Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
No entries.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Welded glass covers for image sensors
A recessed glass cover contacts a glass spacer wafer along flat lands surrounding optical cavities. A focused pulsed laser writes two outer seam lines at the glass interface on opposite sides of each dicing lane. The laser then writes four parallel modification lines inside the cover glass between the seams. A dicing blade follows the lane center, leaving an attachment seam on each neighboring cover.
Component substitution
Borosilicate glass in place of fused silica
Two polished borosilicate wafers replace a fused silica pair and contact each other along the dicing lanes. A near-infrared picosecond laser focuses at the interface and scans two parallel paths to fuse the wafers locally. The focus then shifts into the upper wafer and scans four longitudinal modification tracks between the two seams. Test tracks on a coupon from the same glass lot set the pulse energy and scan speed for continuous seams and confined inner tracks.
Parameter or scale variation
Six inner tracks in a wider lane
Two contacting glass sheets carry parallel outer seam centerlines 240 micrometers apart. Six inner tracks run parallel to the seams at lateral offsets of minus 75, minus 45, minus 15, plus 15, plus 45 and plus 75 micrometers from the lane center. A pulsed laser places the outer seams at the interface and the inner tracks 40 micrometers above it in the upper sheet. A blade with a 60 micrometer kerf follows the lane center and removes the two innermost tracks.
Inner tracks at two substrate depths
Two 500 micrometer thick glass plates contact each other and carry outer seams 200 micrometers apart at their interface. A pulsed laser writes inner tracks at lateral offsets of 20 and 60 micrometers on each side of the lane center. The two tracks at 20 micrometers sit 30 micrometers above the interface, and the two tracks at 60 micrometers sit 90 micrometers above it. The laser writes the deeper tracks first through the upper surface so later scans form the shallower tracks.
Combination with existing systems
Laser welding with a wafer dicing saw
A laser welding head and a spindle dicing saw share a motion stage carrying the contacting wafer pair on a framed dicing film. The laser head uses wafer fiducials to locate each lane and writes two interface seams and four upper-wafer tracks along it. The saw uses a calibrated offset from the laser head to follow the centerline between the seams. The film supports the dies during cutting and retains their positions for pickup.
Automated or data-driven variant
Sensor guided focus along bowed wafers
A low-coherence optical sensor measures interface depth along each dicing lane before the laser scan. Motion-control software interpolates the depth measurements and moves the focusing objective to keep the beam waist at the local interface during both outer seam scans. The controller reuses the depth map with a fixed offset into the upper wafer for each of the four inner tracks. The stage encoder synchronizes the focus commands with the position along the lane.
Cite aspatent.fyi, US 2026/0365508 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365508/, SHA-256 3f5e7e16aa54e30aa2f42ba2b7fdcacfdbfe4a1ed04df530911da700e9278db8