patent.fyi
Applications  /  US 2026/0364675
United States Patent Application Publication

US 2026/0364675 A1

Published
Nov 19, 2026
Filed
Oct 20, 2023
Earliest date on the face
Dec 12, 2022
Classification
B22F 1/05
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Nickel and calcium eutectic forming additions

What ifWhat if nickel and calcium form the thermally stable intermetallic network without iron and cerium?
Claim language“iron and cerium”

Adding 2.0 to 5.5 wt. % nickel and 0.5 to 2.0 wt. % calcium to the melt produces a fine cellular eutectic network of aluminum-nickel and aluminum-calcium intermetallics during rapid laser solidification. Both elements have low solid solubility and low diffusivity in solid aluminum, which resists precipitate coarsening at service temperatures up to 300 degrees Celsius. The narrow freezing range of the eutectic composition suppresses hot tearing across steep thermal gradients during layerwise melting.

1.2Cobalt and erbium strengthening additions

What ifWhat if cobalt and erbium provide dispersoid strengthening and thermal stability without manganese, lanthanum and yttrium?
Claim language“manganese, lanthanum and yttrium”

Dissolving 0.4 to 1.2 wt. % cobalt and 0.2 to 0.8 wt. % erbium in the gas-atomized melt creates supersaturated solid solutions during rapid cooling at rates above 10000 Kelvin per second. Subsequent aging at 300 to 375 degrees Celsius precipitates coherent aluminum-erbium dispersoids and fine aluminum-cobalt intermetallic particles that pin dislocations and grain boundaries. This dual-precipitate microstructure maintains yield strength at elevated temperatures without manganese, lanthanum, or yttrium.

1.3Ceramic nanoparticle inoculation for grain refinement

What ifWhat if ex-situ ceramic nanoparticles nucleate equiaxed grains without zirconium, vanadium, chromium, hafnium and scandium?
Claim language“zirconium, vanadium, chromium, hafnium and scandium”

Electrostatic mixing or low-energy ball milling coats the base aluminum powder with 0.5 to 2.0 wt. % titanium diboride or titanium carbide particles sized at 20 to 200 nanometers. During laser melting, these high-melting-point ceramic particles remain solid inside the melt pool and act as low-mismatch heterogeneous nucleation sites ahead of the solidification front. Nucleation across the melt pool transitions columnar growth into fine equiaxed grains of 1 to 5 micrometers, preventing solidification cracking.

1.4Lithium addition with vacuum degassing

What ifWhat if vacuum-degassed lithium provides solid-solution strengthening and weight reduction without hydrogen and magnesium?
Claim language“hydrogen and magnesium”

Vacuum induction melting and inert gas atomization with dry argon reduce dissolved gas content below 1 ppm while incorporating 1.0 to 2.5 wt. % lithium into the aluminum matrix. Rapid solidification retains lithium in solid solution, increasing elastic modulus and reducing alloy density by 3 percent per weight percent added. Post-build aging at 150 to 190 degrees Celsius precipitates coherent aluminum-lithium particles that raise room-temperature tensile strength.

1.5Deliberate silicon and copper alloying additions

What ifWhat if silicon and copper are added deliberately at major alloying levels?
Claim language“unavoidable impurities”

Formulating the melt with 7.0 to 10.5 wt. % silicon and 1.5 to 3.5 wt. % copper shifts the composition near the aluminum-silicon eutectic point, lowering the liquidus temperature and narrowing the solidification interval. During laser powder bed fusion, the high-silicon liquid exhibits high fluidity that fills interdendritic channels and reduces hot cracking. Subsequent solution treatment and artificial aging at 160 to 190 degrees Celsius precipitate aluminum-copper phases for elevated room-temperature hardness.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cold spray repair of worn marine turbine casings

A high-pressure cold spray deposition unit accelerates the aluminum-iron-cerium-titanium alloy powder with group A and group B additions through a converging-diverging nozzle using preheated helium or nitrogen gas at 2.5 to 4.0 megapascals and 350 to 450 degrees Celsius. The supersonic particle stream impacts a grit-blasted aluminum alloy marine turbine casing at velocities between 650 and 900 meters per second, bonding to the damaged surface through severe plastic deformation without melting the feedstock. The solid-state deposition retains the sub-micrometer intermetallic dispersion and supersaturated solid solution formed during powder solidification, producing a dense corrosion-resistant repair layer with porosity below 1.0 percent. A five-axis machining center mills the deposited buildup back to the original casing geometry after spraying completes.

Component substitution

Erbium and nickel substitution for cerium and iron

In this feedstock composition, erbium replaces cerium at 0.35 to 2.6 weight percent and nickel replaces iron at 0.3 to 1.5 weight percent within the aluminum matrix, while retaining titanium, group A elements, and group B elements in their base concentration ranges. During rapid solidification in laser powder bed fusion, nickel forms thermally stable aluminum-nickel eutectic networks along cellular boundaries and erbium precipitates coherent tri-aluminide dispersoids together with zirconium or scandium from group B. The alloy melt is prepared in an induction furnace under an inert argon atmosphere at 820 to 880 degrees Celsius to dissolve the higher-melting rare-earth and transition-metal master alloys completely prior to atomization. Resulting consolidated parts undergo direct aging at 300 to 350 degrees Celsius for 4 to 8 hours without a separate solution heat treatment step.

Ultrasonic atomization replacing gas atomization for powder production

An ultrasonic atomization unit replaces a gas atomization nozzle to convert molten aluminum-iron-cerium-titanium alloy with group A and group B additions into spherical additive manufacturing powder. A molten stream feeds at 0.5 to 1.5 kilograms per hour onto a heated titanium-alloy sonotrode vibrating at 20 to 40 kilohertz inside an argon-filled chamber maintained at atmospheric pressure. Capillary waves on the thin liquid film break into droplets with a narrow particle size distribution centered at 35 micrometers and satellite particle counts below 2 percent. Droplets solidify in free fall through a 1.8 meter argon cooling column and collect in a sealed stainless-steel hopper without high-pressure gas consumption.

Parameter or scale variation

Bimodal particle size distribution for high-speed laser melting

Two sieved fractions of the aluminum-iron-cerium-titanium powder alloy are blended in a dry tumbling mixer to produce a bimodal feedstock consisting of 70 weight percent coarse particles sized 45 to 75 micrometers and 30 weight percent fine particles sized 10 to 20 micrometers. The fine fraction fills interstitial voids between the coarse spheres during recoating, raising the powder bed tap density from 56 percent to 68 percent of theoretical alloy density. A laser powder bed fusion machine processes this blended bed at a layer thickness of 80 micrometers, a laser power of 650 watts, a scan speed of 1800 millimeters per second, and a hatch spacing of 0.14 millimeters. The build platform is maintained at 180 degrees Celsius throughout fabrication to limit residual thermal gradients across the thicker melt pools.

Combination with existing systems

Laser powder bed fusion coupled with hot isostatic pressing

Parts consolidated from the aluminum-iron-cerium-titanium powder alloy in a laser powder bed fusion system are transferred directly on their build plate into a heated pressure vessel for hot isostatic pressing. The vessel pressurizes with 99.999 percent pure argon to 100 to 150 megapascals while heating the components to 380 to 420 degrees Celsius for 2 to 3 hours, collapsing internal lack-of-fusion pores and gas voids through localized creep deformation. A controlled cooling loop inside the vessel reduces the temperature at 15 degrees Celsius per minute to suppress coarsening of the iron-rich and cerium-rich intermetallic phases while preserving precipitation strengthening from the group B elements. After depressurization, a wire electrical discharge machine separates the densified parts from the build plate.

Automated or data-driven variant

Closed-loop melt pool control using coaxial optical pyrometry

A coaxial two-color optical pyrometer and a high-speed photodiode are mounted in the optical path of a laser powder bed fusion machine to sample thermal emission from the aluminum alloy melt pool at 50 kilohertz. A real-time digital signal processor compares the measured radiance against a lookup table trained on prior test builds of the aluminum-iron-cerium-titanium powder alloy to detect magnesium vaporization plumes or balling instabilities. When the emission signal crosses upper or lower threshold bands, a proportional-integral-derivative controller modulates the laser power between 250 and 450 watts within 100 microseconds to keep the melt pool cross-section constant. The control unit logs synchronized layer coordinates, laser power traces, and pyrometer readings to a local time-series database for automated voxel-level defect flagging after the build finishes.

Specific version of a part

Master alloy dosing of iron and cerium

Induction melting combines pure aluminum ingot with pre-alloyed aluminum-10 wt. % iron and aluminum-20 wt. % cerium master alloys at 850 to 920 degrees Celsius under an argon blanket. Holding the melt at 900 degrees Celsius for 20 minutes with electromagnetic stirring dissolves refractory intermetallic lumps and homogenizes iron at 0.8 wt. % and cerium at 1.5 wt. %. Rapid cooling during atomization freezes the iron and cerium into submicron intermetallic networks without coarse primary needles.

Zirconium and scandium precipitation hardening pair

Adding 0.7 wt. % zirconium and 0.4 wt. % scandium into the melt creates primary aluminum-zirconium-scandium trialuminide nuclei along the melt pool boundary during laser solidification. These coherent cubic nuclei drive equiaxed grain formation across the melt pool bottom, yielding grain sizes of 1 to 3 micrometers. A direct post-build aging cycle at 325 degrees Celsius for 4 hours precipitates nanoscale core-shell dispersoids throughout the aluminum matrix.

Magnesium strengthening with controlled hydrogen degassing

Pure magnesium is plunged into the molten bath at 760 degrees Celsius to reach 3.0 wt. % while a rotary impeller injects dry argon gas to control dissolved hydrogen at 10 to 25 ppm. Vacuum drying of the atomized powder at 80 degrees Celsius for 6 hours removes surface moisture before laser scanning. Controlling hydrogen within this narrow window limits spherical gas porosity in as-built parts below 0.2 volume percent while magnesium provides solid-solution strengthening.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2007/0297936 A1
Published
Dec 27, 2007
Filed
Jun 23, 2006
Class
C22C 21/10
Document BUS 2019/0078186 A1
Published
Mar 14, 2019
Filed
Mar 8, 2017
Class
C22F 1/06
Claim 1
Document A
Document B
1.1iron and cerium
1.2at least one element from group A comprising manganese, lanthanum and yttrium
For example, in Patent Literatures 1 and 2, the plastic deformability has been improved by the addition of rare earth elements including yttrium (Y), cerium (Ce), and lanthanum (La).
B · US 2019/0078186 A1 · ¶ 3
1.3at least one element from group B comprising zirconium, vanadium, chromium, hafnium and scandium
The aluminum alloy contains about 2.2-3.0 wt. % magnesium, about 0.1-0.97 wt. % scandium, and about 0.14-0.9 wt. % zirconium. The alloy may also contain about 0.1-0.4% wt. % iron, 0.001-0.2 wt. % chromium, 0.02-0.94 wt. % titanium, and silicon, copper, zinc and manganese up to about 0.20 wt. %, 0.1 wt. %, 0.1 wt. %, and 0.01 wt. %, respectively, either as additives intentionally added during processing or as impurities, the remainder being aluminum.
A · US 2007/0297936 A1 · abstract
In Patent Literature 3, a fine grain Mg alloy in which one kind of elements selected from the group consisting of Ca, Sr, Ba, Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Dr, Tm, Yb, and Lu, each of which is a rare earth element or a general-purpose element, are contained in a minute amount; the grains are refined; and the strength properties are excellent has been disclosed.
B · US 2019/0078186 A1 · ¶ 5
1.4optionally: hydrogen and magnesium
The aluminum alloy contains about 2.2-3.0 wt. % magnesium, about 0.1-0.97 wt. % scandium, and about 0.14-0.9 wt. % zirconium.
A · US 2007/0297936 A1 · abstract
1.5aluminum and unavoidable impurities, including silicon, copper and zinc
The alloy may also contain about 0.1-0.4% wt. % iron, 0.001-0.2 wt. % chromium, 0.02-0.94 wt. % titanium, and silicon, copper, zinc and manganese up to about 0.20 wt. %, 0.1 wt. %, 0.1 wt. %, and 0.01 wt. %, respectively, either as additives intentionally added during processing or as impurities, the remainder being aluminum.
A · US 2007/0297936 A1 · abstract
1.6said elements having the following concentrations, in wt. %:

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.4 1.5. Only Document B has a passage for 1.2. Both have a passage for 1.3.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Therefore, the need exists for aluminum alloys with magnesium content lower than 3 wt. % to counter corrosion attack.
A · US 2007/0297936 A1 · ¶ 4
Testing has shown that the addition of scandium provides greater strength than aluminum alloys of comparable magnesium content through the formation of fine, evenly distributed aluminum-scandium dispersoids, while the addition of zirconium prevents dispersoid coarsening at elevated temperatures, thereby providing flexibility in forming products with the alloy.
A · US 2007/0297936 A1 · ¶ 10
More specifically, the present invention relates to a wrought processed Mg-based alloy of fine grains, which is added by bismuth (Bi) and excellent in ductility at room temperature, and to a method for producing the wrought processed Mg-based alloy.
B · US 2019/0078186 A1 · ¶ 1
In addition, from the viewpoint of the productivity, development of an Mg-based alloy that is excellent in ductility at room temperature and the formability in a faster deformation speed range has been desired.
B · US 2019/0078186 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0364675 A1, claim 1, first published 2026-11-23T05:37:27-05:00, https://patent.fyi/US20260364675/, SHA-256 6b6dfcea1685ef4c6a758907b3a34cd33bed8223e63ccbe7e922213f5c151d62
First published
Permanent addresshttps://patent.fyi/US20260364675/
Content fingerprint (SHA-256)6b6dfcea1685ef4c6a758907b3a34cd33bed8223e63ccbe7e922213f5c151d62
Methodv2026-11-18.2 · automated, not reviewed by a person