1.1Gelation by solvent exchange
An ethanol bath exchanges with water in the cast dispersion and causes the cellulose nanofibers to associate into a wet network. A vacuum dryer removes the ethanol from the gel before carbonization.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
An ethanol bath exchanges with water in the cast dispersion and causes the cellulose nanofibers to associate into a wet network. A vacuum dryer removes the ethanol from the gel before carbonization.
Freezing separates water ice from a sucrose-rich phase. Vacuum sublimation removes the ice, and staged heating under nitrogen dehydrates and carbonizes the sugar into a char for final heat treatment.
A refrigerated chamber keeps the body below the melting point while dry nitrogen flows over its exposed surfaces. Ice sublimes into the gas stream, and a cold trap captures the water before the nitrogen recirculates.
The frozen body thaws in a support basket, and successive ethanol baths displace water from the wet fiber network. A pressure vessel exchanges the ethanol with liquid carbon dioxide, heats the fluid above its critical temperature at sufficient pressure, and vents it isothermally to dry the network without a liquid–vapor meniscus.
A perforated ceramic basket holds pieces of dried cellulose below the surface of a molten sodium chloride and potassium chloride mixture at about 700 °C. The melt transfers heat as the cellulose decomposes and releases volatile products. After cooling, a water rinse dissolves residual salt and leaves the carbonaceous solid.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Freeze an aqueous cellulose nanofiber dispersion, vacuum-dry the frozen body, and carbonize the dried body under flowing nitrogen. Heat the resulting amorphous carbon under argon while applying uniaxial pressure to grow graphite crystallites within the hard carbon. Mill the hard carbon, disperse the powder into the resin component of a two-part epoxy floor coating, and add the curing agent before application. Adjust the carbon loading using surface resistance measurements on cured test panels.
Freeze and vacuum-dry a cellulose nanofiber gel, then carbonize the dried body under flowing argon. Load the amorphous carbon into a thin-walled molybdenum capsule, evacuate the capsule, and seal it by welding. Heat the capsule in a hot isostatic press and apply argon pressure to its exterior so the capsule compresses the carbon from all sides during crystallite growth. Cool and depressurize the vessel before removing the capsule and recovering the hard carbon.
Dispense a 1.5 percent by mass aqueous cellulose nanofiber dispersion into shallow metal trays to a depth of 3 mm and freeze it on a shelf held at −40 °C. Transfer the frozen trays to a vacuum dryer and hold the chamber at 20 Pa during primary drying, using tray temperature probes to keep the material below its collapse temperature. Carbonize the dried sheets under flowing argon by ramping at 2 °C per minute to 800 °C and holding for 60 minutes. Stack the carbonized sheets in a die and heat the stack under argon at 1,600 °C and 30 MPa for 30 minutes to grow graphite crystallites.
Freeze a cellulose nanofiber gel, vacuum-dry it, and load the dried bodies into a nitrogen-purged batch retort. Connect the retort outlet to a thermal oxidizer through a heated transfer line that carries the vapors and gases released during carbonization. Introduce combustion air at the oxidizer and use an outlet pressure controller to maintain the retort slightly above ambient pressure. Cool the amorphous carbon under nitrogen, then transfer it to an argon-purged hot press for pressure-assisted crystallite growth.
Place the frozen cellulose nanofiber bodies on temperature-controlled shelves and fit the vacuum chamber with a capacitance manometer, a thermal conductivity vacuum gauge, and product temperature probes. A controller adjusts shelf temperature to keep the product below its measured collapse temperature and tracks convergence of the two pressure readings as water vapor flow declines. When the readings converge, the controller briefly isolates the chamber from the pump and advances to secondary drying if the pressure rise stays below a threshold established with dry reference batches. Carbonize the dried bodies under nitrogen and heat the resulting amorphous carbon under argon while applying pressure.
Freeze and vacuum-dry cellulose nanofiber bodies, carbonize them under argon, and load a measured mass of the amorphous carbon into a hot-press die. A controller uses a temperature sensor and a load cell to hold the programmed temperature and compressive stress under argon. It subtracts thermal expansion and load-dependent tooling deflection from punch displacement using calibration runs, then starts cooling after the corrected shrinkage rate stays below a threshold for a preset interval. Establish the threshold from calibration batches by comparing their shrinkage curves with graphite crystallite dimensions estimated from X-ray diffraction.
A shallow mold holds an aqueous cellulose nanofiber dispersion against a copper plate held at about −40 °C. Ice grows away from the plate and concentrates the nanofibers between adjacent ice crystals.
A vacuum freeze dryer holds the frozen body on a temperature-controlled shelf and maintains chamber pressure near 30 Pa during primary drying. A condenser at about −70 °C captures sublimed water vapor while the shelf supplies heat to sustain sublimation.
A ceramic boat holds the dried nanofiber body in a tube furnace purged with flowing nitrogen. The furnace ramps at about 3 °C per minute to 800 °C and holds for one hour while the cellulose releases volatile products and forms an amorphous carbon-rich residue.
Graphite punches compact the amorphous carbon powder in a heated graphite die under argon at about 30 MPa and 1,600 °C. The hot dwell increases local graphitic ordering while the punches maintain contact between particles and consolidate the powder.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
It is summarized that a method of producing cellulose-nanofiber carbon according to an aspect of the present invention is a method of producing cellulose-nanofiber carbon by carbonizing a cellulose nanofiber, the method comprising: a freezing step of freezing a solution or gel containing the cellulose nanofiber to obtain a frozen product; a drying step of drying the frozen product in a vacuum to obtain a dried product; and a carbonizing step of heating and carbonizing the driA · US 2021/0163293 A1 · ¶ 11
The drying step dries the frozen product, frozen in the freezing step, in a vacuum to obtain a dried product (step S3).A · US 2021/0163293 A1 · ¶ 42
In the drying step, the liquid is removed from the mixed solution (step S6). When drying the slurry-like mixed solution (mixed slurry), a constant temperature bath, a vacuum dryer, an infrared dryer, a hot air dryer, a suction dryer, or the like may be used.B · US 2022/0098040 A1 · ¶ 73
The carbonizing step heats and carbonizes the dried product, dried in the drying step, in an atmosphere which does not burn the dried product, thereby obtaining cellulose-nanofiber carbon (step S4).A · US 2021/0163293 A1 · ¶ 44
A method for producing cellulose nanofiber carbon by carbonizing cellulose nanofibers, the method comprising: semi-carbonizing a dispersion liquid or gel containing cellulose nanofibers with a heat medium to obtain a semi-carbonized product; and heating and carbonizing the semi-carbonized product in an atmosphere that does not burn the semi-carbonized product to obtain cellulose nanofiber carbon.B · US 2022/0098040 A1 · claim 1
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.1. Both have a passage for 1.2 1.3. Both are classified in CPC C01B, as is this patent.
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
In addition, in the case of obtaining a carbon material by heat treating cellulose nanofibers, the cellulose nanofibers agglomerate during drying and sinter during heat treatment, resulting in a dense carbon material.A · US 2021/0163293 A1 · ¶ 9
Related claim parts: 1.2 1.3
In addition, a method for producing cellulose nanofibers from cellulose derived from natural products is also being studied, but when the cellulose nanofibers are heat-treated to obtain a carbon material, the cellulose nanofibers aggregate during being dried and are sintered during the heat treatment, and the obtained carbon material has a high density and is difficult to have a large specific surface area.B · US 2022/0098040 A1 · ¶ 7
Related claim parts: 1.1
A carbon nanofiber produced by a conventional production method has problems of the lack of elasticity to cause plastic deformation which makes it impossible to return to the original shape after compression and bending, and low mechanical strength.A · US 2021/0163293 A1 · ¶ 8
The present invention has been made in view of the above problem, and an objective thereof is to provide cellulose-nanofiber carbon which has stretchability and high mechanical strength and can achieve a large specific surface area, and a method of producing the same.A · US 2021/0163293 A1 · ¶ 10
The present invention has been made in view of this problem, and an object of the present invention is to provide cellulose nanofiber carbon having elasticity, high mechanical strength, and capable of increasing its specific surface area, and a method for producing the same.B · US 2022/0098040 A1 · ¶ 8
patent.fyi, US 2026/0365517 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365517/, SHA-256 10a88d40678a0e12a0d2633b0e0aae603e088a73dd2b773488ed527c1ecaf25a