Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Closed mold with fill ports

What ifWhat if the first mold encloses the coating cavity on all sides and receives the mixture through a fill port?
Claim language“being open on at least one side”

Gasketed mold halves clamp around the spray body and define an annular cavity. A low-pressure pump feeds the mixture through a bottom port while displaced air exits through a top vent.

1.2Hollow alumina particle filler

What ifWhat if the dispersion uses hollow crystalline alumina spheres as its filler?
Claim language“a fibrous material or glass micro balloons”

A low-shear paddle mixer folds the spheres into the ceramic particle dispersion. The gas-filled cavities in the spheres reduce heat conduction through the set layer.

1.4Room temperature vacuum drying

What ifWhat if reduced pressure dries the exposed surface of the mixture in the first mold at room temperature?
Claim language“applying heat to the ceramic particle liquid mixture”

A vacuum chamber holds the filled mold with its open face exposed to the chamber. The pump lowers pressure gradually to limit bubbling and removes water vapor until the exposed surface firms.

1.5Demolding after wet gelation

What ifWhat if the first mold comes off while the outer surface is still wet, once the mixture has gelled?
Claim language“after an outer surface portion of a ceramic thermal insulation layer has dried”

A thermogelling cellulose binder forms a network when the filled mold warms under humid conditions. The gel supports the ceramic particles during demolding, and the second mold supports the layer during drying.

1.6Sintered porous mold wall

What ifWhat if a rigid sintered metal wall supports the layer during heating and lets vapor escape through interconnected pores?
Claim language“a mesh portion”

Two curved shells made from sintered stainless steel powder fit around the insulation layer. The rigid shells retain the profile while interconnected pores carry water vapor to the surrounding air.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Insulated spray tips for glass forming

A fixed spray tip applies water-based lubricant to hot glass-forming dies. An open-sided solid mold fits around the tip body, and plugs seal the fluid inlet and discharge orifice during molding. The mold cavity receives a ceramic particle dispersion filled with glass microspheres and holds it during heating until the exposed surface dries. A split mesh shell replaces the solid mold for final heated drying, and the shell and plugs come off after the layer sets.

Component substitution

Expanded perlite filler for ceramic insulation

Expanded perlite granules replace the fibrous filler or glass microspheres in the ceramic particle dispersion. A low-speed paddle folds the granules into the dispersion, and the mixture fills the gap between the spray body and an open-sided solid mold. Heat dries the exposed surface before the solid mold comes off. A split mesh shell supports the layer during final heated drying and comes off after the layer sets.

Perforated sheet support during final drying

A perforated stainless steel clamshell replaces the mesh wall of the second mold. The clamshell halves are formed to the insulation contour and use external hinges and latches to close around the layer after the first mold comes off. During final heating, punched holes vent moisture and the sheet between the holes supports the layer. The clamshell opens after the layer sets.

Parameter or scale variation

Two insulation thicknesses on one body

A split solid mold provides 3 mm of radial clearance around the rear shank and 8 mm around the discharge-end shoulder, with a 10 mm tapered transition between the two sections. A removable plug seals the discharge orifice while the filled ceramic dispersion enters through the open side of the mold. Heat dries the exposed surface before the mold halves separate. A matching two-piece mesh shell supports both thicknesses and the tapered transition during final heating and comes off after the layer sets.

Combination with existing systems

Insulated nozzles on a recirculating manifold

Individually insulated nozzles mount on a heated recirculating coating manifold through threaded swivel unions. During fabrication, a split solid mold surrounds each nozzle barrel, and its end collars keep the union seat and discharge face clear while the filled ceramic dispersion undergoes initial drying. A matching split mesh mold supports the layer during final heating and comes off after the layer sets. The manifold supplies each nozzle through a branch port and returns excess coating through a separate return line.

Automated or data-driven variant

Gravimetric control of both drying stages

A heated chamber suspends the spray body and mold from a load cell outside the hot zone, and a controller records mass and chamber temperature. During solid-mold heating, the controller compares mass loss with a threshold established by checking when the exposed surface dries on reference parts of the same geometry. At that threshold, a fixture opens the solid mold and closes a split mesh shell around the layer. During final heating, the controller ends the cycle when the mass-loss rate stays below a recipe limit for a specified interval, and the fixture removes the mesh shell after cooling.

Specific version of a part

Open aluminum trough mold

A machined aluminum trough follows the contour of the lower half of a cylindrical spray body. Its solid curved wall sets the outer profile of the insulation, and its open top provides access for filling.

Metered syringe filling

A piston syringe with a wide-bore tip dispenses the mixture into one end of the open mold as the tip travels along the cavity. A straightedge levels the fill against the mold rim.

Curved woven wire shell

Two semicylindrical frames carry woven stainless steel wire cloth with openings approximately 0.5 mm wide. The frames clamp around the insulation layer and hold the cloth to the desired outer profile.

Radial split mold release

Toggle latches release the two halves of the second mold after the insulation sets. Opposed guide pins direct each half radially outward to limit scraping of the coating.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2005/0239630 A1
Published
Oct 27, 2005
Filed
Jun 30, 2003
Document BUS 2012/0164441 A1
Published
Jun 28, 2012
Filed
Sep 1, 2010
Class
B32B 18/00
Claim 1
Document A
Document B
1.1providing a first mold in the shape of at least a portion of the spray component, the first mold having at least one solid wall and being open on at least one side;
The premixed material 1 was mixed through the line mixer 9 to obtain a room-temperature-hardenable premixed material 11, which was cast through a nozzle 10 into a cavity between a permanent lining 12 and a mold 13.
A · US 2005/0239630 A1 · ¶ 58
1.2mixing at least one filler into a ceramic particle liquid dispersion to produce a ceramic particle liquid mixture, the filler comprising a fibrous material or glass micro balloons;
An alternative method for forming the ceramic-coated powder is a method in which the ceramic layers are formed by adding the carbon particles into a slurry of ceramic particles to allow the ceramic particles to adhere to the surfaces of the carbon particles.
B · US 2012/0164441 A1 · ¶ 20
1.3adding the ceramic particle liquid mixture into the first mold;
1.4applying heat to the ceramic particle liquid mixture in the first mold;
The premixed materials are hardened usually by heating via the molds.
A · US 2005/0239630 A1 · ¶ 4
1.5removing the first mold after an outer surface portion of a ceramic thermal insulation layer has dried;
Because the premixed materials are not hardened at room temperature, it is necessary to harden the materials by some means to remove molds after casting. The premixed materials are hardened usually by heating via the molds.
A · US 2005/0239630 A1 · ¶ 4
1.6placing a second mold over the ceramic thermal insulation layer, the second mold having at least one wall comprising a mesh portion;
1.7applying heat to the ceramic thermal insulation layer and the second mold until the ceramic thermal insulation layer sets; and
1.8removing the second mold from the spray component.
As a result, there is no necessity for heat hardening for removing a mold from a refractory body, which is carried out in using conventional premixed materials, and thus the periodic maintenance of a mold thermally deformed by the heat hardening may be omitted, resulting in drastic reduction of energy and casting cost.
A · US 2005/0239630 A1 · ¶ 62

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1 1.4 1.5 1.8. Only Document B has a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Because the premixed materials are not hardened at room temperature, it is necessary to harden the materials by some means to remove molds after casting.
A · US 2005/0239630 A1 · ¶ 4
Accordingly, an object of the present invention is to provide a castable refractory powder composition containing alumina cement capable of providing a premixed material by tempering with water, which can keep flowability for a long period of time.
A · US 2005/0239630 A1 · ¶ 8
However, carbon materials generally have a problem in that they are poor in oxidation resistance and strength.
B · US 2012/0164441 A1 · ¶ 3
In addition, it is technically difficult to provide uniform coating on graphite base materials having three-dimensionally complex shapes.
B · US 2012/0164441 A1 · ¶ 4
Cite aspatent.fyi, US 2026/0364613 A1, claim 1, first published 2026-11-23T04:38:59-05:00, https://patent.fyi/US20260364613/, SHA-256 c88b5d4b0e7bac060d181f1f7e21e6da145979fa828ac88704cd69a98bc597cb
First published
Permanent addresshttps://patent.fyi/US20260364613/
Content fingerprint (SHA-256)c88b5d4b0e7bac060d181f1f7e21e6da145979fa828ac88704cd69a98bc597cb
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi