1.1Reusable coated iron mold
Two machined cast iron halves close around a cavity and receive molten aluminum through a gravity-fed sprue. A refractory wash limits adhesion, and ejector pins release the casting after solidification.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Two machined cast iron halves close around a cavity and receive molten aluminum through a gravity-fed sprue. A refractory wash limits adhesion, and ejector pins release the casting after solidification.
A roller conveyor indexes the filled mold between two freestanding nozzle racks. Opposing rows of jets sweep the exposed mold faces, and the warmed gas discharges into the surrounding air.
Two flat platens press against machined pads on a steel flask surrounding the sand mold. Heat conducts through the sand, flask, and platens into water circulating through sealed channels.
A centrifugal blower directs a free jet into a bellmouth receiver on the nozzle manifold. The receiver recovers part of the jet's velocity pressure, which drives airflow through short, large-bore nozzles aimed at the mold.
A fixed-speed blower feeds the nozzles throughout the casting run. The conveyor carries each filled mold through the jet zone, where the zone length divided by belt speed sets the exposure time.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Full-width slot diffusers replace the individual spray nozzles on two opposing walls of the cooling bath. A tapered distribution plenum feeds each slot, and a centered stand exposes both sides of the sand mold to the resulting sheets of gas. The controller regulates a common supply valve, and a roof outlet draws the warmed gas out of the bath.
A shared cooling bath holds two sand molds with footprints up to 300 by 300 millimeters on separate stands spaced 150 millimeters apart edge to edge. Each stand has four inward-facing round nozzles with 8-millimeter outlets placed 75 millimeters from the mold sidewalls. The controller sets each branch to 20 cubic meters per hour at nozzle inlet conditions for an initial trial and adjusts the branch settings independently using measured cooling curves.
An indexing roller conveyor carries filled sand molds on heat-resistant pallets from a pouring station into the cooling bath. A locating stop centers each pallet between the nozzle banks, and a position switch confirms that the mold is in place before the bath doors close. The conveyor controller holds the pallet in place during gas flow and releases it to the shakeout station after the cooling controller closes the gas valve and the doors reopen.
A return duct connects the top of the cooling bath to a sand dust filter, a gas-to-water heat exchanger, and a variable-speed recirculation blower in that order. The blower feeds the nozzle manifold, and a chilled water loop removes heat from the returning gas through the exchanger. The controller adjusts the water valve to hold the manifold inlet temperature and changes blower speed to hold gas flow as the filter loads.
Thermocouples embedded at equal depths in the sand beside two casting sections report temperatures to the controller. Two independently valved nozzle banks face the corresponding mold surfaces, and the controller estimates each zone's cooling rate from a moving window of temperature readings. At a fixed gas inlet temperature, the controller increases flow when a zone cools more slowly than its programmed rate, reduces flow when it cools faster, and closes both valves when both readings reach their programmed endpoints.
A quarter-turn ball valve sits upstream of the nozzle manifold. The operator opens the valve after loading the mold and closes it after a measured dwell.
A two-part mold uses silica sand mixed with a room-temperature curing resin binder. A tapered sprue feeds a runner and ingates, and a riser supplies liquid metal as the casting contracts during solidification.
A sheet steel cooling bath holds the filled mold on a raised steel grate. Two banks of straight-bore nozzles point toward opposite mold faces, and an upper vent discharges warmed gas.
A centrifugal blower draws air through an intake filter and feeds a common manifold through a flexible duct. Balancing dampers in the branch ducts set the flow to each nozzle bank.
A thermocouple embedded at a fixed depth below the mold exterior supplies temperature readings to a controller. The controller commands a variable-frequency drive to run the blower at high speed after loading and reduce speed when the reading falls below a preset threshold.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
To form a sand casting, sand is mixed with a binder resin, a cavity is formed within a block of this sand-binder combination, and molten metal is poured into the cavity to form a molded metal part.A · US 7,896,059 B2 · ¶ 1
One embodiment of the present invention describes a method of casting a metal alloy comprising the following steps: forming a sand based mold having the appropriate geometry to generate a desired object to be cast, placing the sand based mold in an open pressure vessel, filling the sand based mold with a molten metal alloy, immediately thereafter closing and pressure sealing the pressure vessel, pressurizing the sealed pressure vessel with an inert gas for a predetermined meaB · US 2016/0158837 A1 · ¶ 11
FIG. 3D shows an embodiment of the present invention in which the encapsulant may also preferably incorporate two nozzles 22 and 23 in order to facilitate drawing a vacuum on the mold and/or continuously or non-continuously flushing the mold with non-reactive or inert gases such as helium, nitrogen, argon, SF6 or CO2, to provide an inert mold cavity environment. The inert gas may continuously be drawn through the mold to purge, or it may be intermittently purged to achieve certain heat transfer results.A · US 7,896,059 B2 · ¶ 59
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.2. Both have a passage for 1.1. Both are classified in CPC B22D, as is this patent.
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
There have always been problems with this method, including the production of dross and oxidized state metals at the surface, along with all the problems of what to do with the sand after the casting has been made.A · US 7,896,059 B2 · ¶ 1
In addition, another problem arises because delivery of the molten metal is a relatively slow process into the sand cast mold because of turbulence issues, i.e. oxide problems need to be alleviated for faster delivery times.A · US 7,896,059 B2 · ¶ 2
Sand casting is a relatively inexpensive means to produce common everyday metal objects as well as intricate aerospace and military components.B · US 2016/0158837 A1 · ¶ 3
Sand molds can also be created by compacting the sand and binding agent in a flask and carving the desired mold form and gating directly into the aggregate mixture.B · US 2016/0158837 A1 · ¶ 3
A system and method of increasing a cooling rate of a metal sand casting during solidification.C · US 2023/0211406 A1 · abstract