1.2Resistance spot welded lap joint
Copper alloy electrodes clamp a 12 mm overlap and pass current through the sheets to form fused nuggets at the interface. The row of nuggets transfers shear between the sheets across the overlap during forming.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Copper alloy electrodes clamp a 12 mm overlap and pass current through the sheets to form fused nuggets at the interface. The row of nuggets transfers shear between the sheets across the overlap during forming.
A flat backing fixture aligns the side B surfaces of the 1.0 mm and 1.5 mm sheets. A laser produces a full-penetration butt seam, and a recessed die face accommodates the 0.5 mm step on side A during forming.
An electroplated zinc layer provides sacrificial corrosion protection on side A. Laser ablation clears a narrow strip along the joining edge before butt welding, and the joined blank is cold stamped.
The sheet retains its side B zinc coating during edge preparation. A laser butt-welding fixture leaves clearance beneath the seam for zinc vapor to vent while a root wider than the locally depleted zone reaches the remaining coating.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A welded blank feeds a transfer press with a draw station, a flange station, and a restrike station. The loading nest supports both thicknesses on stepped pads and registers the butt seam parallel to the long axis of the part. The draw station forms a channel, the flange station bends its edges, and the restrike station sets the final channel width. Each station provides relief where the weld crosses a tool surface and uses support pads that match the two sheet heights.
Opposed laser line profilers measure both faces of the clamped sheets at several positions along the butt joint. The controller fits a line to the sheet surfaces on each side of each scan and computes the two face steps at the joint. Servo lift pads adjust the height and tilt of the thinner sheet until the larger step is at least 1.1 times the smaller step along the seam. The clamps hold the corrected position while a welding head follows the measured joint.
A focused laser beam traverses the abutting sheet ends and melts both edges through their thicknesses. The common molten pool solidifies into a continuous weld that joins the two ends.
The aluminum-silicon plated layer on side A extends to the prepared edge of the first sheet. The side A weld toe meets the remaining plated layer along the seam.
patent.fyi, US 2026/0364665 A1, claim 1, first published 2026-11-23T05:16:15-05:00, https://patent.fyi/US20260364665/, SHA-256 1bd4f513ce324a23aa0efa00a7c240ae78ec6e30abef5a9f85b6b6cec50a0be2