patent.fyi
Applications  /  US 2026/0364660
United States Patent Application Publication

US 2026/0364660 A1

Published
Nov 19, 2026
Filed
Aug 8, 2024
Earliest date on the face
Sep 5, 2023
Classification
B21C 23/002
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Low silicon magnesium alloy

What ifWhat if the extrusion uses 0.20 mass % silicon and 2.50 mass % magnesium?
Claim language“1.80 to 3.00 mass % of Si”

A heated aluminum billet containing 2.50 mass % magnesium, 0.30 mass % manganese, 0.15 mass % iron, and 0.20 mass % silicon passes through a profile die. Magnesium strengthens the aluminum matrix in solid solution, and a rotating friction stir tool joins the supported extrusion to an aluminum mating member.

1.1Chromium dispersoid control

What ifWhat if the alloy uses 0.03 mass % manganese and 0.20 mass % chromium to control grain boundary motion?
Claim language“0.10 to 1.60 mass % of Mn”

A billet containing 2.20 mass % silicon, 0.03 mass % manganese, 0.20 mass % chromium, and 0.15 mass % iron undergoes homogenization before hot extrusion. Chromium-bearing dispersoids impede grain boundary motion during hot working, and a friction stir tool joins the extruded flange to an aluminum mating member.

1.2Coarse grained brazing flange

What ifWhat if the outermost layer of the joined flange has an average grain size of 300 μm?
Claim language“200 μm or less in an outermost layer”

Controlled deformation and annealing set the flange surface grain size before joining. An aluminum-silicon filler melts in the lap gap while the members remain solid, and the filler solidifies to transfer load across the overlap.

1.2Fine grained thin wall

What ifWhat if the thinnest wall has an average grain size of 150 μm at a depth of 100 μm?
Claim language“400 μm or more in a section”

A cold sizing pass stores deformation in the thin wall, and a controlled recrystallization anneal sets the local grain size. The profile places the thermal joint on a thicker flange, which transfers load into the thin wall through a radiused transition.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Brazed cold plate for optical instruments

An aluminum alloy extrusion forms the base of a liquid cold plate, and a pure aluminum cover seals its longitudinal coolant grooves. The outermost layer of the extrusion at the joint has an average grain size of 200 μm or less, and the section 100 μm below the surface at the thinnest groove floor has an average grain size of 400 μm or more. Aluminum-silicon filler preforms sit on the perimeter and rib lands, and a furnace cycle melts the filler to join the cover and seal the flow passages.

Component substitution

Copper cover for a transition joint

A nickel-plated copper cover replaces the aluminum mating member and overlaps a flange on the aluminum alloy extrusion. A zinc-aluminum filler foil sits between the flange and the plated cover, and local induction heating melts the foil while both members remain solid. The nickel coating limits direct interaction between the copper and aluminum during heating, and a fixture holds the overlap in position until the filler solidifies.

Parameter or scale variation

Thicker web with deeper grain measurement

An aluminum alloy extrusion has a minimum web thickness of 2.0 mm and a 4 mm wide flange that overlaps an aluminum cover. Local rolling of the flange face before thermal joining promotes surface recrystallization, with an average grain size of 150 μm or less at the joined surface. The grain size evaluation uses a section 250 μm below the surface at the thinnest web, where the average grain size is 350 μm or more.

Combination with existing systems

Extruded manifold in a refrigeration loop

An extruded aluminum alloy header receives flat aluminum tubes through slots in one wall, and filler preforms surround the tube ends at the slots. A furnace cycle brazes the tubes to the header, with the fine-grained outermost layer located on the header side of each joint and the coarse-grained region located in the thinnest header wall. The header connects to the discharge line of a vapor-compression refrigeration loop and distributes refrigerant among the parallel condenser tubes.

Automated or data-driven variant

Closed-loop heating of brazed lap joints

A fixture holds an aluminum alloy extrusion and an aluminum cover in overlap with a filler preform between their joining faces. Two thermocouples on the extrusion monitor the temperature next to the overlap and in the thinnest wall while a controller adjusts induction power using a thermal cycle established from sectioned trial joints. The controller starts the hold when the joint reaches the filler melting range and reduces power when the thin wall reaches its qualified temperature limit.

Machine vision for grain size verification

A sample assembly from each joining batch is sectioned through the joint and through the thinnest extrusion wall, then polished and etched to reveal the grain boundaries. A calibrated optical microscope captures tiled images, and image analysis measures mean grain intercept length in the outermost joined layer and along a trace 100 μm below the thin-wall surface. The software records both measurements with the batch identifier and flags results above 200 μm at the joint or below 400 μm in the thin wall.

Specific version of a part

Midrange silicon extrusion billet

A cast billet contains 2.40 mass % silicon, 0.60 mass % manganese, and 0.20 mass % iron, with the balance aluminum and incidental impurities. The billet undergoes homogenization and hot extrusion through a die that forms a thin web and a thicker joining flange.

Recrystallized joining surface

A local cold rolling pass deforms the joining flange surface, and a controlled anneal recrystallizes the deformed layer before brazing. The outermost layer of the extruded member at the completed joint has an average grain size of 150 μm.

Coarse grained thin web

Extrusion temperature and a subsequent grain-growth anneal set the microstructure in a 1.2 mm web that forms the minimum wall thickness of the profile. Polished sections taken after joining show an average grain size of 450 μm at a depth of 100 μm from the web surface.

Cite aspatent.fyi, US 2026/0364660 A1, claim 1, first published 2026-11-23T05:16:15-05:00, https://patent.fyi/US20260364660/, SHA-256 64e3ef26bb82a20f57fad95d4b6c531fdf39be993130f68e292c3d23fca2951b
First published
Permanent addresshttps://patent.fyi/US20260364660/
Content fingerprint (SHA-256)64e3ef26bb82a20f57fad95d4b6c531fdf39be993130f68e292c3d23fca2951b
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi