ¶ 7
The present invention has been done in view of such circumstances, and accordingly its object is to further inhibit the granular growth of noble metal at high temperatures.
A · US 2006/0105908 A1 · ¶ 8
According to this invention, the noble metals are liable to migrate from the inside to the coating surface, which leads to the reduction of noble metal concentration from the surface to the inside, over-accumulation of noble metals on the surface, and high loss rate, and finally causes poor catalyst performance.
B · US 2017/0216820 A1 · ¶ 3
The present invention aims to overcome the problem in the prior art that it cannot be catalyzed without noble metals on sections of automobile exhaust catalyst powders that are newly formed during the ball-milling slurry-making process to reduce the catalyst performance, and provides an automobile exhaust catalyst and a preparation method thereof.
B · US 2017/0216820 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0364577 A1, claim 1, first published 2026-11-23T04:01:59-05:00, https://patent.fyi/US20260364577/, SHA-256 cd706a0e46a8e280f82b5bf8b6911ad2c1366f7eaa26cf7d9cc27622220474f7