patent.fyi
Applications  /  US 2026/0365515
United States Patent Application Publication

US 2026/0365515 A1

Published
Nov 19, 2026
Filed
Dec 6, 2023
Earliest date on the face
Dec 16, 2022
Classification
C01B 17/22
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Use solid sulfate grains

What ifWhat if the precursor consists of solid, angular lithium sulfate grains with no central cavity?
Claim language“has a hollow shape”

Crystallization followed by crushing produces solid lithium sulfate grains. The grains are mixed with carbon black and heated under argon to reduce the sulfate to lithium sulfide.

1.1Use open-pore sulfate granules

What ifWhat if the precursor consists of granules with a continuous solid skeleton and interconnected pores that open to the surface?
Claim language“has a hollow shape”

Wet granulation binds fine lithium sulfate and carbon particles into granules, and vacuum drying removes liquid from the spaces between grains. During heating under argon, the carbon reduces the sulfate and the open pore network lets gaseous reaction products escape.

1.3Use a number median

What ifWhat if D50 represents the diameter at which 50% of the particle count is accumulated?
Claim language“the particle size at which 50% of the volume is accumulated”

An automated microscope measures the projected area of each dispersed particle and converts it to the diameter of a circle with the same area. The diameter at the 50th percentile by count serves as the characteristic precursor size.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Component substitution

Ultrasonic atomizer for hollow precursor particles

An ultrasonic atomizer replaces the pressure nozzle in a closed-loop spray dryer. A metering pump feeds the filtered precursor liquid onto the vibrating atomizer surface, and a nitrogen sweep carries the droplets into the heated chamber. Solvent evaporation forms a shell around each shrinking droplet, producing hollow particles under shell-forming drying conditions. An inert gas classifier removes fines and coarse particles to bring the collected powder to a volume-based particle size span of 15 or less.

Parameter or scale variation

Separate product cuts by median diameter

An inert gas classifier divides a hollow spray-dried precursor lot into fine and coarse fractions. The fine fraction targets a D50 of 8–12 μm, and the coarse fraction targets a D50 of 25–35 μm. Each fraction is collected in a separate sealed hopper and checked for a volume-based particle size span of 15 or less. The two fractions are heat-treated in separate batches to produce lithium sulfide powder.

Controlled wall thickness in hollow particles

A spray dryer produces hollow precursor particles with a D50 of 25–35 μm and a target median shell thickness of 2–4 μm. The liquid feed solids concentration controls the amount of material deposited in each shell, and the atomizer settings control droplet size. Cross sections of embedded particles provide shell thickness measurements for adjusting the feed solids concentration between runs. A gas classifier trims the size distribution to a volume-based particle size span of 15 or less before heat treatment.

Combination with existing systems

Sealed transfer to a rotary kiln

The spray dryer collector feeds a nitrogen-purged lock hopper connected to a sealed rotary tube kiln. The collector supplies hollow precursor powder with a volume-based particle size span of 15 or less. The lock hopper cycles its inlet and outlet valves, and a screw feeder meters the powder into the inclined, heated tube. Tube rotation advances the powder through the heated zone, and the converted lithium sulfide cools under inert gas before discharge.

Specific version of a part

Spray-dry hollow sulfate shells

A two-fluid nozzle atomizes an aqueous lithium sulfate solution into heated nitrogen. Rapid evaporation concentrates salt at the droplet surface, where a shell forms around a hollow core as drying proceeds.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2016/0326053 A1
Published
Nov 10, 2016
Filed
Nov 3, 2014
Class
C04B 14/361
Document BUS 2021/0078866 A1
Published
Mar 18, 2021
Filed
Aug 25, 2020
Class
C01B 33/124
Claim 1
Document A
Document B
1.1wherein the precursor has a hollow shape, and
Example methods are disclosed for producing hollow ceramic microspheres from hollow spheres with walls consisting of silica or glass (containing silica) using a transforming solution or transformation powder that contains a highly reactive atom, M, that replaces silicon atoms in silica or silica containing glass.
B · US 2021/0078866 A1 · ¶ 7
1.2satisfies the following Equation 1: (Dmax−Dmin)/D50≤15 <Equation 1>
The ground improvement material according to the present embodiment contains a soil that satisfies a condition in which, when a particle diameter of the largest particle is defined as Dmax and a particle diameter of the smallest particle is defined as Dmin on a grain size accumulation curve created through a particle diameter analysis of the soil, a product of an accumulative passage rate (Pos) from a value obtained by multiplying Dmin by 4.45 to the Dmax value and an accumul
A · US 2016/0326053 A1 · ¶ 38
1.3(wherein Dmax, Dmin, and D50 respectively represent the maximum particle size, the minimum particle size, and the particle size at which 50% of the volume is accumulated).

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2. Only Document B has a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Therefore, it is necessary to adjust the particle diameter distribution of the soil in order to promote the strength of the embankment body, which is formed by the replacement method and embankments.
A · US 2016/0326053 A1 · ¶ 6
An embodiment of the present invention is directed to provide a ground improvement material and a method for manufacturing the same improving the strength of the embankment body formed by the replacement method or embankments, by changing the particle diameter distribution of the soil.
A · US 2016/0326053 A1 · ¶ 8
At high temperatures their low viscosity will lead to their collapse, and the presence of heavy metals poses both environmental and physical problems.
B · US 2021/0078866 A1 · ¶ 4
Non-spherical shapes can be produced by increasing the transformation temperature whereby the viscosity of the walls of the HSMS and/or the HGMS is reduced Microcomposite—uniform distribution of the hollow spheres in a matrix producing isotropic properties throughout the composite MO—represents oxides of M.
B · US 2021/0078866 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0365515 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365515/, SHA-256 c9c1fba53a69e225311cbf37578efe0fdf879be341b51426303a5e4801b01135
First published
Permanent addresshttps://patent.fyi/US20260365515/
Content fingerprint (SHA-256)c9c1fba53a69e225311cbf37578efe0fdf879be341b51426303a5e4801b01135
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi