Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Supported cobalt hydroxide precursor
What ifWhat if the starting material carries cobalt hydroxide on porous silica?
Claim language“cobalt oxide”
Aqueous cobalt nitrate and sodium hydroxide precipitate cobalt hydroxide onto suspended silica particles. The washed solid dries below its dehydroxylation temperature, and a subsequent hydrogen treatment converts the supported precursor to metallic cobalt.
1.1Self-supporting porous cobalt oxide
What ifWhat if the starting material consists of self-supporting porous cobalt oxide granules?
Claim language“cobalt oxide disposed on a support”
Cobalt carbonate granules release carbon dioxide during calcination in air and leave a porous cobalt oxide skeleton. Hydrogen flows through the granule bed and reduces the oxide to metallic cobalt surfaces within the pore network.
1.2Electrochemical removal of oxygen
What ifWhat if an applied voltage removes oxygen from the supported cobalt oxide?
Claim language“contacting the first catalyst material with a first reducing agent”
A thin cobalt oxide deposit on a porous conductive support forms the cathode of a cell with a heated zirconia electrolyte. The cathode supplies electrons to the oxide, and oxygen ions cross the electrolyte to the counterelectrode, where they leave as oxygen gas.
1.3Paraffin coating for transfer
What ifWhat if molten paraffin covers the reduced cobalt particles before transfer?
Claim language“contacting the reduced catalyst material with carbon monoxide”
The particles enter molten paraffin under nitrogen, and the paraffin solidifies around them on cooling. The solid coating limits oxygen access during handling and melts into the hydrocarbon liquid when the slurry reactor heats up.
1.3Controlled surface oxide formation
What ifWhat if dilute oxygen forms a thin protective oxide layer on the reduced cobalt?
Claim language“contacting the reduced catalyst material with carbon monoxide”
After the catalyst cools under nitrogen, a low concentration of oxygen enters the bed while thermocouples track the oxidation exotherm. The exposure forms a surface oxide layer, and hydrogen removes that layer during reactor startup.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Reference powders for diffraction laboratories
A materials characterization laboratory packs cobalt oxide on alumina into a gas-flow tube. Hydrogen reduces the supported oxide, and an inert purge separates the hydrogen stage from the carbon monoxide stage. Carbon monoxide converts part of the reduced cobalt to cobalt carbide, and the laboratory loads the resulting powder into sealed diffraction holders under inert gas. The laboratory uses the carbide reflections to check phase identification in supported cobalt samples.
Component substitution
Silicon carbide as the catalyst support
Porous silicon carbide granules serve as the support for cobalt oxide. An aqueous cobalt nitrate solution fills the granule pores, and drying and calcination leave cobalt oxide on the pore surfaces. A fixed-bed vessel exposes the granules to hydrogen, purges the bed with nitrogen, and then admits carbon monoxide to form cobalt carbide. The silicon carbide conducts heat away from the cobalt-containing regions during gas treatment.
Parameter or scale variation
Parallel treatment of gram scale beds
Four 8 mm internal diameter tubes each hold 2 g of supported cobalt oxide granules between porous retainers. A common furnace heats the tubes, and individual mass flow controllers distribute hydrogen, nitrogen, and carbon monoxide to the beds. After reduction and nitrogen purging, the controllers supply carbon monoxide to the four beds for 15, 30, 60, and 120 minutes, respectively. Nitrogen displaces carbon monoxide from each tube at the end of its assigned interval.
Combination with existing systems
Preparation skid with slurry reactor charging
A gas distributor fluidizes supported cobalt oxide particles in a preparation vessel during hydrogen reduction and subsequent carbon monoxide treatment, with a nitrogen purge between the two stages. A hot gas filter retains entrained particles, and a sealed transfer line connects the vessel outlet to a nitrogen-blanketed mixing tank. After a final nitrogen purge, the carbide-containing particles fall into the tank and disperse in a liquid hydrocarbon carrier. A solids-handling pump charges the suspension into a slurry bubble column reactor.
Carbon monoxide recovery through gas recirculation
A fixed-bed vessel connects to a recycle loop containing a gas cooler, a condensate separator, and a gas circulator. Hydrogen reduction runs with the loop isolated, and nitrogen then purges the vessel and loop before carbon monoxide enters. During carbide formation, the circulator returns carbon monoxide from the vessel outlet to the inlet, while fresh gas replaces consumed carbon monoxide and gas removed through a controlled bleed. An outlet analyzer measures carbon monoxide and carbon dioxide, and the flow controls adjust makeup and bleed to maintain the selected carbon monoxide concentration.
Automated or data-driven variant
Gas analysis controls treatment stage transitions
A programmable controller operates the hydrogen, nitrogen, and carbon monoxide valves on a packed-bed treatment vessel. An outlet moisture analyzer tracks water produced during cobalt oxide reduction, and the controller opens the nitrogen purge when the water signal stays near its inlet baseline for a preset interval. An outlet hydrogen analyzer confirms that the purge reaches a configured residual hydrogen limit before the controller admits carbon monoxide. Bed thermocouples trigger a switch back to nitrogen when any measured temperature exceeds the configured limit.
Specific version of a part
Cobalt oxide on porous silica
An aqueous cobalt nitrate solution fills the pore volume of silica granules by incipient wetness impregnation. Drying removes water, and calcination in air decomposes the nitrate to cobalt oxide on the pore walls.
Hydrogen reduction in a fixed bed
A tubular vessel holds the supported cobalt oxide pellets while flowing hydrogen contacts the bed at 350 °C and near atmospheric pressure. The gas stream carries away water from the reduction, and an outlet moisture sensor tracks its decline.
Pressurized slurry reduction
A stirred vessel suspends fine cobalt oxide on silica in a high-boiling paraffinic liquid at 280 °C under hydrogen at 20 bar absolute. A submerged sparger disperses hydrogen through the slurry, and a flowing gas outlet carries reaction water to a condenser.
Gas phase carbide passivation
A nitrogen purge displaces residual hydrogen after reduction, and flowing carbon monoxide contacts the catalyst bed at 220 °C near atmospheric pressure. The contact carburizes exposed cobalt and forms a passivated material containing cobalt carbide.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1providing a first catalyst material comprising cobalt oxide disposed on a support;
The novel catalyst of the present invention can be produced by using an aluminosilicate as a support, and supporting microparticles of cobalt oxide on the surface of this aluminosilicate.
A · US 2006/0045834 A1 · ¶ 38
The cobalt oxide catalyst can have a form of powder, wire, chip, disk, rod, strip, bead, monolith with/without porosity, or cobalt oxide particles supported on a substrate comprising metals, ceramics, polymers, glass, fibers, fabrics, textiles, wovens, nonwovens, fibers, alloys, zeolites, molecular sieves, ion exchange resins, graphite, metal oxide, metal carbide, metal boride, metal nitride, and mixtures thereof.
B · US 2007/0004582 A1 · ¶ 21
1.2contacting the first catalyst material with a first reducing agent at a first temperature and a first pressure to form a reduced catalyst material; then
1.3contacting the reduced catalyst material with carbon monoxide, thereby forming a passivated catalyst material comprising cobalt carbide.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.1. Both are classified in CPC B01J, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
When cobalt oxide is supported on this novel aluminosilicate, the result is a catalyst of even higher activity, and the aluminosilicate catalyst supporting cobalt oxide of the present invention can be utilized in a wide range of technological fields dealing with the environment, energy, the chemical industry (manufacturing process), and so forth.
A · US 2006/0045834 A1 · ¶ 3
Related claim parts: 1.1
Given this situation, the use of the same catalytic converters in two-wheeled vehicles as those used in passenger vehicles has been studied, but existing catalytic converters would be disproportionately costly on inexpensive two-wheeled vehicles, and a less expensive exhaust gas purification catalyst needs to be developed.
A · US 2006/0045834 A1 · ¶ 5
From a practical point of view, a high performance catalyst for hydrogen generation having low production cost is highly desirable.
B · US 2007/0004582 A1 · ¶ 5
The invention also relates to a method of making, sintering, activating a cobalt oxide catalyst, regenerating a deactivated cobalt oxide catalyst, and the use of the catalyst for oxidative reaction on various chemical systems.
B · US 2007/0004582 A1 · ¶ 1
Cite aspatent.fyi, US 2026/0364586 A1, claim 1, first published 2026-11-23T04:20:00-05:00, https://patent.fyi/US20260364586/, SHA-256 b55173288f35aeef0bf6e203941f833690f5e23cf1275915b82be512d7e23737