patent.fyi
Applications  /  US 2026/0364672
United States Patent Application Publication

US 2026/0364672 A1

Published
Nov 19, 2026
Filed
Nov 23, 2023
Earliest date on the face
Nov 25, 2022
Classification
B22D 19/16
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Ceramic molds printed directly

What ifWhat if the molds were printed directly from ceramic slurry and fired?
Claim language“formed by a lost wax method”

A light source cures successive layers of a slurry containing alumina powder and a light-sensitive binder. Drain ports let uncured slurry flow out of the cavities before binder burnout and firing consolidate the ceramic walls.

1.2Solid charges inside each mold

What ifWhat if each mold received a solid alloy charge and the stack had no common melt receiver?
Claim language“a bucket capable of receiving liquid metal”

Each solid charge rests on a ceramic ledge above its mold cavity. The hot zone melts the charges in place, and gravity fills each cavity while the base remains liquid until directional cooling begins.

1.3Separate radial feed channels

What ifWhat if separate radial channels connected the bucket to the mold vertices without a circumferential passage?
Claim language“a ring connecting the bucket”

A central bucket feeds individual ceramic channels that slope outward toward the mold inlets. The channel cross sections and slopes set the flow resistance along each path.

1.3Side entry below mold vertices

What ifWhat if the ring fed each mold through a side inlet below its vertex?
Claim language“to each vertex of each mold”

Short ceramic gates connect the ring to the mold sidewalls. Melt enters below the vertices and rises through the cavities as gas exits through vents at the high points.

1.4Gravity feed through radial gates

What ifWhat if a shallow distribution tray fed the mold gates without a separate descending conduit from the bucket?
Claim language“a downcomer connected to the bucket”

The bucket opens directly onto a shallow ceramic tray positioned just above the gate entrances. The melt level in the tray provides the pressure head, and slightly sloped radial gates carry metal into the molds.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Directional casting of glass forming plungers

The stack holds lost wax molds for nickel alloy plungers that press hot glass, with each working tip above its stem. A common ring connects the upper bucket to the mold tips, the central downcomer connects to the bucket, and a grain selector extends from each stem end to a chill plate. A solid alloy charge melts in the bucket and fills the molds through the ring. Cooling starts at the chill plate, and the solidification front advances from each stem toward the working tip.

Component substitution

Straight capillary grain selectors

A straight alumina capillary replaces each helical grain selector at the bottom of a mold. The upper end opens into the mold cavity, and the lower end joins a starter chamber on the chill plate. Alloy melted in the bucket fills the mold from the ring and continues into the capillary and starter chamber. Grains grow upward from the starter chamber, and the narrow bore limits how many enter the mold.

Leachable cores for hollow castings

A leachable fused silica core replaces the solid pattern interior in each lost wax mold for a hollow part with a through passage. Ceramic core prints at both ends seat in the shell, and the upper ring gate enters the cavity beside the upper print. Alloy melted in the bucket flows around the core and solidifies upward from the grain selector at the mold bottom. After shell removal, a heated alkaline solution dissolves the core through the exposed passage openings.

Parameter or scale variation

Sixteen molds on one ring

Sixteen molds for parts with 12 mm maximum width sit at 22.5 degree intervals on a 240 mm pitch circle. Equal-length inlet gates connect their vertices to the annular runner, and four radial passages connect the runner to the central bucket at 90 degree intervals. The downcomer extends from the center of the bucket, and the sixteen grain selector bases sit at the same height on a common chill plate. A solid charge sized for the combined cavity and channel volumes melts in the bucket and fills the ring before the stack is withdrawn into the cooling zone.

Combination with existing systems

Casting stack with liquid metal cooling

A vacuum withdrawal furnace holds the charged stack above a liquid tin bath, with a radiation baffle between the heating zone and the bath. The solid charge melts in the bucket and flows through the ring into the preheated molds. A ram lowers the sealed ceramic ends beneath the grain selectors through the baffle and into the bath. Continued withdrawal moves the cooled region upward through the molds as the solidification fronts advance toward the ring.

Automated or data-driven variant

Sensor controlled withdrawal of the stack

Two thermocouples at known vertical spacing sit in ceramic sleeves against the outside of a representative mold, between the grain selector and the upper feed gate. After the solid charge melts and fills the molds, a controller starts the motorized withdrawal stage and records both temperatures and stage position. The controller divides the temperature difference by sensor spacing and adjusts withdrawal speed within preset limits to keep the measured gradient in the operating band for the alloy. The stage completes withdrawal when the upper sensor cools below the alloy solidus by a calibrated margin.

Specific version of a part

Zircon faced ceramic shell molds

Each wax pattern receives a fine zircon slurry coat followed by coarser ceramic backup coats. Steam removes the wax, and firing strengthens the shell before casting.

Preheated alumina receiving bucket

A dense alumina bucket tapers toward a bottom outlet that feeds the distribution passages. Preheating the bucket reduces heat loss from the first metal entering it.

Tapered ceramic downcomer

A fired ceramic downcomer joins the bucket outlet to the lower runner. Its bore narrows toward the runner to match the accelerating gravity flow and keep the passage filled during steady pouring.

Helical selectors above starter chambers

A starter chamber beneath each mold sits on a chilled plate and develops columnar grains as solidification begins. A narrow helical passage limits the number of grains that continue growing into the mold cavity.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2016/0158836 A1
Published
Jun 9, 2016
Filed
Jun 6, 2015
Class
B22D 27/003
Document BUS 10,576,537 B2
Published
Mar 3, 2020
Filed
Feb 5, 2019
Class
B22D 19/16
Claim 1
Document A
Document B
1.1a plurality of molds formed by a lost wax method, each mold of the plurality of molds having a vertex, an intermediate portion and a bottom,
The ceramic mold, known as the investment mold, is produced by three repeating steps: coating, stuccoing, and hardening.
A · US 2016/0158836 A1 · ¶ 4
The solid wax with embedded core assembly (and optionally with other wax gating components or additional patterns attached) is then dipped in ceramic slurry to form the outer shell mold. Once the shell is dried, the wax is melted and drained out leaving behind a hollow cavity between the outer shell and the inner core.
B · US 10,576,537 B2 · ¶ 74
1.2a bucket capable of receiving liquid metal,
Step #8: Place the investment mold pouring cup upwards, and fill the investment mold with molten metal.
A · US 2016/0158836 A1 · ¶ 4
If the mold assembly were to be grown naturally with no seed, then a molten metal charge is melted in the melt cup or crucible and poured through the pour cup to fill the mold.
B · US 10,576,537 B2 · ¶ 78
1.3a ring connecting the bucket to each vertex of each mold of the plurality of molds,
1.4a downcomer connected to the bucket,
A casting mold has a pour cone, a downsprue, and a part-forming cavity having a lower end and an upper end. The downsprue extends from the pour cone toward the part-forming cavity and has: a lower portion having a plurality of ports in communication with the part-forming cavity; and an upper portion telescoping relative to the lower portion and coupling the lower portion to the pour cone.
B · US 10,576,537 B2 · abstract
1.5a plurality of grain selectors each connected to a bottom of a mold of the plurality of molds,
If the alloy is to be cast with the naturally favored <100> orientation along the long axis (the spanwise direction) of the blade the shell may include means such as a hollow helical passage joined to a hollow cavity at the bottom, to form a starter block (grain starter). Wax forming the helix and block may be molded as part of the pattern or secured thereto prior to shelling.
B · US 10,576,537 B2 · ¶ 76

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document B has a passage for 1.4 1.5. Both have a passage for 1.1 1.2. Both are classified in CPC B22D, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

It is used to produce common everyday metal objects as well as intricate aerospace and military components.
A · US 2016/0158836 A1 · ¶ 3

Related claim parts: 1.4 1.5

One aspect of the disclosure involves casting an alloy part in a mold having a part-forming cavity.
B · US 10,576,537 B2 · ¶ 7

Related claim parts: 1.1 1.2

Investment casting can produce complicated shapes that would be difficult or impossible with other methods and requires little surface finishing and only minor post-machining.
A · US 2016/0158836 A1 · ¶ 3
The disclosure relates to casting of aerospace components.
B · US 10,576,537 B2 · ¶ 2
A further embodiment may additionally and/or alternatively include the pouring of the first alloy terminating before the blocking of the passageway.
B · US 10,576,537 B2 · ¶ 8
Cite aspatent.fyi, US 2026/0364672 A1, claim 1, first published 2026-11-23T05:37:27-05:00, https://patent.fyi/US20260364672/, SHA-256 a165b163d95afe399b989f62813eac30e71ca04e83e50eb0eac20f0b78354bea
First published
Permanent addresshttps://patent.fyi/US20260364672/
Content fingerprint (SHA-256)a165b163d95afe399b989f62813eac30e71ca04e83e50eb0eac20f0b78354bea
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi