Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Hot backward extrusion
What ifWhat if hot backward extrusion through an open annular passage produces the preform?
Claim language“closed-die hot forging”
A punch enters the heated billet inside a cylindrical container, and displaced metal flows backward through the open gap around the punch to form a cup. A contoured punch land varies the annular gap over the extrusion stroke to produce an axially profiled rim for the next forming operation.
1.1Uniform thickness preform rim
What ifWhat if the preform rim has constant wall thickness along its axial height?
Claim language“varies in an axial direction”
Concentric cylindrical die surfaces set the same radial gap from the base fillet to the rim lip. During hot closing, an internal support backs the lower wall while an external die bends and compresses the free lip inward to form the undercut.
1.2Cold spinning the rim
What ifWhat if cold spinning brings the rim inward at room temperature?
Claim language“hot forming the rim”
An annealed low-carbon steel preform rotates against a segmented mandrel, and a spinning roller closes the lip in successive passes. The final pass sets the mouth diameter and lip thickness, and the mandrel segments retract through the smaller opening.
1.2Outward expansion behind mouth
What ifWhat if the wall below the mouth expands radially outward to create the undercut?
Claim language“the rim radially inward”
An external collar holds the mouth at its original diameter while an axial wedge drives segmented shoes outward against the heated wall below it. The shoes expand the wall into a surrounding die recess, then retract through the mouth.
1.2Cylindrical radial forming jaws
What ifWhat if hydraulically actuated jaws close the rim with cylindrical contact faces?
Claim language“at least one tapered section”
Radial cylinders drive a ring of jaws inward against the heated upper rim while a support ring holds the lower wall. The jaws form a cylindrical band at the mouth, and a retractable internal sizing ring sets the opening diameter and final lip thickness.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Undercut for a pump seal carrier
A closed die hot forges a billet into an annular pump seal carrier preform with a rim that thickens toward its free edge. A lower nest locates the preform by its base and supports the base while an external die with a tapered bore drives the rim radially inward. The rim bends and changes thickness as it forms an internal shoulder that captures the flange of a seal cartridge inserted from the opposite face.
Component substitution
Segmented jaws for radial rim forming
A ring of twelve guided jaws replaces a continuous forming sleeve. Each jaw carries a tapered inner face, and an axially moving cam ring drives the jaws radially inward around a hot preform seated in a lower nest. The jaws engage the axially profiled rim, bending it inward and changing its wall thickness to form the undercut. When the cam ring retracts, return springs pull the jaws outward to release the part.
Collapsible mandrel for internal cavity sizing
A collapsible mandrel replaces the plain locating boss in the lower nest and enters the hot preform through its rim opening. A tapered drawbar expands the mandrel sectors so their outer faces define the cavity immediately below the intended undercut. An external die with a tapered bore bends the rim inward and compresses it against the upper faces of the sectors to set the shoulder thickness. After the external die retracts, the drawbar releases the sectors so they collapse and pass through the finished opening.
Parameter or scale variation
Two passes reduce the rim opening
A closed die hot forges a preform with an 80 mm rim opening and a wall that thickens from 5 mm at the root to 8 mm at the lip. A first tapered die bends the hot rim inward to a nominal opening of 74 mm. A second tapered die reduces the opening to 68 mm, with the base supported in a matching nest during each pass. The two passes change the rim wall thickness and leave an internal cavity wider than the finished opening.
Combination with existing systems
Induction reheating between separate forming presses
A transfer line connects a closed-die forging press to a separate rim-forming press through an induction reheating station. A gripper holds the forged preform by its base and centers its tapered-thickness rim inside an annular induction coil. A pyrometer measures the rim temperature, and the heater shuts off at the forming setpoint for the billet alloy. The gripper then places the reheated preform in a locating nest where a tapered die bends the rim inward and changes its wall thickness.
Automated or data-driven variant
Press stroke control from measured rim geometry
An optical profile station measures the inner and outer rim surfaces of each hot preform at several axial levels before the forming stroke. A controller calculates the opening diameter and wall thickness at those levels and interpolates a target die stroke from calibration runs that relate those measurements to the finished opening. A servo-hydraulic press uses ram position feedback to execute the target stroke while a load sensor enforces a preset force limit. The tapered die bends the rim inward and changes its wall thickness to form the internal undercut.
Specific version of a part
Stepped rim cavity
A stepped punch and cylindrical outer die form a cup in a closed-die forging stroke. The annular gap is 8 mm near the rim root and 6 mm near the lip, with a radiused transition between them.
Thickened lip for hot forming
A closed-die punch has a smaller diameter near the mouth, which creates a wider gap for metal flow at the lip. The resulting preform has an 8 mm lip and a 5 mm lower rim wall, with a gradual transition along the axis.
Conical entry and sizing land
An annular closing die advances axially over the heated rim, and a conical entry inclined 25 degrees to the axis bends the lip inward. A cylindrical land sets the outside diameter while a collapsible internal ring sets the inside diameter and squeezes the lip to its final thickness.
Two stage tapered closure
A first annular die with a tapered inner face bends the upper rim partway inward while the lower wall rests in a support ring. A second die with a steeper taper closes the opening further and compresses the lip against a segmented internal tool to set its final thickness.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1closed-die hot forging of a billet to produce a preform having a rim with a wall thickness that varies in an axial direction; and
A hot forging die for closed die hot forging of a material to be forged, wherein the material to be forged is made of a nickel alloy or a titanium alloy, the hot forging die being for producing, as hot closed die forged products, turbine disks for aircraft jet engines and gas turbine disks for generation, by closed die hot forging of the material to be forged, the hot forging die comprising a plurality of ring-shaped die pieces which are combined concentrically and fastened w
A · US 9,597,725 B2 · claim 1
(1) in the present invention, the proposed forming method of amorphous alloy parts combines the micro-jetting and bonding 3D printing technology and the hot closed-die forging technology, in which amorphous alloy powder is printed into a pre-forging blank by the micro-jetting and bonding 3D printing technology, and then the pre-forging blank is placed in a closed forging die to perform hot closed-die forging so as to obtain an amorphous alloy part.
B · US 10,946,448 B2 · ¶ 28
1.2forming a forged part from the preform by hot forming the rim radially inward using a tool having an inner surface with at least one tapered section to create the undercut inside of the forged part by bending the rim inward and changing the wall thickness of the rim during the hot forming of the rim.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The present invention relates to a hot forging die.
A · US 9,597,725 B2 · ¶ 1
Related claim parts: 1.1
Therefore, the forging material after completion of hot forging is forged only at the part being in contact with the die pieces, and the material to be forged invades into the gaps between the moved die pieces, which makes it difficult to make the part into the desired shape.
A · US 9,597,725 B2 · ¶ 7
The object of the present invention is to provide an inexpensive hot forging die which allows a desired shape to be obtained even from a large-sized forging material.
A · US 9,597,725 B2 · ¶ 8
Thus, it is necessary to develop a new precision forming method of large-size and complex-shaped amorphous alloy parts.
B · US 10,946,448 B2 · ¶ 4
Thus, a cold additive and hot forging combined forming method of large-size and complex-shaped amorphous alloy parts is correspondingly obtained, thereby solving the technical problems such as size limitation, shape limitation and poor density in the forming methods of bulk amorphous alloys in the prior art.
B · US 10,946,448 B2 · ¶ 5
Cite aspatent.fyi, US 2026/0364667 A1, claim 1, first published 2026-11-23T05:37:27-05:00, https://patent.fyi/US20260364667/, SHA-256 76d504f254cf931087630d36e8590450b2b664276e09aef828feee98cece5b04