1.1Lubrication at the die wall
A spray nozzle coats the die bore with a thin wax film before powder filling. The film reduces sliding friction against the die wall during compaction and ejection.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A spray nozzle coats the die bore with a thin wax film before powder filling. The film reduces sliding friction against the die wall during compaction and ejection.
A porous ceramic mold draws liquid from a suspension of titanium powder by capillary action. Powder accumulates against the cavity wall, and a small binder fraction holds the particles together after drying.
A shaped die cavity defines the outer profile, and a core pin forms the through-hole. Annular punches compact powder around the pin, which withdraws before the compact is ejected.
A vacuum pump maintains reduced pressure as the furnace heats a compact containing a low-molecular-weight paraffin lubricant. Wax vapor travels through interconnected pores and condenses in a cooled trap upstream of the pump.
The cut compact sits on a support tray in a circulating heptane bath that dissolves its paraffin lubricant. Fresh solvent maintains the concentration gradient through the open pores, and room-temperature evacuation removes residual solvent.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A uniaxial die with a core pin pressure-molds lubricated titanium powder into annular blanks for seawater pump shaft assemblies. A lathe cuts the faces and bore of each green blank, with machining allowances based on measured axial and radial sintering shrinkage. An argon furnace removes the lubricant at 400 °C or below, and a vacuum furnace sinters the blanks. Face grinding sets the final spacer thickness and parallelism.
A vacuum debinding chamber replaces the inert-gas chamber for heat treatment of the cut green compacts. The compacts contain a low-molecular-weight paraffin wax as the compaction lubricant and rest on open trays connected by a vapor path to a condensate trap upstream of the vacuum pump. The chamber heats the compacts in stages through the wax volatilization range, with holds that let vapor escape through the connected pores. The dried compacts then enter a vacuum furnace for sintering.
Opposed punches pressure-mold lubricated titanium powder into cylindrical green blanks 40 mm in diameter and 25 mm high. A supported machining fixture holds each blank while a drill cuts a 20 mm axial through-bore, leaving a 10 mm radial wall. The bore gives lubricant vapor an escape surface at the inner diameter during argon debinding at 400 °C or below. Vacuum sintering follows, and the bore and outside diameter contract from their green dimensions.
A batch furnace combines a controlled argon inlet, a debinding exhaust with a condensate trap, and a separately valved high-vacuum pumping line. Cut green compacts rest on refractory setters while flowing argon carries lubricant vapor to the trap during heating at 400 °C or below. After the debinding hold, the controller closes the argon inlet and debinding exhaust, then evacuates the chamber through the vacuum line. The furnace raises the same load to the sintering temperature under vacuum.
A heated sampling line carries part of the argon exhaust from the debinding furnace to a flame ionization detector. The controller records the hydrocarbon signal against an empty-furnace baseline and holds the load at the selected debinding temperature at or below 400 °C. The hold ends when the signal stays below a threshold established by comparing trial runs with residual carbon measurements on debound compacts. The controller logs the endpoint and releases the batch for vacuum sintering.
A laser micrometer measures the axial and radial dimensions of reference pieces before and after vacuum sintering. Software stores separate axial and radial shrinkage factors for each powder lot and compaction recipe. A numerically controlled lathe applies those factors to the target finished dimensions and cuts the lubricated green compacts to the resulting larger dimensions. The cut compacts undergo argon debinding at 400 °C or below followed by vacuum sintering, and measured finished dimensions supply feedback for subsequent batches.
A sealed rotating drum blends titanium powder with 0.5 percent by mass of micronized paraffin wax. Repeated tumbling distributes the wax through the powder before die filling.
Upper and lower punches compress the lubricated powder in a rigid cylindrical die at a nominal axial pressure of 500 MPa. Punch travel from both ends reduces the axial density gradient.
A supported fixture holds the powder compact while a sharp carbide end mill cuts a shallow groove in several passes. The groove dimensions account for shrinkage during sintering.
After cutting, a furnace heats the compact under flowing dry argon at about 1 °C per minute through the lubricant removal range. A hold at 380 °C gives residual paraffin time to volatilize, and the gas flow carries vapor to a cooled collector.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Further, in the kneaded material, other than the titanium alloy powder, the organic binder, and the plasticizer, for example, any of a variety of additives such as a lubricant, an antioxidant, a degreasing accelerator, and a surfactant can be added.A · US 2019/0061003 A1 · ¶ 100
The molding method is not particularly limited, and for example, any of a variety of molding methods such as a powder compacting (compression molding) method, a metal injection molding (MIM) method, and an extrusion molding method can be used.A · US 2019/0061003 A1 · ¶ 105
A method for producing a nitrogen solid solution titanium sintered compact according to the present invention includes a step of mixing a titanium component powder made of a titanium component having an α-phase with nitride particles of a metal other than titanium, a step of applying a compression force to shape a mixed powder obtained through the mixing, and a step of heating and sintering a compressed shaped compact, which is obtained through the compression shaping, in a sB · US 10,807,164 B2 · ¶ 14
Further, if desired, the molded body may be subjected to machining processing such as grinding, polishing, or cutting.A · US 2019/0061003 A1 · ¶ 111
The atmosphere when the molded body is heated is not particularly limited, and an atmosphere of a reducing gas such as hydrogen, an atmosphere of an inert gas such as nitrogen or argon, an atmosphere of an oxidative gas such as air, a reduced pressure atmosphere obtained by depressurizing such an atmosphere, and the like are exemplified.A · US 2019/0061003 A1 · ¶ 116
Subsequently, the obtained degreased body is fired in a firing furnace, whereby a sintered body is obtained.A · US 2019/0061003 A1 · ¶ 120
Pressurized vacuum sintering was carried out on the above mixed powder with use of a spark plasma sintering machine (SPS) under the conditions with a sintering temperature of 1273 K, holding time of 3.6 ks, an applied pressure of 30 MPa, and a vacuum degree of 6 Pa or less.B · US 10,807,164 B2 · ¶ 139
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.1 1.3 1.4. Both have a passage for 1.2 1.5. Both are classified in CPC B22F, as is this patent.
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Further, in the application of a titanium alloy in this manner, by using a powder metallurgy method, a titanium sintered body having a shape close to the final shape can be easily produced.A · US 2019/0061003 A1 · ¶ 3
Related claim parts: 1.2 1.5
However, a titanium sintered body produced by a powder metallurgy method is likely to reflect the properties of a raw material powder, and therefore, it is difficult to obtain an appearance with a high design property.A · US 2019/0061003 A1 · ¶ 4
An advantage of some aspects of the invention is to provide a titanium sintered body, an ornament, and a timepiece having a high design property.A · US 2019/0061003 A1 · ¶ 7
Since the demand for compatibility between a high strength and a high ductility and for reduction of the material cost on titanium is extremely strong, various studies have been made so far.B · US 10,807,164 B2 · ¶ 4
An object of the present invention is to provide a high-strength titanium sintered compact and a method for producing the same that can achieve an improvement in the characteristics by incorporating other metals or compounds into a matrix in addition to solid solution strengthening by nitrogen atoms.B · US 10,807,164 B2 · ¶ 8
patent.fyi, US 2026/0364677 A1, claim 1, first published 2026-11-23T05:37:27-05:00, https://patent.fyi/US20260364677/, SHA-256 12140b64d063f70bba7b392b02e0ef5d9f718ab7b043985d13460e0ec46cd295