Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Crosslinked epoxy substrate

What ifWhat if a cured epoxy panel supports the laminate without melting during assembly?
Claim language“a substrate having a melting temperature”

A heated mold cures an epoxy and glass fiber charge into a rigid, crosslinked panel. A two-part polyurethane adhesive cures between the panel and the laminate at room temperature.

1.2Perimeter-clamped optical laminate

What ifWhat if a removable bezel clamps the laminate against the substrate?
Claim language“a laminate bonded to the substrate”

A shallow recess locates the laminate laterally, and screws draw the bezel against the substrate. A silicone gasket distributes the clamping load along the laminate perimeter.

1.2Direct ultrasonic spot welds

What ifWhat if ultrasonic spot welds join the bonding film directly to the optical film?
Claim language“an adhesive layer”

A patterned ultrasonic horn presses the films together at points along the perimeter, outside the viewing area. Compatible thermoplastic surfaces melt locally and fuse as the spots cool under pressure.

1.3Common polyester melting point

What ifWhat if the substrate and optical film use the same polyester grade and have a melting-temperature difference of about 0 °F?
Claim language“is about 50 to 250 °F”

An extruded polyethylene terephthalate sheet provides support, and a biaxially oriented film of the same resin grade provides the optical surface. A room-temperature acrylic transfer adhesive joins the layers without relaxing the film orientation.

1.3Melting gap above 250 degrees

What ifWhat if the substrate melts near 649 °F and the optical film melts near 329 °F?
Claim language“is about 50 to 250 °F”

A polyether ether ketone plate supports a clear biaxially oriented polypropylene film, with a melting-temperature gap of about 320 °F. A low-surface-energy acrylic adhesive bonds the film to the plasma-treated plate under roller pressure at room temperature.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Viewing window for a seed hopper

The window uses a 2 mm clarified polypropylene substrate, a 75 µm polypropylene bonding film, a cured polyurethane adhesive layer, and a 100 µm clear polyester optical film. The adhesive joins the two films, and a heated perimeter die welds the exposed polypropylene face of the laminate to the substrate. The window mounts in the hopper wall with the polyester face outward, where it provides a wipeable viewing surface for checking the fill level.

Component substitution

Polyamide film for a translucent cover

A 50 µm translucent polyamide 6 film serves as the optical film and melts near 220 °C. A two-part polyurethane adhesive bonds the polyamide film to a corona-treated high-density polyethylene bonding film, and the adhesive cures before the assembly step. A heated press fuses the exposed polyethylene face to a high-density polyethylene substrate that melts near 130 °C.

Copolyester sheet as the adhesive layer

A 25 µm thermoplastic copolyester adhesive sheet sits between a clear polyester optical film and a glycol-modified polyester bonding film with a crystalline melting transition near 165 °C. Heated rollers activate the adhesive sheet near 110 °C and wet both film surfaces. The bonding film faces a molded substrate made from the same glycol-modified polyester. A short heated press cycle applies heat through the substrate to fuse the mating faces, while a cooled platen supports the optical film and limits heating of the adhesive.

Parameter or scale variation

Segmented film on a wide panel

A 600 mm wide high-density polyethylene panel carries six 95 mm wide strips with 5 mm gaps between adjacent strips. Each strip contains a 75 µm high-density polyethylene bonding film, a 15 µm cured polyurethane adhesive layer, and a 100 µm clear polyester optical film. A heated roller bonds the strips to the panel one at a time with the polyethylene faces down. The gaps interrupt the optical skin across the panel width and let adjacent strips move independently during thermal cycling.

Combination with existing systems

Laminated diffuser for a machine vision backlight

A machine vision backlight uses a translucent polypropylene substrate as the front diffuser over a light-emitting diode array. A cured polyurethane adhesive joins a matte polyester optical film to a polypropylene bonding film, and the exposed polypropylene face is welded around the diffuser perimeter. The diffuser spreads light from the array, and the matte outer surface reduces specular reflections from overhead lighting during image capture.

Automated or data-driven variant

Closed-loop welding with thermal feedback

A servo press welds a high-density polyethylene substrate to a laminate containing a high-density polyethylene bonding film, a cured polyurethane adhesive layer, and a clear polyester optical film. A setup coupon carries a thin thermocouple at the polyethylene interface to establish the relationship between tool temperature, dwell time, and interface temperature. During production, a tool thermocouple and a load cell provide feedback for heater output and press force, and the controller uses the coupon calibration to set dwell time. The fixture holds the assembly under pressure during cooling to limit warping.

Specific version of a part

Alumina ceramic substrate

The alumina plate supplies stiffness and a flat mounting face. An acrylic transfer adhesive wets the cleaned ceramic under roller pressure and holds the laminate against it.

Molded polypropylene support

Injection molding forms a 2 mm polypropylene substrate with a flat laminate mounting face and reinforcing ribs on the reverse side. The polypropylene homopolymer has a melting peak near 329 °F.

Polyethylene-backed polyester laminate

An optically clear acrylic adhesive joins a 50 µm polyethylene terephthalate optical film to a 75 µm high-density polyethylene bonding film after corona treatment of the polyethylene. A heated press bonds the exposed polyethylene face to a high-density polyethylene substrate, with both polyethylene layers melting near 266 °F and the optical film melting near 482 °F.

Polypropylene and polyester pair

A polypropylene substrate melts near 329 °F, and a polyethylene terephthalate optical film melts near 482 °F. The resulting melting-temperature difference is about 153 °F.

Nylon and polypropylene pair

A nylon 6 substrate melts near 428 °F, and a clear biaxially oriented polypropylene optical film melts near 329 °F. The resulting melting-temperature difference is about 99 °F.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2005/0127575 A1
Published
Jun 16, 2005
Filed
Dec 15, 2003
Document BUS 10,392,845 B2
Published
Aug 27, 2019
Filed
Mar 10, 2015
Class
E05D 15/165
Claim 1
Document A
Document B
1.1a substrate having a melting temperature in a first temperature range; and
A method of manufacturing a vehicle trim component includes providing a thermoplastic substrate.
A · US 2005/0127575 A1 · abstract
1.2a laminate bonded to the substrate, the laminate comprising: a bonding film having a melting temperature in the first temperature range; an adhesive layer; and an optical film having a melting temperature in a second temperature range,
A method of manufacturing a vehicle trim component, the method comprising the steps of: a. providing a substrate; b. providing a first material comprising a first layer and a thermoplastic layer; c. exposing portion of a surface of the thermoplastic layer of the first material to a source of heat such that the portion of the surface of the thermoplastic layer exposed to the source of heat is melted; and d. positioning the first material onto the substrate so as to bring the m
A · US 2005/0127575 A1 · claim 13
1.3wherein a difference between the melting temperature of the substrate and the melting temperature of the optical film is about 50 to 250 °F.
For example, one of the materials (polyamide, for example) has a melting point above 220° C., for example between approx. 210° C. and 265° C., while the other materials (POM and a thermoplastic elastomer, for example) have a melting point of below 190° C., for example in the range between approx. 165° C. and 190° C., and below 170° C., for example between approx. 80° C. and 170° C.
B · US 10,392,845 B2 · ¶ 17

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1 1.2. Only Document B has a passage for 1.3.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

However, known methods of manufacturing interior vehicle trim panels can add significant cost to each vehicle produced.
A · US 2005/0127575 A1 · ¶ 3
The first material is then positioned onto the thermoplastic substrate so as to bring the first material into contact with the melted surface of the thermoplastic substrate, thereby bonding the first material to the thermoplastic substrate and forming a vehicle trim component.
A · US 2005/0127575 A1 · ¶ 4
By using a separate sliding body, the carrier element has a friction-optimized portion only in a localized manner, and it is not necessary for the carrier element to have to be produced entirely from the expensive friction-reducing material.
B · US 10,392,845 B2 · ¶ 4
In order for the assembly effort to be reduced it is further known for the carrier element for a window lifting device to be produced by a multicomponent injection-molding method, so as not to produce individual bodies of the carrier element that are provided for dissimilar functions separately from one another and subsequently have to assemble said bodies.
B · US 10,392,845 B2 · ¶ 5
Cite aspatent.fyi, US 2026/0364918 A1, claim 1, first published 2026-11-23T09:08:10-05:00, https://patent.fyi/US20260364918/, SHA-256 899dee4813d82e22257f14ef3506a9caebd0d087860764fc51840603aa64a5a2
First published
Permanent addresshttps://patent.fyi/US20260364918/
Content fingerprint (SHA-256)899dee4813d82e22257f14ef3506a9caebd0d087860764fc51840603aa64a5a2
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi