Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.6Cross-section electron probe profiling
What ifWhat if the K and Na concentration fluctuation in each layer were measured by energy-dispersive X-ray line scans on a polished cross-section?
Claim language“measured by SIMS along the lamination direction”
A cross-section of the element is cut and polished, and a focused electron beam steps across it in the lamination direction. The characteristic X-ray counts for K and Na are recorded at each step, and the maximum and minimum counts per layer are read from the line profile. The ratios of the maxima-minima differences are then computed from these counts.
1.5Uniform alkali concentration in each layer
What ifWhat if each piezoelectric layer had a flat K and Na concentration along the lamination direction, with the difference between the lower and upper bodies set by an overall composition step?
Claim language“a concentration of each of K and Na fluctuates along the lamination direction”
Each layer is deposited from a single precursor solution with a fixed K to Na ratio, and is crystallized in one thermal step at a constant heating rate so that no concentration gradient forms. The upper body uses a precursor with a different alkali ratio than the lower body. The layers then differ in mean composition, not in the profile within the layer.
1.4Side-by-side electrode arrangement
What ifWhat if the piezoelectric bodies were placed side by side on a single surface and driven by interdigitated electrodes?
Claim language“provided to be arranged in this order in a lamination direction”
A single piezoelectric film is formed on a substrate and a pair of comb-shaped electrodes is patterned on its upper surface. The applied voltage produces an electric field mainly in the film plane, which drives lateral strain. The lower and upper bodies are two adjacent regions of the film with different compositions.
1.1Bulk sintered body in place of layers
What ifWhat if the lower piezoelectric body were a single sintered ceramic plate thinned by grinding?
Claim language“formed of M (M≥1) layers”
Powders of the K, Na and Nb compounds are pressed, sintered, and ground to a thickness of a few tens of micrometers. The plate is bonded to the lower electrode with a conductive adhesive film. The body then has one continuous composition with no layer boundaries.
1.3Conductive liquid contact in place of upper electrode
What ifWhat if the top surface of the upper piezoelectric body were driven through the ejected conductive liquid held in a chamber, with no solid upper electrode?
Claim language“an upper electrode”
The liquid in the pressure chamber is an electrolyte-containing ink in contact with a thin insulating passivation layer over the upper body. A reference voltage is applied to the liquid through a metal contact in the supply path. The potential difference between the liquid and the lower electrode drives the piezoelectric body.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Ultrasonic transducer for medical imaging arrays
A linear array of piezoelectric elements is formed on a silicon substrate with a lower electrode, a two-layer lower piezoelectric body and a three-layer upper piezoelectric body of potassium sodium niobate. Each layer has a K and Na concentration profile with extreme values, and the upper layers have larger SIMS intensity swings than the lower layers. The elements sit on membranes over cavities at a pitch of 150 micrometers. A transmit circuit drives the elements with 3 to 10 MHz bursts, and a receive circuit reads the echo charge from the same electrodes. The graded layers raise the coupling coefficient of the membrane so that a lead-free probe operates in the body contact range.
Component substitution
Platinum-iridium lower electrode with strontium ruthenate seed layer
The lower electrode is a platinum film doped with iridium, 100 nm thick, covered by a 20 nm strontium ruthenate film that acts as the crystal seed for the first potassium sodium niobate layer. The M lower layers and N upper layers are deposited by sol-gel spin coating, with each coat dried at 180 °C and crystallized at 700 °C. The coating solutions use different K and Na precursor ratios per coat so that the concentration of each element oscillates inside each layer. SIMS depth profiling confirms that the upper layers show a wider K and Na swing than the lower layers, and the seed film holds the (100) orientation across the stack.
Parameter or scale variation
Thin stack with two lower and six upper layers
The piezoelectric stack uses M=2 lower layers of 60 nm each and N=6 upper layers of 60 nm each, for a total thickness of about 480 nm. The sputtered or sol-gel layers have an average K to Na ratio of 0.5 to 0.5 in both bodies. The K and Na intensity swings in the upper layers are set to 1.6 times those of the lower layers by increasing the precursor ratio step between coats from 5 percent to 8 percent. The element is driven at 20 V peak, below the 40 V used for thicker stacks, and is patterned at a 42 micrometer pitch for a high-density nozzle row at 1200 dots per inch.
Combination with existing systems
Piezoelectric element in a recirculating inkjet printhead
The element is mounted on a diaphragm above a pressure chamber in a silicon chamber plate. The chamber plate is bonded to a nozzle plate and to a manifold that supplies ink and recirculates it through a pump and a filter. A drive circuit applies a push-pull waveform of 25 V with a 2 microsecond rise time. The upper layers have larger K and Na swings than the lower layers, and this raises the displacement per volt so that a lower drive voltage ejects the same 5 picoliter drop. The head is fitted in a wide-format printer with a carriage or a fixed line bar.
Automated or data-driven variant
Closed-loop deposition control using in-line SIMS data
A deposition line records the SIMS depth profile of a test coupon after each production lot. Software extracts I1 to I8 for each layer and computes the ratios (I5−I6)/(I1−I2) and (I7−I8)/(I3−I4). If a ratio falls below 1.20, the controller raises the precursor ratio step for the upper coats of the next lot by 0.5 percent. A regression model trained on past lots links the ratios to the measured displacement, and the model sets the ratio limit that each lot must meet before release.
Self-calibrating drive using impedance sensing of elements
A printhead controller measures the capacitance and the residual vibration of each element after a test pulse. A trained regression model converts these values into an estimated displacement per volt for each element. The controller scales the drive voltage of each element within a range of ±10 percent so that every nozzle ejects the same drop volume. The calibration runs at power-up and after every 10,000 pages, and the results are stored in a table in non-volatile memory.
Specific version of a part
Sol-gel layers with repeated coating
The lower piezoelectric body is formed by spin-coating a precursor solution of potassium, sodium and niobium alkoxides and acetates, drying at 180 degrees Celsius, and degreasing at 380 degrees Celsius. Each layer is then crystallized at 700 degrees Celsius, and the cycle repeats for M equal to 5 layers.
Sputtered upper body with graded growth
The upper piezoelectric body is deposited by radio-frequency sputtering from a ceramic target containing K, Na and Nb oxides. The substrate temperature is cycled between 450 and 600 degrees Celsius during growth, and each cycle forms one layer with a periodic K and Na profile.
Platinum upper electrode with adhesion layer
The upper electrode is a sputtered platinum film of 50 nanometers thickness on a 5 nanometer titanium adhesion layer. The film is patterned by ion milling to match the pressure chamber width.
Lower electrode of iridium on titanium oxide
The lower electrode is a platinum film of 100 nanometers thickness, oriented along the (111) direction, grown on a titanium oxide seed layer over a silicon oxide film on a silicon substrate. The orientation of the electrode promotes (100) oriented growth of the alkali niobate layers above it.
Cite aspatent.fyi, US 2026/0364941 A1, claim 1, first published 2026-11-23T09:08:10-05:00, https://patent.fyi/US20260364941/, SHA-256 b89bbe341e1e0121390c869c9be1591233f4a2aa0963aeed2049859dea40e8a1