Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Single population polyethylene coating
What ifWhat if the coating uses a unimodal high-pressure low-density polyethylene homopolymer?
A high-pressure reactor polymerizes ethylene by free-radical initiation to produce a resin with a single molecular-weight mode and long-chain branching. The branches increase melt strength as the extruder draws the molten curtain onto the moving web.
1.1Higher density barrier coating
What ifWhat if the multimodal polyethylene coating resin has a bulk density of 925 kg/m³?
Claim language“a density of from 910 to 915 kg/m3”
A larger mass share of the denser polyethylene fraction raises the overall resin density and increases the crystalline content of the cooled coating. A flat die deposits the melt on the substrate, and a chill roll solidifies the coating under nip pressure.
1.2Lower melt flow ratio
What ifWhat if the polyethylene copolymer has an MFR21/MFR2 ratio of 15?
Claim language“a range of from more than 20 to 100”
The resin uses overlapping molecular-weight populations to limit the increase in melt flow as the test load rises. A short die-to-nip air gap and a moderate draw ratio limit the time and strain imposed on the unsupported melt curtain.
1.2Capillary viscosity process check
What ifWhat if a capillary rheometer measures melt viscosity across several shear rates for coating process control?
Claim language“MFR2 and MFR21 being determined”
A piston drives the melt through a capillary at fixed temperature and several controlled speeds while a transducer measures pressure upstream of the die. The resulting viscosity curve shows how the resin flows across the shear-rate range used in the coating die.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Polyethylene coating for temporary floor protection
A roll-fed kraft paper web carries a multimodal polyethylene coating on its exposed face. A flat die delivers the molten coating into the nip between a rubber-covered pressure roll and a chilled steel roll, with the polyethylene facing the steel. The coated face sheds incidental water during interior construction, and the paper backing supports the film during handling and removal.
Component substitution
Ethylene octene in the lower density fraction
An ethylene and 1-octene copolymer serves as the lower-density fraction and contains 15 to 25 wt. % incorporated 1-octene. A twin-screw extruder melt blends this fraction with the higher-density multimodal polyethylene fraction. Measurements on the compounded pellets guide the feed ratio to reach a density of 910 to 915 kg/m³, an MFR2 of 0.5 to 20 g/10 min, and an MFR21/MFR2 ratio above 20 and at most 100. A flat die extrudes the pellet blend onto a moving substrate at a chilled nip.
Polypropylene film as the coating substrate
A biaxially oriented polypropylene web replaces the machine-direction-oriented polyethylene substrate, and the multimodal polyethylene blend forms the outer coating. An inline corona treater activates the polypropylene surface, and a two-manifold flat die delivers a maleic-anhydride-grafted polypropylene tie layer against that surface with the polyethylene blend facing outward. A chilled nip presses the layers together and removes heat before winding.
Parameter or scale variation
Narrow web coating at two line speeds
A flat die deposits a 15 g/m² layer of the multimodal polyethylene blend on a paper web with a net coated width of 300 mm. The line runs at either 50 or 100 m/min, corresponding to net coating outputs of 13.5 and 27 kg/h. A melt pump meters the net output plus the measured edge-trim allowance, and a chilled roll sets the coating before winding.
Combination with existing systems
Extrusion lamination with an aluminum barrier
A two-web extrusion laminator feeds paper and aluminum foil from separate unwind stations. A flat die deposits the multimodal polyethylene blend on the paper at the first nip, and a second extrusion station applies an ethylene acrylic acid tie layer between the polyethylene surface and the foil. A chilled pressure nip consolidates the paper, polyethylene blend, tie layer, and foil into a single web.
Automated or data-driven variant
Feedback control of coating mass
An upstream transmission gauge measures the base web mass per unit area, and a downstream gauge measures the coated web after the chill roll. A web encoder synchronizes the two readings so the controller subtracts measurements from the same section of web. The controller averages the calculated coating mass across successive scans and trims melt-pump speed to hold the target, with measured line speed providing the initial pump command.
Specific version of a part
Bimodal first copolymer fraction
Fraction A contains two ethylene and 1-butene copolymer populations with different molecular weights. The combined fraction has a density of 943 kg/m³, an MFR2 of 30 g/10 min, and a 1-butene content of 1.5 wt. % based on the mass of fraction A.
Hexene rich second fraction
Fraction B is an ethylene and 1-hexene copolymer with 20 wt. % 1-hexene based on the mass of fraction B. The fraction has a density of 893 kg/m³ and an MFR2 of 0.3 g/10 min.
Melt flow ratio of forty
A melt flow indexer measures resin flow at 190 °C under loads of 2.16 kg and 21.6 kg. The measured rates are 2 g/10 min and 80 g/10 min, respectively, giving an MFR21/MFR2 ratio of 40.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a multimodal polyethylene copolymer (P) having a MFR2 of from 0.5 to 20 g/10 min, a density of from 910 to 915 kg/m3 and comprising: a first bi- or multimodal polyethylene copolymer fraction (A) having a density of from 920 to 950 kg/m3, a MFR2 of from 2 to 200 g/10 min and a comonomer content of from 0.5 to 5 wt. %, based on the total weight of the first bi- or multimodal copolymer fraction (A), and a second polyethylene homo- or copolymer fraction (B) having a density of from 880 to 915 kg/m3, a MFR2 of from 0.01 to 6 g/10 min and a comonomer content of from 15 to 25 wt. %, based on the total weight of the second ethylene homo- or copolymer fraction (B);
The multimodal ethylene copolymer is a copolymer of ethylene with one or more alpha-olefin comonomers having from 4 to 10 carbon atoms and has a weight average molecular weight of from 70000 g/mol to 250000 g/mol, the ratio of the weight average molecular weight to the number average molecular weight, Mw/Mn, of from 15 to 50, a melt index MFR2 of from 0.05 g/10 min to 5 g/10 min, a melt index MFR5 of from 0.5 to 10 g/10 min and a density of from 930 kg/m to 955 kg/m3.
A · US 2011/0120587 A1 · abstract
The total comonomer content of the multimodal copolymer of the present invention ranges from 6% to 25% by weight, preferably from 6% to 12% by weight more preferably from 7% to 11% by weight; even more preferably from 7% to 9% by weight.
B · US 2011/0294975 A1 · ¶ 19
1.2wherein a ratio MFR21/MFR2 of said multimodal ethylene copolymer (P) is in a range of from more than 20 to 100, MFR2 and MFR21 being determined according to ISO1133.
The MFR is determined at 190° C. for PE. The load under which the melt flow rate is determined is usually indicated as a subscript, for instance MFR2 is measured under 2.16 kg load, MFR5 is measured under 5 kg load or MFR21 is measured under 21.6 kg load.
A · US 2011/0120587 A1 · ¶ 106
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.2. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, even though the document teaches that the composition has a good processability it still remains a wish to further improve the processability, like maximum throughput and neck-in behaviour.
A · US 2011/0120587 A1 · ¶ 2
The present invention provides polyethylene coated metal pipes that have an improved resistance against stress cracking and/or can be used at high service temperature.
A · US 2011/0120587 A1 · ¶ 3
A disadvantage of this process is that relatively large amounts of hydrogen have to be added to produce the low molecular weight component.
B · US 2011/0294975 A1 · ¶ 4
In addition, it is technically complex to prevent comonomers added in one reactor or hydrogen added as regulator from getting into the next reactor.
B · US 2011/0294975 A1 · ¶ 4
Cite aspatent.fyi, US 2026/0364632 A1, claim 1, first published 2026-11-23T04:57:30-05:00, https://patent.fyi/US20260364632/, SHA-256 e36aa4954e2ada7fcc832e376139e6f936bc92b530ca1e7a4db0dc421900077b