Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Aqueous potassium carbonate misting
What ifWhat if the composition uses an atomized aqueous potassium carbonate mist?
Claim language“liquid ammonia”
A fine mist of aqueous potassium carbonate at 5 to 15 percent concentration by weight is atomized into a heated treatment chamber at 60 to 80 degrees Celsius. The alkaline mist penetrates the wood surface, saponifies wood resins, and reacts with natural tannins to shift the wood color toward darker brown tones. A subsequent drying cycle removes excess moisture while leaving the darkened, softened surface layer intact.
1.2Aqueous surfactant carrier for dye
What ifWhat if the composition replaces methanol with an aqueous non-ionic surfactant carrier to dissolve and transport the dye?
Claim language“methanol; and”
Deionized water mixed with 0.5 to 2 percent by weight of an ethoxylated alcohol surfactant dissolves the dye and reduces liquid-wood interfacial tension. The aqueous carrier wets the cellulose microfibrils and carries dissolved dye molecules into the outer 1 to 3 millimeters of the wood grain under ambient or mild vacuum conditions. Controlled warm-air ventilation then evaporates the water while the dye remains fixed within the cell walls.
1.3Iron salt tannin reaction coloring
What ifWhat if the wood is colored by a chemical reaction between dissolved iron salts and natural wood tannins with no color dye?
Claim language“color dye”
An aqueous solution of ferrous sulfate at 1 to 4 percent concentration by weight is applied to the wood surface prior to or alongside alkaline fuming. The dissolved iron ions bind with endogenous hydrolyzable and condensed tannins in the wood cells to form insoluble dark grey to black iron-tannate complexes. Adjusting the iron salt concentration and wood species tannin content controls the final shade without adding synthetic or natural dye molecules.
1.3Uncolored wood fuming without dye
What ifWhat if the composition omits the color dye completely and relies solely on the volatile reagents to alter wood appearance?
Claim language“color dye”
The liquid ammonia and methanol mixture is applied to tannin-rich hardwood inside a closed fuming chamber at 20 to 35 degrees Celsius for 4 to 24 hours. Ammonia vapors react directly with naturally occurring polyphenols and tannins in the heartwood to produce uniform amber to dark brown coloration throughout the penetrated zone. Because no dye is present, the natural grain contrast and figure of the wood remain visible without surface masking.
1.2Supercritical carbon dioxide carrier fluid
What ifWhat if the treatment transports the ammonia and colorant using supercritical carbon dioxide?
Claim language“methanol; and”
Carbon dioxide is compressed above 7.4 megapascals and heated above 31 degrees Celsius in a high-pressure autoclave containing the wood. The supercritical fluid exhibits gas-like diffusivity and liquid-like solvation, carrying dissolved ammonia and colorant deep into refractory heartwood pores. Depressurizing the vessel returns the carbon dioxide to gas phase, leaving the treated wood dry and free of residual solvent.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Cellulose textile fiber dyeing and softening bath
A pressurized dyeing vessel receives woven cotton or linen fabric alongside a liquid mixture of anhydrous liquid ammonia, methanol, and a reactive azo dye. The ammonia swells the cellulose microfibrils to increase pore volume while the methanol acts as a co-solvent that keeps the dye dispersed in solution. After a residence time of 5 to 15 minutes at -33 degrees Celsius, a heated vacuum chamber evaporates and recovers both solvents in a closed-loop condenser. The treated fabric exits with uniform color penetration and a softened hand without aqueous effluent.
Component substitution
Ethanol co-solvent replacing methanol in ammonia dye
A liquid treatment formulation combines 75 percent by weight anhydrous liquid ammonia, 22 percent by weight anhydrous ethanol, and 3 percent by weight metal-complex dye in a chilled stainless steel mixing tank. Ethanol replaces methanol as the polar protic co-solvent to solubilize the dye while lowering vapor toxicity in open-ventilation transfer lines. A metering pump injects the single-phase solution into a sealed wood impregnation cylinder maintained at 600 kilopascals. Once penetration finishes, a thermal desorption unit flashes off the ammonia and ethanol mixture for fractional condensation and reuse.
Pigment nanoparticle dispersion replacing soluble color dye
A wood coloring mixture substitutes an organic or inorganic pigment dispersion having a particle size below 100 nanometers for the dissolved color dye in the liquid ammonia and methanol carrier. An ultrasonic homogenizer disperses the pigment particles with a polymeric steric stabilizer in methanol before blending the slurry into liquid ammonia inside a cooled pressure vessel. During impregnation, the ammonia plasticizes the wood cell walls while the methanol carrier transports the suspended nanoparticles into the lumen and pit openings. Evaporation of the volatile solvents leaves lightfast pigment particles mechanically locked inside the wood microstructure.
Parameter or scale variation
High-pressure cycle with reduced ammonia concentration
A high-pressure treatment vessel operates with a liquid composition containing 50 to 60 percent by weight liquid ammonia, 35 to 45 percent by weight methanol, and 1 to 5 percent by weight acid dye. Timber boards of 25 millimeter thickness sit inside an autoclave pressurized to 1200 kilopascals with nitrogen gas at 20 degrees Celsius for 45 minutes. The elevated pressure drives the lower-ammonia solution 8 to 12 millimeters into the wood cell walls despite the reduced ammonia fraction. Following depressurization, a 60 degree Celsius air-sweep kiln removes residual methanol over 4 hours.
Combination with existing systems
Closed-loop vacuum impregnation and ammonia recovery system
A wood treatment plant integrates a liquid ammonia, methanol, and dye storage manifold with a vacuum-pressure wood preservation autoclave and a two-stage vapor recovery unit. A rotary vane vacuum pump evacuates air from the loaded autoclave to 10 kilopascals absolute pressure before a transfer valve admits the chilled liquid composition. After soaking, a steam-heated jacket warms the vessel to 50 degrees Celsius while a water-cooled condenser liquefies the escaping methanol and a refrigerated compressor re-liquefies the ammonia gas. Inline check valves and a surge tank return the recovered solvents to the mixing manifold for subsequent batches.
Automated or data-driven variant
Spectrophotometric feedback control for dye and solvent dosing
An automated mixing skid pairs Coriolis mass flow meters and an inline ultraviolet-visible spectrophotometer with a programmable logic controller to regulate the ammonia, methanol, and dye ratios. The controller samples optical absorbance at the dye peak wavelength every 2 seconds and adjusts a positive-displacement dye metering pump to hold concentration within 0.1 percent by weight of the setpoint. Ultrasonic level sensors and pressure transducers inside the impregnation cylinder feed live penetration-rate data to a regression model that calculates the exact soak duration for each wood species and moisture content. When the model predicts full target depth, the controller automatically closes the supply valve and initiates the solvent recovery cycle.
Specific version of a part
Anhydrous pressurized liquid ammonia feed
Liquefied anhydrous ammonia stored in a steel cylinder under its own vapor pressure of approximately 0.85 megapascals at 20 degrees Celsius is metered through a mass flow controller into a chilled mixing manifold. Maintaining the ammonia in an anhydrous liquid state minimizes water-induced swelling of cellulose fibers while maximizing lignin plasticization. A back-pressure regulator prevents premature flashing until the mixture enters the treatment zone.
Anhydrous technical-grade methanol co-solvent
Technical-grade methanol with a water content below 0.1 percent by weight is blended at 20 to 40 percent by volume with the liquid ammonia to lower mixture viscosity and surface tension. The low molecular weight and polar hydroxyl group of methanol allow rapid wetting of hydrophobic resin canals and efficient solvation of the colorant. Following wood contact, the high vapor pressure of methanol enables rapid evaporation at ambient temperature without kiln heating.
Pre-metallized acid azo dye
A 1:2 metal-complex acid azo dye is dissolved at 0.5 to 3 percent by weight in the methanol and liquid ammonia mixture to provide lightfast brown or black coloration. The pre-metallized dye complex remains stable in the strongly alkaline ammonia environment without precipitating or shifting hue. After solvent evaporation, the dye molecules form hydrogen bonds and ionic interactions with polar sites on lignin and hemicellulose.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The fourth (DMPAT) step typically involves reacting the diester with aqueous ammonia, liquid ammonia or NaOH/NH4OH to produce the DMPAT; ammonium chloride is separated from the reaction, e.g., for industrial use.
A · US 11,198,700 B2 · ¶ 21
A system for ammonia distillation may include a condenser to condense ammonia vapor into liquid anhydrous ammonia, a flush tank to receive a flushed portion of the liquid anhydrous ammonia, a collection tank to receive a collected portion of the liquid anhydrous ammonia, and a corrosion inhibitor dispenser to transfer a corrosion inhibitor to the collected portion of the liquid anhydrous ammonia to form corrosion-inhibiting liquid anhydrous ammonia.
B · US 11,485,645 B2 · abstract
1.2methanol; and
The second (monoester) step typically involves reacting thiophosphoryl chloride in either a continuous or batch mode with methanol to produce O-methyl phosphorodichloridothioate (monoester).
A · US 11,198,700 B2 · ¶ 19
1.3color dye.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.2. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Because of the complexity of such insecticidal compositions and the chemicals and reactions associated with their production, there is a constant challenge to generate insecticidal compositions in a safe and effective manner.
A · US 11,198,700 B2 · ¶ 4
The present disclosure is generally related to ammonia distillation and, more particularly, to a system and method for ammonia distillation, for example, yielding high purity ammonia, ultra-high purity ammonia and corrosion-inhibiting ammonia.
B · US 11,485,645 B2 · ¶ 3
However, conventional distillation processes may not yield ammonia of sufficient purity.
B · US 11,485,645 B2 · ¶ 4
Cite aspatent.fyi, US 2026/0364843 A1, claim 1, first published 2026-11-22T17:45:17-05:00, https://patent.fyi/US20260364843/, SHA-256 461dd0f96389b49a36c0d234626b569c07fa730168b163b30773150393492625