United States Patent Application Publication

US 2026/0364920 A1

Published
Nov 19, 2026
Filed
Jul 31, 2023
Earliest date on the face
Oct 21, 2022
Classification
B32B 15/088
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Polyamide 12 outer film

What ifWhat if polyamide 12 were the sole polymer in the outer film?
Claim language“a polyamide 11”

A slot die casts a polyamide 12 web, and a stretching line draws it along and across the web before heat setting. The long methylene segments between amide groups limit moisture uptake, while the oriented film carries tensile load as the laminate draws into the die.

1.1Elastomer-modified polyamide blend

What ifWhat if polyamide 11 made up 70% of the film by mass and a polyether block amide made up the remaining 30%?
Claim language“80% by mass or more”

A twin-screw extruder melt blends the polymers before a slot die casts the web for biaxial drawing. The polyamide-rich phase carries tensile load, and the flexible polyether blocks accommodate local strain as the laminate wraps around the punch corners.

1.2Lower ratio with wider corners

What ifWhat if the larger directional ratio were 1.7 and the forming punch had wider corner radii?
Claim language“2.0 or more and 3.0 or less”

The stretching and heat-setting conditions produce a film whose larger measured F30-to-upper-yield-stress ratio is 1.7. A punch with wider corner radii spreads deformation over a larger area and reduces peak tensile strain and foil thinning at a given draw depth.

1.2Cup testing by draw depth

What ifWhat if production lots were released on the basis of crack-free cup depth?
Claim language“dividing a stress at 30% elongation (F30) by the upper yield stress”

A rectangular punch draws laminated coupons at room temperature to a series of depths using a fixed corner radius and blank-holder force. Optical inspection identifies tears in the outer film, and transmitted light identifies pinholes in the foil. The deepest cup that passes both inspections sets the reported draw depth.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cold formed pockets for optical components

A biaxially stretched polyamide 11 film serves as the outer face of a polymer laminate for packaging polished optical components. A tie layer bonds the film to an inward-facing polyethylene seal layer that contacts the tray lid. At room temperature, a radiused punch draws the laminate into a shallow pocket while a blank holder controls feed from the flange. After loading, a lid with a polyethylene seal face heat seals to the flange.

Component substitution

Polyamide 12 as the film matrix

Polyamide 12 replaces polyamide 11 as the sole film resin. A flat die extrudes the dried resin onto a chill roll, and a laboratory biaxial stretcher draws the cast sheet along both original web axes at a temperature above its glass transition and below its melting point. The stretcher holds the drawn dimensions during heat setting and cooling. Tensile tests along both axes and room-temperature cup draws guide the selection of draw ratios and heat-setting conditions for the polyamide 12 film.

Parameter or scale variation

Thicker film for shallow pocket forming

A biaxially stretched polyamide 11 film has a nominal finished thickness of 50 μm. A cast sheet with a nominal thickness of 300 μm feeds a draw section set to 2.0 times in the flow direction and 3.0 times in the transverse direction, with the cast gauge adjusted against the measured finished thickness. A blank holder feeds the finished film into a room-temperature die with an 8 mm pocket depth and a 3 mm corner radius. Tensile tests on finished film verify that the larger of the two directional ratios of stress at 30% elongation to upper yield stress lies between 2.0 and 3.0.

Combination with existing systems

Web indexed forming and sealing

An intermittent roll-fed form-fill-seal machine feeds a laminate with the biaxially stretched polyamide 11 film facing outward and a heat-sealable polymer layer facing inward. Edge guides align the web, and a mechanical punch forms pockets against a matched die at room temperature while the web is stationary. The machine advances the pockets through loading and lid sealing stations. A downstream cutter separates individual packages through the sealed flange.

Digital strain mapping during die setup

An instrumented forming press combines a load cell and stroke encoder with stereo cameras that view the exposed film surface through an opening in the blank holder. A sacrificial blank of the biaxially stretched polyamide 11 film carries a random speckle pattern on the camera-facing side. The cameras acquire synchronized images during a room-temperature draw, and digital image correlation calculates surface strain at the visible pocket corners and shoulders. An operator adjusts the blank-holder force and compares strain maps between draws to identify settings that reduce strain concentrations.

Automated or data-driven variant

Automated tensile checks across the web

An automated sampling cell cuts film coupons in the flow and transverse directions from the left, center, and right positions of roll-end samples. A robotic gripper loads each coupon into a tensile tester, and an extensometer records strain alongside the measured force. Software identifies the first stress maximum associated with yielding and interpolates the stress at 30% elongation from each trace. The software records the larger directional ratio at each web position, flags values outside 2.0 to 3.0, and routes traces without a resolvable upper yield point for review.

Specific version of a part

Single-resin polyamide 11 film

Dried polyamide 11 pellets supply the entire film formulation. A slot die extrudes the melt onto a chill roll to form a web for biaxial stretching.

Polyamide blend with ten percent elastomer

Gravimetric feeders meter 90 parts polyamide 11 and 10 parts polyether block amide by mass into a twin-screw extruder. The extruder disperses the elastomer in the polyamide matrix and feeds the blend to a flat film die.

Transverse direction governs the ratio

A tensile tester measures upper yield stress and stress at 30% elongation on strips cut along and across the web under the same test conditions. The flow-direction stresses are 40 MPa and 88 MPa, giving a ratio of 2.2. The transverse stresses are 40 MPa and 104 MPa, giving the larger ratio of 2.6.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2010/0318012 A1
Published
Dec 16, 2010
Filed
Jun 15, 2010
Class
A61F 13/00
Document BUS 10,632,696 B2
Published
Apr 28, 2020
Filed
May 5, 2017
Class
B29D 11/00788
Claim 1
Document A
Document B
1.1a polyamide 11 in an amount of 80% by mass or more and 100% by mass or less
Advantageously, the polyamide 11 content by weight represents at least 50%, preferably at least 80%, of the total weight of the textile according to the invention.
A · US 2010/0318012 A1 · ¶ 50
1.2wherein the film has an F30/upper yield stress value of 2.0 or more and 3.0 or less in a direction having a larger F30/upper yield stress value between a flow direction and a transverse direction of the film, where the F30/upper yield stress value is obtained by dividing a stress at 30% elongation (F30) by the upper yield stress.
[(Breaking stress in tension)/(upper yield stress in tension)]≥1 (3)
B · US 10,632,696 B2 · ¶ 22

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1. Only Document B has a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

They require at least one supplementary production step for treating the surface and/or for adding an antibacterial additive to the mass.
A · US 2010/0318012 A1 · ¶ 12
The object of the present invention is therefore to provide bacteriostatic textile materials produced by a simple method, having the least number of steps, that does not adversely affect the flexibility or softness of the textile and which, instead of using agents that are harmful for the environment, rather uses bio-resourced raw materials.
A · US 2010/0318012 A1 · ¶ 14
The present invention relates to a polycarbonate resin film for film stretching which is a film formed from a polycarbonate resin containing a constitutional unit derived from a dihydroxy compound having a specific bonded structure and which has excellent heat resistance and mechanical properties and gives a stretched film reduced in thickness unevenness.
B · US 10,632,696 B2 · ¶ 2
In particular, when a film is produced through a stretching step, there are the cases where partial stretching occurs to give a thin central part and thick edge parts, resulting in an increased difference in thickness between the central part and the edge parts.
B · US 10,632,696 B2 · ¶ 3
Cite aspatent.fyi, US 2026/0364920 A1, claim 1, first published 2026-11-23T09:08:10-05:00, https://patent.fyi/US20260364920/, SHA-256 3f3e6da515c67b28ea1b004259347bcb74061aa53d12b2e51b777f82b6496692
First published
Permanent addresshttps://patent.fyi/US20260364920/
Content fingerprint (SHA-256)3f3e6da515c67b28ea1b004259347bcb74061aa53d12b2e51b777f82b6496692