Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Phosphate-based network former glass
What ifWhat if the glass network were built mainly from phosphorus pentoxide units?
Claim language“SiO2: 60% to 68%”
A phosphate glass melts at 1000 to 1200 degrees Celsius in a refractory-lined furnace. Its network consists of linked phosphate tetrahedra, with small additions of alkali and alkaline-earth oxides to adjust durability. The melt is cast or drawn into sheet and annealed, and the sheet transmits light in the visible and near-infrared bands.
1.12Iron-free glass with a coating filter
What ifWhat if the glass contained no deliberately tracked iron oxide and a thin-film interference stack on one surface set the transmission band?
Claim language“total iron oxide in terms of Fe2O3: 0.0030% to 0.5%”
Raw materials are chosen from low-iron sand and purified carbonates so the bulk glass is nearly colorless. A multilayer stack of alternating high-index and low-index oxide films is deposited by magnetron sputtering. The stack reflects selected infrared and ultraviolet bands and passes visible light.
1.5Zinc oxide as main divalent modifier
What ifWhat if the divalent modifier were zinc oxide and the glass contained no calcium oxide?
Claim language“CaO: 10% to 20%”
Zinc oxide replaces calcium carbonate in the batch and acts as a network modifier that lowers melt viscosity. The batch is melted in a continuous tank furnace and formed on a molten tin bath. The finished sheet is annealed in a lehr to relieve stress.
1.9Ion-exchanged surface in place of bulk alkali
What ifWhat if the bulk glass carried almost no sodium oxide and the alkali content came only from a thin surface layer made by ion exchange?
Claim language“Na2O: 0.0% to 20%”
A base glass is melted with a lithium-rich or potassium-rich composition and formed as sheet. The sheet is immersed in a molten salt bath at 350 to 450 degrees Celsius so that surface ions swap with larger ions from the bath. The exchange creates a compressive surface layer to a depth of tens of micrometers.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Cover glass for rooftop solar collector modules
A glass plate with a calcium-rich soda-lime-alumina composition forms the front cover of a rooftop photovoltaic module. The plate is 3.2 mm thick and is physically tempered by air-jet quenching. It is bonded to a rear sheet with a polymer encapsulant layer that surrounds the cell strings. The low iron oxide content raises transmission across the cell response band, and the high thermal expansion coefficient supports a high tempering stress.
Glazing for refrigerated display cabinets
A tempered glass plate of the recited composition forms the door pane of a refrigerated display cabinet in a retail setting. Two or three plates are spaced by a sealed spacer frame and filled with argon to form an insulating unit. The high expansion coefficient allows high tempering stress, which raises resistance to impact from carts. The low iron content gives a clear view of the products.
Component substitution
Strontium oxide replacing part of calcium oxide
A glass batch replaces 4 mol % of the CaO with SrO while the total RO content stays at 14 mol %. Strontium carbonate is the raw material for the substituted portion, and the remaining oxides stay in the same ranges. The melt is refined in a continuous tank furnace and formed on a molten tin bath as a flat ribbon. The heavier alkaline earth ion raises density and changes the viscosity curve and the glass transition temperature.
Parameter or scale variation
Thin tempered plate for lidar windows
A glass plate is cut to 2.0 mm thickness and 150 mm by 80 mm in area for use as a sensor window. The composition holds total iron oxide at 0.004 mol % and Al2O3 at 2.0 mol %. The plate is air-quenched from 650 °C to a surface compressive stress of 100 MPa. A spectrophotometer verifies transmittance above 90% at 905 nm, and the plate is mounted in a polymer gasket in front of a laser emitter and receiver.
Combination with existing systems
Laminated windshield with embedded sensor zone
Two glass plates are laminated with a polyvinyl butyral interlayer 0.76 mm thick to form a vehicle windshield. The outer plate has the recited composition and is bent by gravity sag bending in a furnace at about 620 °C. A bracket on the inner surface holds a forward-looking infrared ranging unit behind a region of the plate. The low iron content in that region limits infrared absorption along the beam path. The assembly is autoclaved at 130 °C and 1.2 MPa.
Automated or data-driven variant
Closed-loop melt control using spectral sensing
An inline spectrophotometer measures transmittance of the glass ribbon at 1550 nm after the annealing lehr. A controller compares the reading with a target value and adjusts the iron-bearing raw material feed rate and the furnace redox through the combustion air ratio. A regression model trained on batch records predicts the Fe2+ share from furnace temperature and cullet ratio. The controller updates the feed setpoints every 10 minutes.
Specific version of a part
Cerium-based ultraviolet absorption
Cerium oxide is added to the batch at a few tenths of a percent. In the melt it absorbs ultraviolet light through a charge-transfer band near the visible edge. The sheet then passes visible light while limiting ultraviolet exposure of an interlayer or sensor behind it.
Fluxing without boron oxide
The batch contains only silica, alumina, alkali and alkaline-earth sources. The furnace runs at about 1550 to 1600 degrees Celsius, and a sulfate fining agent removes bubbles. The melt is formed by the float process into flat sheet.
Low-iron glass with ferrous control
The batch uses low-iron sand and a small amount of a cerium-based oxidizer. The oxidizer holds most iron in the ferric state, which reduces absorption near 1000 nanometers. Total iron is kept near 0.01 percent in Fe2O3 terms for sensor cover glass.
Yttrium-doped glass for etch resistance
Yttrium oxide at 0.2 to 0.5 mol percent is added as a fine powder to the batch. It raises the elastic modulus and the chemical durability of the surface. The glass is cut and polished to form a sensor window.
Limestone-fed calcium oxide at 12 percent
Calcium oxide is supplied by crushed limestone at 12 mol percent in oxide terms. The batch is melted in a regenerative furnace and formed by the float process. The sheet is annealed and laminated with a polymer interlayer between two glass plies.
Soda ash-supplied sodium oxide at 14 percent
Sodium oxide at 14 mol percent is supplied by dense soda ash. The batch is melted at about 1500 degrees Celsius and refined with sulfate. The result is a float sheet 2 to 4 millimeters thick for building glazing.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Firstly, the alkali-free glass needs to contain silica in an amount of 55 to 65 mol %.
A · US 2006/0213165 A1 · ¶ 61
1.2Al2O3: 1.5% to 5.0%;
1.3B2O3: 0.0% to 5.0%;
As such a component, boron oxide is preferably used in an amount of 1 to 8 mol %.
A · US 2006/0213165 A1 · ¶ 69
The wavelength conversion glass includes a TeO2—B2O3—ZnO—BaO-based transparent glass containing tellurium dioxide (TeO2), boric oxide (B2O3), zinc oxide (ZnO), and barium oxide (BaO); and phosphor micro-particles dispersed in the transparent glass.
B · US 2018/0370847 A1 · abstract
1.4MgO: 0.0% to 10%;
The wavelength conversion glass may further contain at least one of Ta2O5, Nb2O5, Al2O3, ZrO2, Ta2O3, Y2O3, WO3, CeO2, In2O3, ZnO, MgO, CaO, and SrO when appropriate. In this connection, a content of the least one of Ta2O5, Nb2O5, Al2O3, Na2O, Li2O, K2O, La2O3, ZrO2, Ta2O3, Y2O3, WO3, CeO2, In2O3, ZnO, MgO, CaO, and SrO may be in a range of 0 exclusive to 15 mol % inclusive.
B · US 2018/0370847 A1 · ¶ 33
1.5CaO: 10% to 20%;
1.6SrO: 0.0% to 10%;
1.7BaO: 0.0% to 5.0%;
1.8Li2O: 0.0% to 10%;
1.9Na2O: 0.0% to 20%;
1.10K2O: 0.0% to 10%;
1.11Y2O3: 0.0% to 1.0%;
1.12total iron oxide in terms of Fe2O3: 0.0030% to 0.5%; SiO2+Al2O3+B2O3: 62% to 70%; R′2O: 14% to 20%; and RO: 10% to 20% (where RO represents a total content of MgO, CaO, SrO, and BaO, and R′2O represents a total content of Li2O, Na2O, and K2O).
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.1. Only Document B has a passage for 1.4. Both have a passage for 1.3.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
In a ceramic filter having such a structure, there is a fear that not only intended filtration is impossible but also mixing of to-be-treated fluid F into treated fluid after permeation through filter membrane 14 invites contamination of the treated fluid after permeation.
A · US 2006/0213165 A1 · ¶ 8
This has necessitated a water purifier enabling easy production of water which is sufficiently safe and has high quality.
A · US 2006/0213165 A1 · ¶ 3
Further, there is a problem that the PIG may not be used as a wavelength conversion component for a high output light source.
B · US 2018/0370847 A1 · ¶ 4
A purpose of the present disclosure is to provide a wavelength conversion glass exhibiting high transmittance, excellent thermal stability, and wavelength conversion efficiency.
B · US 2018/0370847 A1 · ¶ 6
Low-SiO2 glasses do not have sufficient chemical resistance either, in particular when they contain relatively large amounts of B2O3 and are low in alkaline earth metals.
C · US 7,157,392 B2 · ¶ 17
Related claim parts: 1.1
Document C: US 7,157,392 B2, published Jan 2, 2007. Cited for this statement only.
Cite aspatent.fyi, US 2026/0364923 A1, claim 1, first published 2026-11-23T09:08:10-05:00, https://patent.fyi/US20260364923/, SHA-256 77b10739abf39578bff3db40ef0e51d135c2fa0ffd69145e8b975f7441f65656